journal article·2008-05

Thickness effects on structures and electrical properties of lead zirconate titanate thick films

Peng Lin, Wei Ren, Xiaoqing Wu, Peng Shi, Xiaofeng Chen, Xi Yao

Ceramics International· Volume 34· Issue 4
Publisher page

Abstract

Abstract PbZr 0.52 Ti 0.48 O 3 thick films with thickness of 1–6 μm have been prepared by a polymer-assisted MOD process. The polymer, poly(vinyl acetate) (PVAc) was introduced into PZT precursor solutions. The grain size increased from 30 nm to 100 nm with an increase of the additive amount of PVAc. Meanwhile, the grains grew larger (in a range of 100–500 nm) and the surface of the films became rougher with increasing film thickness. This promotes the structural relaxation and prevents cracking formation. The critical thickness at which the film begins to crack increases significantly. The dielectric constant and remanent polarization ( P r ) increased from 1070 to 1490 and from 36.1 μC/cm 2 to 52.4 μC/cm 2 , respectively, and the coercive field ( E c ) decreased from 57.3 kV/cm to 41.3 kV/cm as the film thickness increased from 0.95 μm to 6.02 μm. PZT thick films prepared in this study are promising materials for MEMS applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Micromachined high frequency ferroelectric sonar transducers, ieee transactions on ultrasonics10.1109/58.655620 ↗
2. Fabrication and characterization of PZT thin-film vibrators for micromotors10.1016/0924-4247(95)00994-9 ↗
3. Design of a novel thin-film piezoelectric accelerometer10.1016/S0924-4247(96)01324-6 ↗
4. Piezoelectric and ferroelectric properties of 1-μm-thick lead zirconate titanate film fabricated by a double-spin-coating process10.1063/1.1794354 ↗
5. Sol–gel preparation of single-layer, 0.75μm thick lead zirconate titanate films from lead nitrate-titanium and zirconium alkoxide solutions containing polyvinylpyrrolidone10.1063/1.1419042 ↗
6. Single-step deposition of gel-derived lead zirconate titanate films: critical thickness and gel film to ceramic film conversion10.1111/j.1151-2916.2002.tb00516.x ↗
7. PVP-assisted sol–gel deposition of single layer ferroelectric thin films over submicron or micron in thickness10.1016/S0955-2219(03)00402-3 ↗
8. Polymer-assisted deposition of metal-oxide films10.1038/nmat1163 ↗
9. Preparation of perovskite Pb(Zn1/3Nb2/3)O3-based thin films from polymer-modified solution precursors10.1063/1.2171801 ↗
10. Single-step dip coating of crack-free BaTiO3 films >1μm thick: effect of poly(vinylpyrrolidone) on critical thickness10.1111/j.1151-2916.2000.tb01330.x ↗
11. Crack-free thick ceramic coating films via non-repetitive dip-coating using polyvinylpyrrolidone as stress-relaxing agent10.1023/A:1008780120351 ↗
12. Domain wall motion and its contribution to the dielectric and piezoelectric properties of lead zirconate titanate films10.1063/1.1325005 ↗