Joining of silicon nitride with a Cu76.5Pd8.5Ti15 filler alloy
Source abstract
Abstract
Abstract Si3N4 ceramic has been joined successfully to itself by brazing in a vacuum at 1373–1573 K holding for 1.8 ks using a Cu76.5Pd8.5Ti15 alloy filler. By observation and analysis of the microstructure of the joints, it is found that the joints comprise three parts: (1) a continuous reaction layer of TiN between Si3N4 and filler alloy, (2) a discontinuous reaction layer containing TiN, Pd2Si and Ti5Si3 connecting the continuous reaction layer, and (3) the Cu-based solid solution in the mid of the joint and some reaction products (TiN, Pd2Si, PdTiSi and Ti5Si3) in the solution. With increasing brazing temperature, both the thickness of the continuous reaction layer and amount of reaction phases increase, which improves the bending strength of the joints. When the brazing temperature surpasses 1473 K, voids are formed in the joint because of the decomposition of the Si3N4 ceramic, leading to a decrease of the bond strength. The room-temperature bending strength of the joint brazed at 1423 K reaches a maximum value of 155.8 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · Material Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. The wetting, reaction and bonding of silicon nitride by Cu–Ti alloys10.1007/BF01124666 ↗
2. Silicon nitride-stainless steel brazed joining with an active filler metal10.1007/BF00354573 ↗
3. Ag effect on microstructures and strength of Si3N4/Si3N4 joint brazed with Cu–Ag–Ti filler metals
4. Study of the reactive brazing of a silicon nitride to steel using ternary Ag–Cu–Ti: microstructures and mechanical strength of the bonds10.1080/09603409.1994.11752533 ↗
5. Evaluation of brazed silicon nitride joints: microstructure and mechanical properties10.1111/j.1151-2916.1996.tb08764.x ↗
6. Joining silicon nitride ceramic using a composite powder as active brazing alloy10.1016/j.msea.2003.10.276 ↗
7. Metal-ceramic interfaces: joining silicon nitride-stainless steel10.1016/j.apsusc.2004.05.290 ↗
8. Joining of silicon nitride with a titanium foil interlayer10.1016/S0921-5093(02)00892-4 ↗
9. Joining of silicon nitride by interposing metal foils: effect of temperature and bonding pressure10.4028/www.scientific.net/MSF.426-432.4075 ↗
10. Effect of adhesive composition on bonding of silicon nitride ceramic10.1016/S0272-8842(02)00118-9 ↗
11. Joining Si3N4-based ceramics with oxidation-formed surface layers
12. Heat-resistant active brazing of silicon nitride. Part 2: metallurgical characterization of the braze joint
13. Ceramic to metal joints brazed with palladium alloys
14. Recent process in ceramic joining10.4028/www.scientific.net/KEM.161-163.657 ↗
15. The reactive route to ceramic joining: fabrication, interfacial chemistry and joint properties
16. Y.J. Liang, Y.C. Che, Thermodynamic Data Manual for Inorganic Matter, The Northeastern University Press, 1993.
17. Titanium metallization of Si3N4 ceramic by molten salt reaction: mechanism and interfacial structure10.1023/A:1004850605285 ↗
18. Y.W. Ren, Technology of brazing in vacuum, Mechanical Engineering Publishing House, 1993, pp. 12–20 (in Chinese).
19. He · 1983