Compressive strength, abrasion resistance, and microstructure of alkali-activated slag mortar at elevated temperatures

Quynh Thi Ngoc Le, Tong Nguyen, Thanh Tai Tran

Ceramics International· Volume 51· Issue 25
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Fire effects on concrete materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Effect of fire and cooling mode on the properties of slag mortars10.1016/S0008-8846(01)00561-0 ↗
2. Influence of binder composition on the gel structure in alkali activated fly ash/slag pastes exposed to elevated temperatures10.1016/j.ceramint.2016.11.042 ↗
3. Effect of temperature on the physico-mechanical and mineralogical properties of homra pozzolanic cement pastes10.1016/S0008-8846(00)00403-8 ↗
4. Chemical and mechanical stability of sodium sulfate activated slag after exposure to elevated temperature10.1016/j.cemconres.2011.10.007 ↗
5. Hewlett · 1998
6. Hydro-abrasive erosion of steel-fibre reinforced hydraulic concrete10.1016/S0043-1648(02)00215-6 ↗
7. Abrasion resistance of metakaolin-based geopolymers through accelerated testing and natural wear
8. Concrete pavement blocks - requirements and test methods
9. 1997
10. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
11. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
12. Metakaolin geopolymer characterization and application for ammonium removal from model solutions and landfill leachate10.1016/j.clay.2015.10.027 ↗
13. Alkali-activated materials10.1016/j.cemconres.2017.02.009 ↗
14. Alkali-activated fly ash/slag cements: strength behaviour and hydration products10.1016/S0008-8846(00)00298-2 ↗
15. The role of inorganic polymer technology in the development of ‘green concrete’10.1016/j.cemconres.2007.08.018 ↗
16. Carbon footprint and water use of alkali-activated and hybrid cement mortars10.1016/j.jclepro.2021.128653 ↗
17. Fire-resistant geopolymer produced by granulated blast furnace slag10.1016/S0892-6875(03)00008-6 ↗
18. Residual strength properties of sodium silicate alkali activated slag paste exposed to elevated temperatures10.1617/s11527-009-9546-3 ↗
19. Clinkerless ultra-high strength concrete based on alkali-activated slag at high temperatures10.1016/j.cemconres.2021.106465 ↗
20. Residual compressive behavior of alkali‐activated concrete exposed to elevated temperatures10.1002/fam.983 ↗
21. The effect of elevated temperature on the residual tensile strength and physical properties of the alkali-activated slag concrete10.1016/j.jobe.2018.08.015 ↗
22. Influence of recycled concrete aggregates on alkali-activated slag mortar exposed to elevated temperatures
23. Microstructural alteration of alkali activated slag mortars depend on exposed high temperature level10.1016/j.conbuildmat.2015.12.070 ↗
24. The influence of curing conditions and alkaline activator concentration on elevated temperature behavior of alkali activated slag (AAS) mortars10.1016/j.conbuildmat.2018.09.099 ↗
25. Standard test method for compressive strength of hydraulic cement mortars (using 2-in
26. Freedman · 2009
27. Behaviour of alkali-activated fly ash-slag paste at elevated temperatures: an experimental study10.1016/j.cemconcomp.2024.105438 ↗
28. Abrasion resistance of alkali-activated slag concrete designed by taguchi method10.1016/j.conbuildmat.2015.08.128 ↗
29. Effect of binder content on the performance of alkali-activated slag concretes10.1016/j.cemconres.2010.08.017 ↗
30. Very early-age reaction kinetics and microstructural development in alkali-activated slag10.1016/j.cemconcomp.2014.09.001 ↗
31. Temperature and activator effect on early-age reaction kinetics of alkali-activated slag binders10.1016/j.conbuildmat.2016.03.098 ↗
32. Effects of curing: Comparison of optimised alkali-activated PC-FA-BFS and PC concretes10.1680/macr.13.00231 ↗
33. High strength blended cement concrete incorporating volcanic ash: performance at high temperatures10.1016/j.cemconcomp.2006.01.013 ↗
34. Mechanical and microstructural properties of heat cured alkali-activated slag mortars10.1016/j.matdes.2011.10.005 ↗
35. Compressive strength of concrete at high temperatures: a reassessment10.1680/macr.1992.44.161.291 ↗
36. Mechanical and microstructural evolutions of fly ash/slag-based geopolymer at high temperatures: effect of curing conditions10.1016/j.ceramint.2022.09.175 ↗
37. A preliminary study of alkali-activated slag blended with silica fume under the effect of thermal loads and thermal shock cycles10.1016/j.conbuildmat.2012.10.014 ↗
38. Effect of elevated temperature on the mechanical properties of concrete produced with finely ground pumice and silica fume10.1016/j.firesaf.2010.08.002 ↗
39. Damage behavior of geopolymer composites exposed to elevated temperatures10.1016/j.cemconcomp.2008.08.001 ↗
40. Mechanical and thermal characterisation of geopolymers based on silicate-activated metakaolin/slag blends10.1007/s10853-011-5490-z ↗
41. Dehydration and rehydration processes of cement paste exposed to high temperature environments10.1023/B:JMSC.0000025827.65956.18 ↗
42. Gel nanostructure in alkali-activated binders based on slag and fly ash, and effects of accelerated carbonation10.1016/j.cemconres.2013.06.007 ↗
43. Characterization of alkali activated slag paste after exposure to high temperatures10.1016/j.conbuildmat.2013.06.070 ↗
44. Influence of the activator concentration of sodium silicate on the thermal properties of alkali-activated slag pastes10.1016/j.conbuildmat.2015.11.023 ↗