Si-SiC-ZrB2 ceramics by silicon reactive infiltration
Source abstract
Abstract
Abstract Silicon carbide ceramics obtained by silicon reactive infiltration are nowadays employed within industry in several high temperature applications. Although these ceramics show good thermo-mechanical properties and oxidation resistance, they suffer temperature limitations (1400 °C). At higher temperatures another type of ceramics, commonly known as ultra high temperature ceramics (UHTCs), is under study. These include the transition metal diborides of group IV; one in particular, zirconium diboride, is interesting in certain applications (e.g. aerospace) because of its low relative density. ZrB 2 -SiC ceramics show good thermo-mechanical properties and maintain the “protective” passive oxidation regime of their scales over a wide range of temperatures. This paper presents a feasibility study on a manufacturing methodology to produce Si-SiC-ZrB 2 bulk ceramics taking advantage of the reactive infiltration technique. This technique allows lower processing temperatures and near to net shape capability due to low shrinking of the green compacted bodies. C-SiC-ZrB 2 preforms were successfully infiltrated with molten silicon. The resulting Si-SiC-ZrB 2 composites showed promising oxidation behavior, similarly to that reported in other works. Bulk material optimization was performed with a view to manufacturing Si-SiC-ZrB 2 ceramic matrix composites by silicon reactive infiltration in future.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Silicon/silicon carbide composites
2. NIST-JANAF themochemical tables, fourth edition
3. Heidenreich · 2008
4. The effect of porous carbon preform and the infiltration process on the properties of reaction-formed SiC10.1016/j.carbon.2004.03.018 ↗
5. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
6. Oxygen transport in silica at high temperatures: implications of oxidation kinetics10.1111/j.1151-2916.2001.tb01061.x ↗
7. Ultra high temperature ceramic composites
8. R.A. Cutler, Engineering Properties of Borides, in ASTM Engineered Materials Handbook, vol. 4 – Ceramics and Glasses, Schneider, S.J., technical chairman, pp. 787–803, 1991.
9. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
10. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
11. New route to process uni-directional carbon fiber reinforced (SiC+ZrB2) matrix mini-composites10.1007/s10853-009-3437-4 ↗
12. Preparation and characterization of C/SiC-ZrB2 composites by precursor infiltration and pyrolysis process10.1016/j.ceramint.2009.11.015 ↗
13. Thick protective UHTC coatings for SiC-based structures: process establishment10.1111/j.1551-2916.2008.02360.x ↗
14. ZrB2-SiC oxidation protective coating on C/C composites prepared by vapor silicon infiltration process10.1111/j.1551-2916.2009.03481.x ↗
15. The effect of carbon on the processing of SiC/SiCf composites
16. C Fiber Reinforced Ceramic Matrix Composites by a Combination of CVI, PIP and RB
17. Mechanical properties of sintered ZrB2-SiC ceramics10.1016/j.jeurceramsoc.2010.11.013 ↗
18. Pressureless sintering of ZrB2-SiC ceramics10.1111/j.1551-2916.2007.02006.x ↗
19. Thermodynamic analysis of ZrB2-SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
20. Wetting of Sic, Si3N4, and Carbon by Si and Binary Si Alloys10.1111/j.1151-2916.1975.tb19006.x ↗
21. Wetting and infiltration of carbon by liquid silicon10.1007/s10853-005-1950-7 ↗
22. Reactive wetting in the liquid-silicon/solid-carbon system10.1111/j.1151-2916.1996.tb08519.x ↗
23. Wettingand adhesion in metal–silicon carbide systems: the effect of surface polarity of SiC10.1016/S1359-6462(99)00325-5 ↗
24. Samsonov · 1972
25. Wettability and interfacial energies in SiC-liquid metal systems10.1007/BF02403656 ↗
26. A. Passerone, personal communication, July 13, 2008.
27. Toward oxidation-resistant ZrB2-SiC ultra high temperature ceramics10.1007/s11661-010-0540-8 ↗
28. Effect of SiC, TaB2 and TaSi2 additives on the isothermal oxidation resistance of fully dense zirconium diboride10.1557/jmr.2009.0216 ↗
29. Toward oxidation-resistant ZrB2-SiC ultra high temperature ceramics
30. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
31. Thermodynamic analysis of ZrB2-SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
32. Oxidation of ZrB2- and HfB2-based ultra-high temperature ceramics: effect of Ta additions10.1023/B:JMSC.0000041693.32531.d1 ↗
33. Processing, properties, and arc jet oxidation of hafnium diboride/silicon carbide ultra high temperature ceramics10.1023/B:JMSC.0000041689.90456.af ↗
34. Oxidation of ZrB2-SiC10.1002/9780470294680.ch27 ↗