journal article·2016-01

Oxidation behavior of sintered tubular silicon carbide in pure steam Ι: Experiments

Youho Lee, Thomas J. McKrell, Aline Montecot, Michael Pantano, Yann Song, Mujid S. Kazimi

Ceramics International· Volume 42· Issue 1
Publisher page

Abstract

Abstract Experimental investigations are conducted on sintered tubular SiC in oxidizing environments containing pure steam at 1 atm with temperature range of 1140–1500 °C and velocity between 0.8 and 10 m/s. Linear weight loss was observed with time. The linear weight loss rates exhibit sensitive dependence on flow rate at a given temperature, demonstrating effects of flow boundary-layer diffusion rate on silica volatilization kinetics. Silica scale exhibits morphology change with respect to exposure time in an oxidizing environment, progressively demonstrating bubble formation and surface smoothing, extensive formation of cracks and pores, and crack reduction. Yet, strength measurements of pressure-less sintered SiC show no significant change after oxidation in the tested conditions. Hence, the primary life-time limiting factor for structural application of pressure-less sintered SiC in the tested environments is anticipated to be the loss of the material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Thermodynamic analysis of the high-temperature stability of silicon nitride and silicon carbide10.1016/0390-5519(76)90022-3 ↗
2. SiO(g) formation from SiC in mixed oxidizing-reducing gases10.1007/BF01051042 ↗
3. Passivity during the oxidation of silicon at elevated temperatures10.1063/1.1723429 ↗
4. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
5. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe–Cr alloys10.1149/1.2424115 ↗
6. SiC recession caused by SiO2 conditions: II, thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
7. Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
8. Arnold · 2011
9. Advanced treatment of zircaloy cladding high-temperature oxidation in severe accident code calculations Part I. Experimental database and basic modeling10.1016/j.nucengdes.2004.02.013 ↗
10. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
11. Material properties of a sintered α-SiC10.1063/1.556000 ↗
12. Effects of high water–vapor pressure on oxidation of silicon carbide at 1200°C.10.1111/j.1151-2916.2003.tb03460.x ↗
13. Variation of the oxidation rate of silicon carbide with water–vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
14. Oxydation of silicon carbide in oxygen and in water vapour at 1500°C10.3891/acta.chem.scand.35a-0247 ↗
15. Silicon oxidation studies: roles of H2O10.1149/1.2133151 ↗
16. High-temperature oxidation of chemically vapor-deposited silicon carbide in wet oxygen at 1823 to 1923K10.1111/j.1151-2916.1990.tb04261.x ↗
17. High-temperature passive oxidation of chemically vapor deposited silicon carbide10.1111/j.1151-2916.1989.tb07658.x ↗
18. Development of oxide scale microstructure on single-crystal SiC10.1007/BF02402838 ↗
19. Kinetics of crystallization of stoichiometric SiO2 Glass in H2O atmospheres10.1111/j.1151-2916.1966.tb15387.x ↗
20. Some new perspectives on oxidation of silicon carbide and silicon nitride10.1111/j.1151-2916.1991.tb04348.x ↗
21. Oxidation kinetics of hot-pressed and sintered α-Sic10.1111/j.1151-2916.1981.tb10297.x ↗
22. Oxidation kinetics of silicon carbide crystals and ceramics: I, in dry oxygen10.1111/j.1151-2916.1986.tb07470.x ↗
23. Oxidation kinetics of hot-pressed silicon carbide10.1007/BF00545142 ↗
24. Bubble formation in oxide scales on SiC
25. Effects of gaseous corrosion on the strength of SiC and Si3N4
26. Strength distributions of SiC ceramics after oxidation and oxidation under load10.1111/j.1151-2916.1981.tb15896.x ↗
27. E. Minford, J.A. Costello, I.S. Tsong, R.E. Tressler, Oxidation effects on crack growth and blunting in SiC ceramics, in: R.C. Bradt, A.G. Evans, D.P. Hasselman, F.F. Lange (Eds.), Fracture Mechanics of Ceramics, 6, 1983, 511–522.
28. R.E. Tressler, Environmental effects on long term reliability of SiC and Si3N4 ceramics, in: R.E. Tressler, M. McNallan (Eds.), CeramicTransacions, 10: Corrosion and Corrosive Degradation of Ceramics, 1990, 99–124.
29. Thermal shock fracture of tot silicon carbide immersed in water10.1016/j.jnucmat.2015.09.020 ↗
30. Failure probabilities of SiC clad fuel during a LOCA in public acceptable simple SMR (PASS)10.1016/j.nucengdes.2015.05.023 ↗
31. A structural model for multi-layered ceramic cylinders and its application to silicon carbide cladding of light water reactor fuel10.1016/j.jnucmat.2014.12.013 ↗
32. Thermal shock fracture of silicon carbide and its application to LWR fuel cladding performance during reflood10.5516/NET.02.2013.528 ↗
33. Safety assessment of SiC cladding oxidation under loss of coolant accident (LOCA) conditions in LWRs10.13182/NT12-122 ↗
34. Youho. · 2013
35. Carpenter · 2007
36. Carpenter · 2010
37. Stempien · 2011
38. Dobisesky · 2011
39. Bloore · 2013
40. Snead · J. Nucl. Mater. · 2007 · 371 · 32910.1016/j.jnucmat.2007.05.016 ↗
41. Snead · J. Nucl. Mater. · 2011 · 417 · 33010.1016/j.jnucmat.2011.03.005 ↗
42. Snead · J. Nucl. Mater. · 2014 · 448 · 38910.1016/j.jnucmat.2013.09.056 ↗
43. Terrani · J. Am. Ceram. Soc. · 2014 · 97 · 233110.1111/jace.13094 ↗
44. Terrani · J. Nucl. Mater. · 2015 · 465 · 48810.1016/j.jnucmat.2015.06.019 ↗
45. Zinkle · J. Nucl. Mater. · 2014 · 448 · 37410.1016/j.jnucmat.2013.12.005 ↗
46. Ben-Belgacem · J. Nucl. Mater. · 2014 · 447 · 12510.1016/j.jnucmat.2014.01.006 ↗
47. Pint · J. Nucl. Mater. · 2013 · 440 · 42010.1016/j.jnucmat.2013.05.047 ↗
48. Kim · J. Nucl. Mater. · 2015 · 458 · 2910.1016/j.jnucmat.2014.11.117 ↗