journal article·2003-01

Wear in metal/silicon nitride sliding pairs

G. Akdogan, T.A. Stolarski

Ceramics International· Volume 29· Issue 4
Publisher page

Abstract

Ball-on-rotating disc tests were conducted to assess the relative wear behaviour of various disc materials in contact with silicon nitride under lubricated environment at room temperature high load and high speed conditions. Some selected tests were also performed under unlubricated conditions for comparison. The discs were made of grey cast iron, Al-bronze, bronze, aluminium and stainless steel. The lubricant was commercial additive free mineral base oil having a viscosity grade of 68. The applied normal load ranged between 16 and 300 N. The sliding speed changed from 0.5 to 4.0 m/s. The behaviour of grey cast iron and Al-bronze in sliding contact with silicon was characterised by a decrease in wear with an increase in sliding speed. Bronze and aluminium experienced very high wear rates as sliding speed increased. Stainless steel exhibited high wear and also caused significant damage to silicon nitride. Severity of wear between stainless steel and silicon nitride increased with the speed. High wear occurred at both low and high sliding speeds, which were accompanied by high wear track temperatures on the disc surface. This phenomenon resulted in considerable wear on both mating surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Wear Analysis · Lubricants and Their Additives · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Metallic film transfer during metal–ceramic unlubricated sliding10.1016/0043-1648(89)90084-7 ↗
2. Wear mechanism of ceramic tools10.1016/0043-1648(93)90425-L ↗
3. S. Sasaki, The effects of surrounding atmosphere in friction and wear, in: K.C. Ludema (Ed.), Proc. Int. Conf. on Wear of Materials, ASME, 1989, pp. 409–417.10.1016/S0167-8922(08)70213-X ↗
4. Effect of selected chemical compounds on the lubrication of silicon nitride10.1080/10402009108982052 ↗
5. The lubricated wear of ceramics10.1016/0301-679X(95)00024-X ↗
6. Effect of antiwear additives on the friction and wear of Si3N4 sliding contacts10.1016/S0043-1648(96)07215-8 ↗
7. Use of ceramic tools when machining nickel bas aerospace alloys10.1179/mst.1986.2.7.700 ↗
8. S.K. Samanta, et al., Method of Using Si3N4 System for Machining Cast Iron, US Patent 4,323,325, 6 April, 1982.
9. Chemical interaction between a sialon cutting tool and iron based alloys10.1016/0921-5093(94)90345-X ↗
10. Tribological behaviour of silicon nitride materials under unlubricated sliding between 22 °C and 1000 °C
11. High temperature friction and wear testing of silicon nitride ceramics10.1016/0301-679X(95)00020-5 ↗
12. Limitation on the use of ceramics in unlubricated sliding applications due to transfer layer formation10.1016/0043-1648(94)90162-7 ↗
13. Unlubricated sliding wear mechanism of fine ceramic Si3N4 against high chromium cast iron10.1016/0301-679X(94)90029-9 ↗
14. An investigation on component and formation of tribochemical film in Si3N4/white iron sliding pair lubricated with distilled water10.1016/S0301-679X(97)00057-1 ↗