Wear mechanisms of TiN–TiB2 ceramic in sliding against alumina from room temperature to 700°C

Zhen-Lin Yang, Jia-Hu Ouyang, Zhan-Guo Liu, Xue-Song Liang

Ceramics International· Volume 36· Issue 7
Publisher page

Abstract

Abstract TiN–TiB 2 ceramic was prepared by the reactive hot-pressing method using titanium and BN powders as raw materials. The friction and wear properties of TiN–TiB 2 ceramic were evaluated in sliding against alumina ball from room temperature to 700 °C in air. The TiN–TiB 2 ceramic has a relative density of 98.6%, a flexural strength of 731.9 MPa and a fracture toughness of 8.5 MPa m 1/2 at room temperature. The TiN–TiB 2 ceramic exhibits a distinct decrease in friction coefficient at 700 °C as contrasted with the friction data obtained at room temperature and 400 °C. Wear mechanisms of TiN–TiB 2 ceramic depend mainly upon testing temperature at identical applied loads. Lubricious oxidized products caused by thermal oxidation provide excellent lubrication effects and greatly reduce the friction coefficient of TiN–TiB 2 ceramic at 700 °C. However, abrasive wear and tribo-oxidation are the dominant wear mechanisms of TiN–TiB 2 ceramic at 400 °C. Mechanical polishing effect and removal of micro-fractured grains play important roles during room-temperature wear tests.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Resistance of titanium diboride to high-temperature plastic yielding10.1111/j.1151-2916.1985.tb09637.x ↗
2. Transient plastic phase processing of titanium–boron–carbon composites10.1111/j.1151-2916.1993.tb03924.x ↗
3. Microstructural evolution during transient plastic phase processing of titanium carbide–titanium boride composites10.1111/j.1151-2916.1996.tb08017.x ↗
4. Combustion synthesis of TiN–TiB2 composites in Ti/BN/N2 and Ti/BN/B reaction systems10.1016/j.jallcom.2005.12.086 ↗
5. Production of TiB2–TiN composites by combustion synthesis and their properties10.1111/j.1151-2916.1997.tb02894.x ↗
6. Synthesis of dense TiB2–TiN nanocrystalline composites through mechanical and field activation10.1111/j.1151-2916.2001.tb00818.x ↗
7. Genesis and role of wear debris in sliding wear of ceramics10.1016/S0043-1648(00)00465-8 ↗
8. Reactive hot pressing of titanium nitride–titanium diboride composites at moderate pressures and temperatures10.1111/j.1151-2916.2004.tb06333.x ↗
9. Frictional properties of sintered TiN–TiB2 and Ti(CN)–TiB2 ceramics at high temperature10.1111/j.1151-2916.1987.tb05014.x ↗
10. Densification and mechanical properties of titanium diboride with silicon nitride as a sintering aid10.1111/j.1151-2916.1999.tb02199.x ↗
11. Sliding friction of ceramics: mechanical action of the wear debris
12. Wear resistance of αSiC-TiB2 composites prepared by reactive sintering10.1016/S0955-2219(98)00250-7 ↗
13. Oxidation behavior of titanium nitride films10.1116/1.1914815 ↗
14. Oxidation of monolithic TiB2 and of Al2O3–TiB2 composite10.1007/BF01151240 ↗
15. Influence of high-temperature oxide formation on the tribological behavior of TiN and VN coatings10.1016/j.wear.2006.11.006 ↗
16. Friction and wear test of titanium boride ceramics at elevated temperatures10.2109/jcersj.101.461 ↗
17. Sliding wear of silicon carbide–titanium diboride ceramic–matrix composite10.1111/j.1151-2916.1993.tb03815.x ↗
18. Ambient and 550°C tribological behavior of select MAX phases against Ni-based superalloys10.1016/j.wear.2007.03.011 ↗
19. Lubricated rolling and sliding wear of SiCW/Si3N4 composite against M2 tool steel10.1111/j.1151-2916.1993.tb03695.x ↗
20. Oxidation of monolithic TiB2 and TiB2–20wt.% MoSi2 composite at 850°C10.1016/j.jeurceramsoc.2004.10.025 ↗