Experimental study on the impact resistance of 2D plain-woven C/SiC composite
Source abstract
Abstract
Abstract As a typical ceramic–matrix composite, the C/SiC composite has been widely applied in the Thermal Protective Structure (TPS) of spacecraft, which will inevitably suffer the external impact in service. In this work, the impact resistance of 2D plain-woven C/SiC composite and 2A12 Aluminum alloy plates have been studied. The damage mechanisms under impact load are investigated by measuring the free surface velocity, recording the debris clouds and metering the damage areas of the target plates. Experimental results indicate that the damage of C/SiC composite is just confined in a local area around the impact point, and the critical penetrating energy of 3 mm C/SiC plate is assessed to be 2.66 J. In addition, we found fiber fracture and matrix powdering are the two major energy conversion forms. All these results can provide useful reference to obtain the dynamic response of C/SiC composite and to further design heat-resistant performance of the damaged TPS.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Velocity Impact and Material Behavior · Advanced ceramic materials synthesis · Mechanical Behavior of Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. C/SiC based rigid external thermal protection system for future reusable launch vehicles: generic shingle, pre-X/FLPP anticipated development test studies
2. Short time oxidation behavior and residual mechanical properties of C/C composites modified by in situ grown carbon nanofibers10.1016/j.ceramint.2014.03.057 ↗
3. A double layer nanostructure SiC coating for anti-oxidation protection of carbon/carbon composites prepared by chemical vapor reaction and chemical vapor deposition10.1016/j.ceramint.2012.11.104 ↗
4. Degradation behaviour of C/C composites by atomic oxygen irradiation10.3724/SP.J.1077.2013.12622 ↗
5. Fabrication and characteristic of non-oxide fiber tow reinforced silicon nitride matrix composites by low temperature CVI process10.1016/j.ceramint.2014.01.053 ↗
6. Laser ablation behavior and mechanism of C/SiC composite10.1016/j.ceramint.2013.02.012 ↗
7. Oxidation resistant carbon-fiber-reinforced ceramic-matrix composites10.1016/S0266-3538(98)00146-8 ↗
8. Progress in research work of new CMC-SiC
9. Advanced ceramic matrix composite materials for current and future propulsion technology applications10.1016/j.actaastro.2004.05.052 ↗
10. Optimising curvature of carbon fibre-reinforced polymer composite panel for improved blast resistance: finite-element analysis10.1016/j.matdes.2014.01.034 ↗
11. Effect of plate curvature on blast response of carbon composite panels10.1016/j.compstruct.2012.11.036 ↗
12. Experimental and numerical evaluation of bending and tensile behaviour of carbon-fibre reinforced SiC10.1016/j.compositesa.2012.07.017 ↗
13. Development of damage in a 2D woven C/SiC composite under mechanical loading: 1. Mechanical characterization10.1016/S0266-3538(96)00094-2 ↗
14. Development of damage in a 2D woven C/SiC composite under mechanical loading: 2. Ultrasonic characterization10.1016/S0266-3538(96)90008-1 ↗
15. Tensile behavior and microstructural evolution of a carbon/silicon carbide composite in simulated re-entry environments10.1016/j.msea.2007.05.015 ↗
16. Compressive behavior of C/SiC composites over a wide range of strain rates and temperatures10.1016/j.carbon.2013.06.044 ↗
17. Modeling the tensile behavior of unidirectional C/SiC ceramic–matrix composites10.1007/s11029-013-9382-y ↗
18. Interlaminar shear damage mechanisms of a 2D-C/SiC composite at elevated temperature in vacuum10.1016/j.vacuum.2014.02.017 ↗
19. Fatigue hysteresis behavior of cross-ply C/SiC ceramic matrix composites at room and elevated temperatures10.1016/j.msea.2013.08.017 ↗
20. Influence of loading frequency on the room-temperature fatigue of a carbon-fiber/SiC-matrix composite10.1111/j.1151-2916.1993.tb07772.x ↗
21. Oxidation effects on the mechanical properties of 2D woven C/SiC composites10.1016/0955-2219(94)90105-8 ↗
22. Damage behavior of 2D C/SiC composites under low velocity impact10.3724/SP.J.1077.2010.00311 ↗
23. Experimental and numerical investigation on hypervelocity impact response of 2D plain-woven C/SiC composite