journal article·2017-04

Improvement of densification and mechanical properties of MgAl 2 O 4 –CaAl 4 O 7 –CaAl 12 O 19 composite by addition of MnO

Xue-liang Yin, Min Chen, Nan Wang, Lei Xu

Ceramics International· Volume 43· Issue 5
Publisher page

Abstract

Abstract Composites containing spinel (MgAl 2 O 4 ) and calcium hexaluminate (CaAl 12 O 19 ) can excellently combine the properties of these two phases. However, their fabrication in dense composites for structural applications is limited on account of the poor sinterability. Considering this aspect, the effect of MnO addition on the sintering, microstructure and mechanical properties of MgAl 2 O 4 -CaAl 4 O 7 -CaAl 12 O 19 composite was investigated by solid state reaction sintering at 1500–1600 °C. The results showed that the grain growth of MA was significantly promoted due to the formation of Mg(Mn)Al 2 O 4 by introducing MnO. The addition of MnO can also weaken the barrier effect of the elongated CA 6 grains, indirectly promoting the development of MA and CA 2 grains. Accordingly, highly uniform and dense microstructures were formed, with the apparent porosity decreased from 18.3% to 3.4% when adding 6 wt% MnO at 1600 °C. Significant improvements in the mechanical properties were also achieved for the MnO added composites sintered at this temperature. The optimum flexural strength was obtained by adding 6 wt% MnO, achieving an increase from 186 to 308 MPa, while the optimum fracture toughness was obtained by adding 4 wt% MnO, with the value increased from 2.3 to 3.5 MPa m 1/2 .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. High-temperature mechanical behavior of stoichiometric magnesium spinel10.1111/j.1151-2916.1995.tb08900.x ↗
2. Effect of preformed and in situ spinels on microstructure and properties of a low cement refractory castable10.1016/S0272-8842(03)00117-2 ↗
3. An efficient MgAl2O4 spinel additive for improved slag erosion and penetration resistance of high-Al2O3 and MgO-C refractories10.1016/S0272-8842(01)00086-4 ↗
4. Spinel-containing alumina-based refractory castables10.1016/j.ceramint.2011.03.049 ↗
5. D. Son, Y. Kim, J. Yang, The application of magnesia-spinel castable to the snorkel in the RH degasser, in: Proceedings of the UNITECER, New Orleans, LA, 1997, pp. 24–26.
6. Grain growth in sintered MgAl2O4 spinel10.1023/A:1018585105949 ↗
7. Studies on densification, mechanical, micro-structural and structure–properties relationship of magnesium aluminate spinel refractory aggregates prepared from Indian magnesite10.1016/j.matchar.2014.11.020 ↗
8. The CaO-Al2O3 system in a moisture-free atmosphere
9. Microstructure development in calcium hexaluminate10.1016/S0955-2219(00)00143-6 ↗
10. R-curve behavior of in-situ-toughened Al2O3: CaAl12O19 ceramic composites10.1111/j.1151-2916.1996.tb08088.x ↗
11. Control of calcium hexaluminate grain morphology in in-situ toughened ceramic composites10.1007/BF00354672 ↗
12. Self-reinforced Ca-hexaluminate/alumina composites with graded microstructures10.1016/j.ceramint.2006.10.001 ↗
13. Calcium hexaaluminate synthesis and its influence on the properties of CA2–Al2O3-based refractories10.1016/j.jeurceramsoc.2015.08.034 ↗
14. The influence of in-situ formation of hibonite on the properties of zirconia toughened alumina (ZTA) composites10.1016/j.ceramint.2013.11.076 ↗
15. Influence of Fe3+ on the sintering and microstructural evolution of reaction sintered calcium hexaluminate10.1016/S0955-2219(98)00067-3 ↗
16. Ternary system Al2O3–MgO–CaO: I, primary phase field of crystallization of spinel in the subsystem MgAl2O4–CaAl4O7–CaO–MgO10.1111/j.1151-2916.1999.tb02062.x ↗
17. Low-temperature synthesis of calcium–hexaluminate/magnesium–aluminum spinel composite ceramics10.1016/j.jeurceramsoc.2015.03.041 ↗
18. Novel calcium hexaluminate/spinel-alumina composites with graded microstructures and mechanical properties10.1038/srep04333 ↗
19. Effect of ZrO2 addition on densification and mechanical properties of MgAl2O4–CaAl4O7–CaAl12O19 composite10.1111/jace.13955 ↗
20. Effect of TiO2 addition on the sintering densification and mechanical properties of MgAl2O4–CaAl4O7–CaAl12O19 composite10.1016/j.ceramint.2016.03.082 ↗
21. Effect of addition of TiO2 on reaction sintered MgO–Al2O3 spinels10.1016/S0955-2219(00)00097-2 ↗
22. The effect of ZnO addition on the densification and properties of magnesium aluminate spinel10.1016/S0272-8842(99)00104-2 ↗
23. Effect of additives on the sintering of MgAl2O410.1016/j.jallcom.2013.10.250 ↗
24. Effect of ZrO2 addition on MgAl2O4 spinel from commercial grade oxide reactants10.1016/j.ceramint.2016.03.167 ↗
25. A comparative study on the effect of different additives on the formation and densification of magnesium aluminate spinel10.1016/j.ceramint.2016.05.206 ↗
26. Kingery · 1960
27. Stress intensity factor, compliance and CMOD for a general three-point-bend beam10.1023/A:1007498132504 ↗
28. Aluminum titanate-calcium dialuminate composites with low thermal expansion and high strength10.1016/j.jallcom.2015.09.237 ↗
29. Hexaluminates as a cleavable fiber-matrix interphase: synthesis, texture development, and phase compatibility10.1016/S0955-2219(99)00255-1 ↗
30. Rahaman · 2003
31. Porosity dependence of physical properties of materials: a summary review10.4028/www.scientific.net/KEM.115.1 ↗
32. Lawn · 1993
33. Fracture behaviour of alumina–calcium hexaluminate composites obtained by colloidal processing10.1016/S0955-2219(00)00123-0 ↗
34. Thermomechanical properties and fracture mechanisms of calcium hexaluminate10.1016/S0955-2219(00)00274-0 ↗