journal article·2026-03

Combined effects of hot and CMAS corrosion and initial heat treatment on HVOF-applied CoNiCrAlY bond coats

Mohammadrasoul Javadi Sigaroodi, Javad Rahimi, Esmaeil Poursaeidi

Ceramics International· Volume 52· Issue 7
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Heterogeneous fatigue damage in a nickel-based single-crystal superalloy unraveled using correlative 3D X-ray technology10.1016/j.actamat.2025.121326 ↗
2. Tensile-tensile fatigue behavior of plain-woven SiCf/SiC ceramic matrix composites with differently spaced film cooling holes and environmental barrier coatings in high-temperature water-oxygen environments10.1016/j.ceramint.2024.02.031 ↗
3. Design of turbine blade internal cooling: a thermofluidic study on the influence of varying cooling channel numbers and configurations10.1134/S0040601524700782 ↗
4. Research status of RE hafnates for thermal/environmental barrier coatings10.1016/j.ceramint.2025.03.091 ↗
5. Experimental and numerical life evaluation of TBCs with different BC and diffusion coating under cyclic thermal loading10.1111/ijac.14426 ↗
6. The effect of ceramic YSZ powder morphology on coating performance for industrial TBCs10.1016/j.surfcoat.2023.130270 ↗
7. Investigation of the hot corrosion effects on the lifetime of TBCs with and without TC10.1016/j.jallcom.2024.175840 ↗
8. Characterization and hot corrosion behavior of the La2(Zr0.7Ce0.3)2O7/8YSZ:Eu double ceramic layer coating prepared by atmospheric plasma spraying
9. Thermal cycling property of the novel Hf6Ta2O17/YSZ TBCs prepared by atmospheric plasma spraying technology
10. Improved thermal shock resistance of GYYZO-YSZ double ceramic layer TBCs induced by induction plasma spheroidization10.1016/j.surfcoat.2024.130372 ↗
11. Role of TiC and WC addition on the mechanism and kinetics of isothermal oxidation and high-temperature stability of ZrB2–SiC composites10.1007/s11085-024-10234-1 ↗
12. Development of thermal barrier coating on single crystal superalloy CMSX-4 by two-source evaporation EB-PVD and hot corrosion performance of the coating in a simulated aero-engine environment10.1016/j.surfcoat.2024.130885 ↗
13. Review of suspension and solution precursor plasma sprayed thermal barrier coatings10.1016/j.ceramint.2016.06.063 ↗
14. Influence of different plasma spraying methods on the physical properties of YSZ coatings
15. Understanding the effect of bondcoat surface treatment on enhanced lifetime of suspension plasma sprayed thermal barrier coatings10.1016/j.surfcoat.2024.130716 ↗
16. Role of bond coat processing methods on the durability of plasma sprayed thermal barrier systems10.1016/j.surfcoat.2019.07.065 ↗
17. Properties of alumina coatings prepared on silica-based ceramic substrate by plasma spraying and sol-gel dipping methods10.1016/j.ceramint.2021.06.168 ↗
18. Kinetics and mechanism of isothermal oxidation of compositionally graded yttria stabilized zirconia (YSZ) based thermal barrier coating10.1016/j.corsci.2014.06.050 ↗
19. Surface & coatings technology influence of molten salt with or without V 2 O 5 on hot corrosion and high-temperature tribological performance of HVOF-sprayed Ni-based self-lubricating composite coating10.1016/j.surfcoat.2021.127210 ↗
20. Effect of thermal spraying method, time and temperature on the thickness of thermally grown oxide and lifetime of thermal barrier coatings10.1007/s11666-023-01670-7 ↗
21. Residual stress in air-plasma-sprayed thermal barrier coatings under long-term high-temperature oxidation10.1016/j.surfcoat.2024.130827 ↗
22. Oxide growth in high-strain tolerance thermal barrier coating with segmented vertical cracks10.1016/j.ceramint.2024.04.228 ↗
23. Heat treatment effect on coating shock resistance of thermal barrier coating system with different types of bond coat10.1016/j.jeurceramsoc.2023.01.035 ↗
24. The effect of two raw YSZ materials with different morphology on TBCs via atmospheric plasma spraying: microstructures and high-temperature performance10.1016/j.surfcoat.2024.130723 ↗
25. High-Temperature hot corrosion resistance of CrAl/NiCoCrAlY/AlSiY gradient composite coating on TiAl alloy10.3390/coatings14081067 ↗
26. Thermal shock resistance of thermal barrier coating with different bondcoat types and diffusion pre-coating10.1016/j.ceramint.2022.09.172 ↗
27. Thermal barrier coatings for high temperature applications – a short review10.1016/j.matpr.2020.08.017 ↗
28. A review on recent applications and future prospects of rare earth oxides in corrosion and thermal barrier coatings, catalysts, tribological, and environmental sectors10.1016/j.ceramint.2022.07.220 ↗
