Bio-inspired crack self-healing of SiC/spinel nanocomposite
Source abstract
Abstract
Abstract Crack self-healing behavior of SiC/spinel nanocomposite, obtained from talc, aluminum and graphite powders was evaluated as a function of time, temperature and the environment atmosphere. The mechanism that was involved in the crack-healing was investigated and the outcome revealed both physical and chemical phenomena are involved in the healing process. In the presence of oxygen at high temperatures, SiC reacts with oxygen to form SiO 2 which is accompanied with about 80% volume expansion. On the other hand, the formed silica reacts with the matrix and produces some transition compounds which can rebond crack walls together. The results showed that cracks can be completely healed after heat treatment at 1545 °C in static air for only 1 min.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Microbial Applications in Construction Materials · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Routes and mechanisms towards self healing behavior in engineering materials
2. High temperature mechanical properties of ceramic materials: I, magnesium dititanate10.1111/j.1151-2916.1958.tb13539.x ↗
3. Temperatures, thermal stresses and displacements in solid uranium dioxide rods, Brit
4. Crack-healing behavior of monolithic alumina and strength of crack-healed member10.2472/jsms.52.667 ↗
5. Crack healing and strengthening of thermally shocked alumina10.1111/j.1151-2916.1976.tb10949.x ↗
6. Healing of surface cracks in polycrystalline Al2O310.1111/j.1151-2916.1970.tb12148.x ↗
7. Crack healing by heat treatment10.1111/j.1151-2916.1970.tb12002.x ↗
8. Crack healing in thermally shocked MgO10.1111/j.1151-2916.1975.tb19578.x ↗
9. In situ study of the recovery of nanoindentation deformation of the (100) face of MgO crystals by atomic force microscopy10.1016/S0039-6028(99)00909-7 ↗
10. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
11. Oxidation-induced crack healing in Zr2Al4C5 ceramic10.1016/j.matdes.2009.02.024 ↗
12. Crack healing behavior of silicon carbide ceramics10.1111/j.1151-2916.2000.tb01632.x ↗
13. Fatigue strength of crack-healed Si3N4/SiC composite ceramics10.1046/j.1460-2695.1999.00210.x ↗
14. A preliminary study on crack healing behavior of Si3N4/SiC composite ceramics10.1046/j.1460-2695.1998.00052.x ↗
15. Crack-healing and oxidation behavior of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
16. Hünecke · 1997
17. Erhabor · 2013
18. Synthesis, characterization and formation mechanism of SiC/spinel nanocomposite10.1016/j.jallcom.2014.02.047 ↗
19. Sintering behavior, microstructure and mechanical properties of vacuum sintered SiC/spinel nanocomposite10.1016/j.jallcom.2014.06.173 ↗
20. High-temperature oxidation, reduction and volatilization reactions of silicon and silicon carbide10.1007/BF00613092 ↗
21. Brittle materials design, high temperature gas turbine
22. Aqueous synthesis of forsterite (Mg2SiO4) and enstatite (MgSiO3)10.1023/A:1015332607551 ↗
23. Effects of fluorine ion and mechanical activation on nanostructure forsterite formation mechanism10.1016/j.powtec.2010.05.007 ↗
24. Effects of mechanical activation and chlorine ion on nanoparticle forsterite formation10.1016/j.matlet.2010.09.038 ↗
25. Synthesis, characterization and formation mechanism of single-phase nanostructure bredigite powder10.1016/j.msec.2011.10.007 ↗
26. Mechanochemical synthesis of single phase nanocrystalline forsterite powder10.1142/S0217979210053987 ↗