Salt bath titanium plating of SiC powders and their application in aluminum matrix composites fabricated via wire-powder-arc additive manufacturing
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Additive Manufacturing Materials and Processes · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Laser powder bed fusion of oxidized microscale sic-particle-reinforced AlSi10Mg matrix composites: microstructure, porosity, and mechanical properties10.1016/j.msea.2023.144860 ↗
2. Effect of Sc microalloying on fabrication, microstructure and mechanical properties of SiCp/Al-Cu-Mg-Sc composites via powder metallurgy10.1016/j.msea.2023.145152 ↗
3. Fabrication of co-continuous SiC/Al composites from novel SiC preforms with high porosity and controllable pore size10.1016/j.ceramint.2020.09.130 ↗
4. Wear properties of aluminum alloys fabricated by laser powder bed fusion10.1016/j.triboint.2023.108769 ↗
5. Mechanical property prediction and configuration effect exploration of particulate reinforced metal matrix composites via an interpretable deep learning approach10.1016/j.msea.2025.147880 ↗
6. Strengthening effects of Mg-Si precipitates on wear resistance of SiCp/A1-Si-Mg composites10.1016/j.wear.2024.205716 ↗
7. Influence of squeeze casting pressure on nanoparticle distribution and mechanical properties of nano-SiCp/Al–Cu composites assisted with ultrasonic vibration10.1016/S1003-6326(23)66237-5 ↗
8. Review on development of metal/ceramic interpenetrating phase composites and critical analysis of their properties10.1016/j.ceramint.2021.09.232 ↗
9. Microstructure and Mechanical properties of 45 vol.% SiCp/7075A1 composite10.1016/j.jmst.2015.01.012 ↗
10. Effect of Ti doping on the microstructure and properties of SiCp/Al composites by pressureless infiltration10.3390/ma17071608 ↗
11. Enhanced intragranular precipitation strengthening in Sc-microalloyed ultrafine-grained SiCp/Al-Cu-Mg composites via retrogression and re-ageing heat treatment10.1016/j.matdes.2025.113789 ↗
12. Advances in additive manufacturing of SiC/Al composites: a review
13. Investigation of Ti alloying for microstructural evolution and strengthening mechanism: avoiding Al4C3 formation in SiCp/Al composites via laser directed energy deposition10.1016/j.jallcom.2023.172371 ↗
14. Effect of a Zr source addition on the microstructure of Al-SiC composites elaborated by the laser powder bed fusion (L-PBF) process10.1016/j.matchar.2024.114472 ↗
15. Selective laser melting of SiC/Al composites: densification, microstructure, and mechanical and tribological properties10.1016/j.ceramint.2021.07.263 ↗
16. Selective laser melting of in-situ Al4SiC4 + SiC hybrid reinforced Al matrix composites: influence of starting SiC particle size10.1016/j.surfcoat.2015.04.029 ↗
17. Effect of SiC particle size on densification behavior and mechanical properties of SiCp/AlSi10Mg composites fabricated by laser powder bed fusion10.1016/j.jallcom.2020.156260 ↗
18. Effect of process parameters on the density and porosity of laser melted AlSi10Mg/SiC metal matrix composite10.1007/s11465-018-0521-y ↗
19. Effect of heat treatment patterns on microstructure and mechanical properties of selective laser melting fabricated SiC/AlSi10Mg composite
20. SiC reinforced AlSi10Mg composites fabricated by selective laser melting10.1016/j.jallcom.2021.162365 ↗
21. Microstructure and mechanical properties of SiC reinforced AlSil0Mg composites fabricated by laser metal deposition10.1016/j.jmapro.2020.08.073 ↗
22. The effect of thermal mismatch on the thermal conductance of Al/SiC and Cudiamond composites10.1063/1.5133982 ↗
23. Selective laser melting of aluminium components10.1016/j.jmatprotec.2010.09.019 ↗
24. Wire-powder-arc additive manufacturing: a viable strategy to fabricate carbide ceramic/aluminum alloy multi-material structures
25. Dual-gradient ceramic/aluminum composite structure fabricated by arc additive manufacturing with co-conveying of wire and powder10.1080/21663831.2024.2336020 ↗
26. High wear-resistant aluminum matrix composite layer fabricated by MIG welding with lateral B4C powder injection10.1007/s11665-018-3672-4 ↗
27. A comparison of aluminium-based metal-matrix composites reinforced with coated and uncoated particulate silicon carbide10.1016/S0266-3538(99)00151-7 ↗
28. Effects of reinforcement surface modification on the microstructures and tensile properties of SiCp/Al2014 composites10.1016/j.msea.2014.11.066 ↗
29. The microstructure and tensile property for Al2014 composites reinforced with Ti5Si3-coated SiCp10.1016/j.msea.2017.02.016 ↗
30. Microstructures and mechanical properties of A1 2519 matrix composites reinforced with Ti-coated SiC particles10.1016/S1003-6326(20)65260-8 ↗
31. Forbes · 2010
32. Molten salt synthesis of Ti-Si-C coating on SiC particles and hot pressing of the prepared powders10.1016/j.ceramint.2024.08.363 ↗
33. Fabrication of plasma-sprayed TiC-Ti5Si3-Ti3SiC2 composite coatings from the annealed Ti/SiC powders10.1016/j.surfcoat.2021.127227 ↗
34. Effects of Ti-coating layer on the distribution of SiCp in the SiCp/2014Al composites10.1016/j.matdes.2015.09.089 ↗
35. Low-temperature preparation of titanium carbide coatings on graphite flakes from molten salts10.1111/j.1551-2916.2007.02184.x ↗
36. Molten salt synthesis and characterization of titanium carbide-coated graphite flakes for refractory castable applications10.1111/j.1744-7402.2010.02529.x ↗
37. Preparation of Ti-coated diamond particles by microwave heating10.1016/j.apsusc.2016.08.168 ↗
38. Reaction mechanisms for Ti coatings on diamond10.1016/j.carbon.2024.119206 ↗
39. Enhanced thermal conductivity of copper/diamond composites by fine-regulating microstructure of interfacial tungsten buffer layer10.1016/j.jallcom.2020.157440 ↗
40. 2023
41. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
42. Microstructure and mechanical properties of Si3N4/Si3N4 joint brazed with Ag-Cu-Ti + SiCp composite filler10.1016/j.msea.2010.01.065 ↗
43. Porosity formation in AI-9 Wt pct Si-3 Wt pct Cu alloy systems: metallographic observations10.1007/BF02648419 ↗
44. Effect of iron content on the formation of β-Al5FeSi and porosity in Al-Si eutectic alloys10.1016/j.jmatprotec.2008.02.073 ↗
45. Effect of SiC particles on the laser sintering of Al-7Si-0.3Mg alloy10.1016/j.scriptamat.2008.03.007 ↗
46. Microstructure and wear studies of laser clad Al-Si/SiC(p) composite coatings10.1016/j.surfcoat.2007.04.003 ↗
47. High wear-resistant aluminum matrix composite layer fabricated by MIG welding with lateral B4C powder injection10.1007/s11665-018-3672-4 ↗
48. Correlation between the characteristics of the mechanically mixed layer and wear behaviour of aluminium, Al-7075 alloy and Al-MMCs10.1016/S0043-1648(00)00463-4 ↗
49. Effect of debris size on the reciprocating sliding wear of aluminium10.1016/j.wear.2016.10.025 ↗