29. Impact of bond coat types on calcium-magnesium-alumina-silicate and hot corrosion behavior in thermal barrier coatings10.1016/j.corsci.2023.111742 ↗
30. Application of thermal gradient and thermal cycling tests to Al2O3/CYSZ functionally graded TBC in the presence of simultaneous hot corrosion and CMAS effects10.1016/j.surfcoat.2022.128688 ↗
31. Cubic fluorite-based lanthanum cerium oxide thermal barrier top-coat fabrication, properties, and performance: present status and prospects10.1016/j.jeurceramsoc.2024.116804 ↗
32. Calcia magnesia alumino silicate (CMAS) corrosion attack on thermally sprayed thermal barrier coatings: a comprehensive review10.1038/s41529-024-00462-w ↗
33. Crystallization behavior of CMAS + sea salt mixture and its effect on the mixture penetration into thermal barrier coatings10.1016/j.surfcoat.2023.130012 ↗
34. Crystallization behavior of CMAS and NaVO3+CMAS mixture and its potential effect to thermal barrier coatings corrosion10.1016/j.ceramint.2021.08.072 ↗
35. Corrosion behaviors and failure mechanism of plasma sprayed Yb2Si2O7/Si environmental barrier coatings exposed to CMAS+ NaVO310.1016/j.jeurceramsoc.2024.117005 ↗
36. Effect of interface roughness on the CMAS + molten salt (Na2SO4 + NaCl + NaVO3) corrosion resistance of EB-PVD thermal barrier coatings10.1016/j.surfcoat.2025.132026 ↗
37. Degradation of YSZ thermal barrier coatings by CMAS and CMAS-Na2SO4 between 1250°C and 1350°C10.1016/j.jeurceramsoc.2025.117405 ↗
38. Thermal shock behavior and CMAS degradation of YSZ-Y2O3 and YSZ-Y2Zr2O7 double ceramic layered thermal barrier coatings10.1016/j.ceramint.2024.12.230 ↗
39. Research status of RE hafnates for thermal/environmental barrier coatings
40. Oxidation and hot corrosion resistance of HVOF/EB-PVD thermal barrier coating system10.1016/j.surfcoat.2021.126862 ↗
41. Research on modified thermal barrier coatings against CMAS corrosion driven by mechanism–data hybrid model10.3390/coatings14121513 ↗
42. Sc-doped Gd2Zr2O7 coating on YSZ thermal barrier coatings to resist CMAS + molten salt attack10.1016/j.ceramint.2022.01.024 ↗
43. Corrosion behavior of CMAS coupling NaVO3 salt for plasma-sprayed Al2O3/YSZ thermal barrier coatings10.1016/j.corsci.2023.111369 ↗
44. Laser surface modification to improve the resistance of CMAS + molten salt coupling corrosion to thermal barrier coatings10.1016/j.ceramint.2023.07.203 ↗
45. Tracking the calcium-magnesium-alumino-silicate (CMAS) infiltration into an air-plasma spray thermal barrier coating using X-ray imaging10.1016/j.scriptamat.2019.09.016 ↗
46. Effects of surface roughness on CMAS wetting and corrosion behaviour of rare earth modified zirconia coatings10.1016/j.ceramint.2023.11.054 ↗
47. Effect of pre-oxidation on the moderate-temperature hot corrosion behavior of CoNiCrAlY-YSZ thermal barrier coatings10.1016/j.surfcoat.2023.129947 ↗
48. Effect of bond coating surface roughness on high-temperature performance of EB-PVD thermal barrier coatings10.1016/j.ceramint.2025.01.267 ↗
49. Evaluation of microstructure, mechanical and corrosion properties of IN718 superalloy components fabricated by laser direct energy deposition10.1016/j.jallcom.2025.183236 ↗
50. Hot corrosion behavior of HVOF-sprayed carbide based composite coatings for boiler steel
51. Hot corrosion and electrochemical behavior of NiCrAlY, NiCoCrAlY and NiCoCrAlYTa coatings in molten NaCl-Na2SO4 at 800 °C10.1016/j.surfcoat.2022.128503 ↗
52. Singh · 2020 · 27
53. Hot corrosion behaviour of HVOF sprayed Ni 3 Ti and Ni 3 Ti + (Cr 3 C 2 + 20NiCr) coatings in presence of Na 2 SO 4 -40 % V 2 O 5 at hot corrosion behaviour of HVOF sprayed Ni 3 Ti and Ni 3 Ti +
54. Laser surface cladding of CoNiCrAlY as Bond Coat on INCONEL718 substrate for thermal barrier coating application10.1016/j.matlet.2024.136831 ↗
55. Outstanding hot corrosion behavior of Pt modified CoNiCrAl medium-entropy alloy10.1016/j.corsci.2024.112193 ↗
56. Hot corrosion and cyclic oxidation performance of a PtAl2-dispersed (Ni,Pt)Al coating prepared by low-activity high-temperature aluminizing10.1016/j.jallcom.2022.164978 ↗
57. Effect of Pt modification on hot corrosion resistance of NiCrAlYSi+AlY coating at 900 °C
58. High temperature performance and interface evolution of a NiCoCrAlY coating with Pt modification and Re-based diffusion barrier10.1016/j.surfcoat.2023.129510 ↗
59. Studies on corrosion resistance (in 3.56 wt.% NaCl solution) of thermal-sprayed CoNiCrAlY (mechanically milled) on Inconel 718 substrate10.1177/09544062251368718 ↗