Surface and structural changes in SiC pre-implanted with helium, silver, and strontium after annealing, and their effect on silver and strontium migration
Source abstract
Abstract
The effect of helium (He), silver (Ag) and strontium (Sr) ions implantation and annealing on the surface and structural properties of SiC as well as the migration of Ag and Sr was investigated in this study. Ag and Sr were sequentially implanted at 360 keV and 280 keV, respectively, each to a fluence of 2×10 16 cm -2 at 600 °C. Some dual implanted (Ag+Sr-SiC) samples were additionally implanted with He of 17 keV to a 1×10 17 cm -2 at 350 °C, forming triple- implanted samples (Ag+Sr+He-SiC). Both dual and triple implanted samples underwent isochronal annealing at 1100, 1200, and 1300 °C for 5 hours. Ag, Sr and He implantation introduced defects in both dual and triple implanted samples. However, triple-implanted samples developed surface blisters and holes due to the migration of He bubbles. At 1100 °C, partial recovery of structural damage was observed in both dual- and triple-implanted samples, but graphite formed in the latter, and holes persisted. At higher temperatures (i.e., 1200 and 1300°C), dual-implanted samples showed significant structural recovery, whereas the graphite in triple-implanted samples impeded the healing of defects. Depth profiling revealed minimal changes in Ag and Sr distributions and concentrations in dual- implanted samples post-annealing up to 1300 °C. However, triple-implanted samples lost ∼20% of Ag and Sr at 1100 °C due to sublimation via holes. At 1200 and 1300 °C, no further losses occurred, but Ag and Sr migrated toward the surface. These findings suggest that He implantation promotes the formation of holes in SiC, facilitating the loss of Ag and Sr at 1100 °C. Additionally, He-induced defects enhance the migration of Ag and Sr toward the surface during annealing at 1200 and 1300 °C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. TRISO-Coated particle fuel performance10.1016/B978-0-08-056033-5.00055-0 ↗
2. Ion beam analysis of materials in the PBMR reactor10.1016/j.nimb.2007.10.046 ↗
3. Topical Review: diffusion of fission products and radiation damage in SiC
4. Coated particle fuel for high temperature gas cooled reactors10.5516/NET.2007.39.5.603 ↗
5. Diffusion of fission products and radiation damage in SiC10.1088/0022-3727/46/47/473001 ↗
6. 1997
7. Evaluation of silver transport through SiC during the German HTR fuel program10.1016/j.jnucmat.2009.09.024 ↗
8. Metal fission product behaviour in high temperature reactors-UO2 coated particle fuel10.1016/0022-3115(76)90005-2 ↗
9. Silver release from coated particle fuel10.13182/NT35-483 ↗
10. Fission-product release during post irradiation annealing of several types of coated fuel particles10.1016/0022-3115(84)90558-0 ↗
11. Influence of radiation damage on strontium and iodine diffusion in silicon carbide10.1016/j.jnucmat.2011.10.032 ↗
12. Influence of radiation damage on diffusion of fission products in silicon carbide10.1002/pssc.201200457 ↗
13. Study of silver diffusion in silicon carbide10.1016/j.jnucmat.2009.02.022 ↗
14. Effect of thermal annealing and neutron irradiation in 6H-SiC implanted with silver at 350 oC and 600 oC10.1016/j.nimb.2011.07.039 ↗
15. Annealing of silver implanted 6H–SiC and the diffusion of the silver10.1016/j.nimb.2011.12.006 ↗
16. Silver ion implantation and annealing in CVD silicon carbide: the effect of temperature on silver migration
17. Effects of Ag and Sr dual ions implanted into SiC10.1016/j.nimb.2020.03.035 ↗
18. Palladium assisted silver transport in polycrystalline SiC10.1016/j.nucengdes.2011.09.064 ↗
19. Iodine assisted retainment of implanted silver in 6H-SiC at high temperatures10.1016/j.nimb.2014.05.015 ↗
20. Palladium and ruthenium supported silver migration in 3C–silicon carbide10.1016/j.jnucmat.2014.10.017 ↗
21. Effects of helium (He) bubbles and annealing on the structural evolution and migration behavior of silver (Ag) implanted into polycrystalline SiC at 350 °C10.1016/j.vacuum.2023.112621 ↗
22. Helium and strontium co-implantation into SiC at room temperature and isochronal annealing: structural evolution of SiC and migration behaviour of strontium10.1016/j.matchemphys.2022.126998 ↗
23. The effects of co-implanting strontium (Sr) and helium (He) into SiC at temperatures exceeding the critical amorphization temperature and annealing above 1000 oC10.1016/j.ceramint.2025.03.140 ↗
24. The influence of helium-induced defects on the migration of strontium implanted into SiC above critical amorphization temperature10.3389/fmats.2023.1192989 ↗
25. The migration behaviour of strontium co-implanted with helium into SiC at room temperature and annealed at temperatures above 1000 °C10.1016/j.vacuum.2024.113676 ↗
26. Helium assisted migration of silver implanted into SiC10.1016/j.vacuum.2020.109865 ↗
27. Unraveling interaction mechanisms of Kr cavities with Ag in irradiated silicon carbide under high temperatures10.1016/j.nimb.2025.165697 ↗
28. The stability of vacancy clusters and their effect on helium behaviors in 3C-SiC10.1016/j.jnucmat.2018.03.010 ↗
29. The effects of helium, strontium, and silver triple ions implanted into SiC10.1016/j.heliyon.2023.e20877 ↗
30. Review of OriginPro 8.510.1021/ja202216h ↗
31. 2004
32. SRIM–The stopping and range of ions in matter, (2010)10.1016/j.nimb.2010.02.091 ↗
33. The efficiency of damage production in silicon carbide10.1016/j.nimb.2003.12.006 ↗
34. Ion implantation effects in silicon carbide10.1016/0168-583X(93)90703-9 ↗
35. Effect of heat treatment on the migration behaviour of selenium implanted into polycrystalline SiC10.1016/j.nimb.2020.08.022 ↗
36. Raman investigation of different polytypes in SiC thin films grown by solid-gas phase epitaxy on Si (111) and 6H-SiC substrates10.4028/www.scientific.net/MSF.645-648.359 ↗
37. Effect of impurities on the Raman scattering of 6H-SiC crystals10.1590/S1516-14392012005000108 ↗
38. Effect of swift heavy ions irradiation in the migration of silver implanted into polycrystalline SiC10.1016/j.nimb.2019.10.002 ↗
39. Effect of SHI irradiation and high temperature annealing on the microstructure of SiC implanted with Ag10.1016/j.nimb.2021.11.016 ↗
40. Impurity effects on solid–solid transitions in atomic clusters10.1039/C6NR06299G ↗
41. Bonding in solids