Abstract Mechanical properties of KD-I-fiber-reinforced silicon carbide matrix composites were evaluated under monotonic tension at room and elevated temperatures. The measured ultimate strength showed a big decline for uncoated specimens from a room temperature value of 350 MPa, to 220 and 200 MPa at 1100 °C and 1300 °C, respectively. The decrease in ultimate strength at elevated temperatures was believed to be partly due to the oxidation embrittlement and fiber strength degradation. Specimens with anti-oxidation coatings tested at 1300 °C exhibited the ultimate strength of 320 MPa, which was comparable to that tested at room temperature. Scanning electron microscopy was employed to evaluate the in-situ KD-I fiber strengths via fracture mirror size measurements. The analysis indicated that oxidation embrittlement was the dominated damage mechanism leading to the decrease of ultimate strength. Measured values of ultimate strengths of the CMCs were compared with predictions made on the basis of in-situ fiber strength characteristics and available model.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Review the physics and mechanics of fibre reinforced brittle matrix composites10.1007/BF00355946 ↗
2. Mechanical behavior of SiC(f)/SiC composites and correlation to in situ fiber strength at room and elevated temperatures10.1111/j.1151-2916.1996.tb07915.x ↗
3. Davies · Comparison between predicted and experimental stress/strain behavior for a 3-D woven SiC/SiC composite tested between room temperature and 1300°C. · 2002 · 21 · 461
4. Theory of mechanical properties of ceramic-matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
5. In situ fiber strengths in ceramic-matrix composites from fracture mirrors10.1111/j.1151-2916.1994.tb07272.x ↗
6. Mechanical properties of continuous-fiber-reinforced carbon matrix composites and relationships to constituent properties10.1111/j.1151-2916.1992.tb04381.x ↗
7. Mechanical behavior of glass and Blackglas® ceramic matrix composites10.1016/S1359-6454(97)00193-6 ↗
8. Mechanical properties of SiC/SiC composites by PIP process with a new precursor at elevated temperature10.1016/j.msea.2014.03.011 ↗
9. ASTM, Standard Test Method for Monotonic Tensile Behavior of Continuous Fiber-Reinforced Advanced Ceramics with Solid Rectangular Cross-Section Test Specimens at Ambient Temperature, in C1275-10. 2010.
10. ASTM, Standard Test Method for Monotonic Tensile Strength Testing of Continuous Fiber Reinforced Advanced Ceramics With Solid Rectangular Cross-Section Test Specimens at Elevated Temperatures, in C1359-11. 2011.
11. Models of high-temperature, environmentally assisted embrittlement in ceramic-matrix composites10.1111/j.1151-2916.1996.tb08982.x ↗
12. Subcritical crack growth processes in SiC/SiC ceramic matrix composites10.1016/j.jeurceramsoc.2004.12.015 ↗
13. Backhaus-Ricoult · Two-dimensional SiC-C-SiC(O)fibre composite · 1995 · 30 · 3487
14. Fibre strength parameters measured in situ for ceramic-matrix composites tested at elevated temperature in vacuum and in air10.1016/S0266-3538(99)00011-1 ↗
15. Mirror constant for Tyranno® silicon–titanium–carbon–oxygen fibers measured in situ in a three-dimensional woven silicon carbide/silicon carbide composite10.1111/j.1151-2916.2002.tb00151.x ↗
16. In-plane mechanical properties of several ceramic-matrix composites10.1111/j.1151-2916.1995.tb08618.x ↗
17. In-plane cracking behavior and ultimate strength for 2D woven and braided melt-infiltrated SiC/SiC composites tensile loaded in off-axis fiber directions10.1111/j.1551-2916.2007.01887.x ↗