journal article·2017-01

Microstructure and ablation behavior of double anti-oxidation protection for carbon-bonded carbon fiber composites

Baosheng Xu, Yumin An, Peng Wang, Xinxin Jin, Guangdong Zhao

Ceramics International· Volume 43· Issue 1
Publisher page

Abstract

Abstract To improve the oxidation protective ability of carbon–bonded carbon fiber (CBCF) composites, double anti-oxidation protection for CBCF composites were prepared, i.e., ceramic coating-coated CBCF composites combined with ceramic-modified carbon fiber in CBCF matrix. The ablation behavior of modified CBCF composites was tested under an oxyacetylene flame at 1600 °C for 300 s and 800 s, respectively. The results indicate that the ZrB2 in matrix and ZrB2-based ceramic coating can play double protection for CBCF composites during ablation process. The linear ablation rate of the sample after ablation for 300 s and 800 s were −1.1×10−4 and 8.38×10−4 cm s−1, respectively. The modified CBCF composites presented excellent oxidation resistance for 300 s. With the increase of the oxidation time for 800 s, the ZrB2-based ceramic coating experienced catastrophic damage. However, the carbon fiber surface only exhibited some circular pits instead of complete oxidation, implying that the ZrB2 on the carbon fiber surface improved the anti-oxidation and ablation resistance of CBCF composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Flame retardant materials and properties · Silicone and Siloxane Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Wei · 1985 · 1
2. Mechanical properties in compression of CVI– densified porous carbon/carbon composite10.1016/S0266-3538(98)00059-1 ↗
3. Microstructural investigation of low–density carbon–carbon composites10.1007/BF01162488 ↗
4. Effect of chemical vapor infiltration on erosion and thermal properties of porous carbon/carbon composite thermal insulation10.1016/S0008-6223(99)00125-6 ↗
5. Protective coatings for carbon bonded carbon fibre composites10.1016/j.ceramint.2007.03.012 ↗
6. A MoSi2/SiC oxidation protective coating for carbon/carbon composites10.1016/j.corsci.2010.11.024 ↗
7. Protective coatings for carbon bonded carbon fibre composites10.1016/j.ceramint.2007.03.012 ↗
8. Microstructural and compositional characterisation of the pyrocarbon interlayer in SiC coated low density carbon/carbon composites10.1016/j.jeurceramsoc.2010.09.004 ↗
9. High-temperature erosion resistance of ZrB2-based ceramic coating for lightweight carbon/carbon composites under simulated atmospheric re-entry conditions by high frequency plasma wind tunnel test10.1016/j.ceramint.2016.03.029 ↗
10. Microstructure, surface emissivity and ablation resistance of multilayer coating for lightweight and porous carbon–bonded carbon fiber composites10.1016/j.jallcom.2016.06.208 ↗
11. B.DuC.Q.HongS.B.ZhouC.LiuX.H.Zhang, Multi-composition coating for oxidation protection of modified carbon-bonded carbon fiber composites, J. Eur. Ceram. Soc. doi:10.1016/j.jeurceramsoc.2016.05.02810.1016/j.jeurceramsoc.2016.05.028 ↗
12. Fabrication and properties of lightweight ZrB2 and SiC-modified carbon bonded carbon fiber composites via polymeric precursor infiltration and pyrolysis10.1039/C4RA04089A ↗
13. Anti-oxidation and ablation properties of carbon/carbon composites infiltrated by hafnium boride10.1016/j.carbon.2012.09.053 ↗
14. Microstructural investigation of low-density carbon-carbon composites10.1007/BF01162488 ↗
15. Hybrid carbon nanotube/ultra-high temperature ceramic heterostructures:microstructure evolution and forming mechanism10.1111/jace.13813 ↗
16. Mechanical enhancement of lightweight ZrB2-modified carbon-bonded carbon fiber composites with self-grown carbon nanotubes10.1016/j.carbon.2016.02.077 ↗
17. Carbon-bonded carbon fiber composites containing uniformly distributed silicon carbide10.1039/c3ra44913k ↗
18. Preparation of a multi-composition coating for oxidation protection of modified carbon-bonded carbon fiber composites by a rapid sintering method10.1016/j.surfcoat.2015.03.014 ↗
19. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
20. SiO2@SnO2/graphene composite with a coating and hierarchical structure as high performance anode material for lithium ion battery10.1016/j.jallcom.2016.03.136 ↗
21. A multilayer MoSi2–SiC–B coating to protect SiC-coated carbon/carbon composites against oxidation10.1016/j.vacuum.2012.04.045 ↗
22. Ablation resistance of ZrB2 SiC/SiC coating prepared by pack cementation for graphite10.1016/j.jallcom.2016.04.010 ↗
23. Ablation behavior of ZrB2–SiC sharp leading edges10.1016/j.jallcom.2013.03.067 ↗
24. Oxidation behavior and phase transition of ZrB2–SiCw–ZrO2f ceramic10.1016/j.corsci.2013.08.002 ↗
25. Oxidation protection of C/C composites by ultra long SiC nanowire-reinforced SiC–Si coating10.1016/j.corsci.2014.03.029 ↗
26. Ultra-high-temperature tensile properties and fracture behavior of ZrB 2-based ceramics in air above 1500°C10.1016/j.matdes.2013.05.045 ↗
27. Microstructure evolution and oxidation behavior of B modified MoSi2 coating on Nb–Si based alloys10.1016/j.corsci.2015.12.003 ↗
28. Strengthening of porous TiB2–SiC ceramics by pre-oxidation and crack-healing10.1016/j.apsusc.2015.11.125 ↗
29. Oxidation and ablation resistance of the ZrB2–CrSi2–Si/SiC coating for C/C composites at high temperature10.1016/j.jallcom.2015.12.011 ↗