Abstract
Abstract ZrB 2 –SiC–ZrN composites were fabricated by reactive hot pressing using Zr, Si 3 N 4 , and B 4 C powders as starting materials. Sintering was conducted at temperatures of 1800 to 2000 °C under a load of 20 MPa in Ar atmosphere. The composite was densified at 2000 °C. The in situ formed BN flakes which distributed uniformly at the grain boundaries were identified by X-ray diffraction and scanning electron microscopy. The formation of h- BN phase and its effect on the mechanical properties of the composite are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Materials for ultrahigh temperature structural applications
2. Oxidation-based materials selection for 2000 degrees C plus hypersonic aero surfaces: Theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
3. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
4. High-temperature bending strength, internal friction and stiffness of ZrB2-20vol% SiC ceramics10.1016/j.jeurceramsoc.2012.01.035 ↗
5. Properties of a pressureless-sintered ZrB2–MoSi2 ceramic composite10.1111/j.1551-2916.2006.00999.x ↗
6. Pressureless sintering and physical properties of ZrB2-based composites with ZrSi2 additive10.1016/j.scriptamat.2007.11.019 ↗
7. Microstructure and properties of ZrB2–SiC and HfB2–SiC composites fabricated by spark plasma sintering (SPS) using TaSi2 as sintering aid10.2109/jcersj2.118.997 ↗
8. Microstructure and properties of ZrB2–SiC composites prepared by spark plasma sintering using TaSi2 as sintering additive10.1016/j.jeurceramsoc.2010.05.013 ↗
9. Microstructure characterization of ZrB2–SiC composite fabricated by spark plasma sintering with TaSi2 additive10.1016/j.jeurceramsoc.2011.08.024 ↗
10. Pressureless densification of zirconium diboride with boron carbide additions10.1111/j.1551-2916.2006.00949.x ↗
11. Pressureless sintering of zirconium diboride using boron carbide and carbon additions10.1111/j.1551-2916.2007.01936.x ↗
12. High-strength zirconium diboride-based ceramics10.1111/j.1551-2916.2004.01170.x ↗
13. Strong ZrB2–SiC–WC Ceramics at 1600 degrees C10.1111/j.1551-2916.2011.05062.x ↗
14. Elevated temperature thermal properties of ZrB2 with carbon additions10.1111/j.1551-2916.2011.05034.x ↗
15. Beneficial effects of AlN as sintering aid on microstructure and mechanical properties of hot-pressed ZrB210.1002/adem.200300349 ↗
16. Effect of the addition of silicon nitride on sintering behaviour and microstructure of zirconium diboride10.1016/S1359-6462(01)01229-5 ↗
17. Efficacy of HfN as sintering aid in the manufacture of ultrahigh-temperature metal diborides-matrix ceramics10.1557/JMR.2004.0460 ↗
18. Synthesis, microstructure and mechanical properties of (Zr,Ti)B2–(Zr,Ti)N composites prepared by spark plasma sintering10.1016/j.jallcom.2010.01.006 ↗
19. Reactive hot pressing of ZrB2–SiC composites10.1111/j.1151-2916.2000.tb01558.x ↗
20. Low-temperature densification of zirconium diboride ceramics by reactive hot pressing10.1111/j.1551-2916.2006.01299.x ↗
21. Reactive hot pressing of ZrB2–SiC–ZrC ultra high-temperature ceramics at 1800 degrees C10.1111/j.1551-2916.2006.01145.x ↗
22. Reactive hot pressing of ZrB2–SiC–ZrC composites at 1600 degrees C10.1111/j.1551-2916.2008.02507.x ↗
23. ZrB2–MoSi2 composites toughened by elongated ZrB2 grains via reactive hot pressing10.1016/j.scriptamat.2009.04.013 ↗
24. Mechanical properties and microstructure of in situ synthesized ZrB2–ZrN1−x composites10.1007/s10853-006-2870-x ↗
25. Chase · 1998
26. HSC chemistry for Windows 6.1, Outokumpu Research Oy, Pori, Finland.