SiC–YAG sintered composites from hydroxy hydrogel powder precursors
Source abstract
Abstract
Abstract Yttrium hydroxide and aluminium hydroxide hydrogel were derived from yttrium nitrate and aluminium nitrate through hydroxy hydrogel route in which SiC particles were kept dispersed. The gel-like mass was heat treated at 900°C in ambient atmosphere followed by heat treatment at 1400°C in Ar atmosphere. The specimens were then sintered in the temperature range of 1800–1950°C in Ar atmosphere with 30 min soaking. The phases were identified by XRD analysis. Microstructure of the sintered materials were analysed by scanning electron micrograph. With this new method of preparation of powder precursors, the process of sintering was easier and almost theoretical density was achieved with moderate hardness. The mechanism of densification was postulated to be a solid-state initiated liquid phase sintering and the overall process of which was activated by the reactive species formed from hydroxy hydrogel powder precursors.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Pressured–sintered silicon carbide10.1111/j.1151-2916.1956.tb15609.x ↗
2. H. Tanaka, Sintering of silicon carbide, in: S. Somaiya, Y. Inomata (Eds.), Silicon Carbide Ceramics, Elsevier Applied Science, London, 1991, pp. 213–238.10.1007/978-94-011-3842-0_10 ↗
3. Obtention of highly dispersed platelet-reinforced Al2O3 composites10.1007/BF00356591 ↗
4. Silicon carbide platelet alumina composites10.1111/j.1151-2916.1992.tb04432.x ↗
5. Processing and mechanical properties of a silicon carbide platelet alumina matrix composite10.1016/0955-2219(94)90067-1 ↗
6. Silicon carbide platelet alumina composites10.1111/j.1151-2916.1993.tb03925.x ↗
7. Silicon carbide platelet/alumina composites10.1111/j.1151-2916.1993.tb08321.x ↗
8. W.F. Fischer, R.A. Haber, R.M. Anderson, Mechanical properties of alumina matrix composites reinforced with silicon carbide platelets and particulate, in: Ceramic Transactions 19, Advanced Composite Materials, 1991, pp. 773–779.
9. Fracture resistance of a silicon carbide platelet reinforced alumina composite
10. H. Sakai, K. Matsuhiro, Y. Furuse, Mechanical properties of SiC platelet reinforced ceramic composites, Ceramic Transactions 19, Advanced Composite Materials, 1991, pp. 765–771.
11. SiC platelet reinforced alumina composites, Silicates Industries
12. Slow crack growth in SiC plalelet reinforced alumina composite10.1016/1359-6462(96)00026-7 ↗
13. M. Belmonte, J.R. Jurado, D. Trehux, P. Miranzo, Role of triboelectrification mechanism in the wear behaviour of Al2O3/SiC platelet composites, Wear 199 (1) (1996) 54–59.10.1016/0043-1648(96)07210-9 ↗
14. Pressureless sintering of SiC10.1111/j.1151-2916.1982.tb10460.x ↗
15. Kostic · Powder Metall. Int. · 1988 · 20 · 28
16. M.B. Trigg, Australian Patent 00518, 1990.
17. M. Omori et al., US Patent 4 564 490, 1986.
18. K. Suzuki, in: S. Somaiya, Y. Inomata (Eds.), in: Silicon Carbide Ceramics, Vol. 2, Elsevier Applied Science, London, 1991, pp. 163–182.
19. M.B. Trigg, Australian Patent 00271, 1988.
20. W.D.G. Bocker, European Patent 419271 A2, 1990.
21. SiC ceramics with improved strength
22. Hamminger · J. Hard Mater. · 1992 · 3 · 93
23. Mulla · Ceram. Bull. · 1990 · 70 · 439
24. R.A. Cutler, T.B. Jackson, in: V.J. Tennery (Ed.), Ceramic Materials and Components for Engines, Am. Ceram. Soc. Inc., Columbus, OH, 1989, pp. 309–318a.
25. Kratohvil · Adv. Ceram. Mater. · 1987 · 2 · 79810.1111/j.1551-2916.1987.tb00150.x ↗
26. Grag · J. Colloidal Interface Sci. · 1988 · 126 · 64510.1016/0021-9797(88)90168-3 ↗
27. Kawahashi · J. Colloidal Interface Sci. · 1990 · 138 · 53410.1016/0021-9797(90)90235-G ↗
28. Synthesis of hydrous SnO2 and SnO2-coated TiO2 powder by the homogeneous precipitation method and their characterisation10.1007/BF01174698 ↗
29. Particulates composites from coated powders10.1016/0955-2219(91)90057-7 ↗
30. Garg · J. Mater. Res. · 1990 · 5 · 13610.1557/JMR.1990.0136 ↗
31. Preparation of alumina hydrate-coated SiC whisker — effect of reaction condition on the morphology of coated body10.2109/jcersj.101.773 ↗
32. Microencapsulation of silicon nitride particles with yttria and yttria–alumina precursors10.1557/JMR.1990.0136 ↗
33. Fabrication of mullite and mullite-matrix composites by transient viscous sintering of composite powder10.1111/j.1151-2916.1991.tb06780.x ↗
34. The role of boron and carbon in the sintering of silicon carbide
35. Liquid phase sintered silicon carbide
36. Processing of liquid phase sintered SiC — Mechanical and wear properties
37. A. K. Samanta, K. K. Dhargupta, S. Ghatak, Retention of SiC during development of SiC–MxSiyOz composites [M=Al, Zr, Mg] by reaction bonding in air, J. Eur. Ceram. Soc. 20 (12) (2000) 1883–1894.10.1016/S0955-2219(00)00082-0 ↗
38. Homogeneous distribution of sintering additives in liquid-phase sintered silicon carbide10.1111/j.1151-2916.1995.tb08886.x ↗
39. Microstructural development during liquid phase sintering of silicon carbide ceramics10.1016/S0955-2219(96)00198-7 ↗
40. Core/rim structure of liquid-phase sintered silicon carbide10.1111/j.1151-2916.1993.tb03677.x ↗
41. Microstructural development and mechanical properties of pressureless sintered SiC with plate-like grains using Al2O3–Y2O3 additives10.1007/BF01171542 ↗
42. Low-temperature pressureless sintering of β-SiC with aluminium oxide and yttrium oxide additives
43. High temperature phase instability in yttrium orthoaluminate10.1007/BF00550075 ↗