journal article·2018-08

Laser surface nanostructuring for reliable Si3N4/Si3N4 and Si3N4/Invar joined components

Milena Salvo, Valentina Casalegno, Manuela Suess, Laura Gozzelino, Christian Wilhelmi

Ceramics International· Volume 44· Issue 11
Publisher page

Abstract

Abstract IR pulsed laser radiation in air was applied to Si3N4 and Invar to obtain reliable Si3N4/Si3N4 and Si3N4/Invar adhesive bonded components. The laser pre-treatment produced a homogeneous nanostructured oxide layer on the surfaces, which effectively increased the adhesion at the adhesive/adherends interface and led to cohesive failure in the joining material. The mechanical strength of Si3N4/ Si3N4 and Si3N4/Invar joined components was measured, with and without laser nanostructuring, before and after thermal cycling from room temperature to 50 K, and it resulted that the exposure to extremely low temperatures did not affect the mechanical integrity of the joints. It was also demonstrated that this laser pre-treatment did not alter the mechanical properties of the ceramic substrate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Study of joining of carbon/carbon composites for ultra stable structures10.1016/j.jeurceramsoc.2009.12.013 ↗
2. Silicon Nitride ceramics for product and process innovations10.4028/www.scientific.net/AST.65.70 ↗
3. Materials for optical systems
4. Joining similar and dissimilar materials
5. Laser ablative surface treatment for enhanced bonding of Ti-6Al‑4V alloy10.1021/am302293m ↗
6. Influence of surface pre-treatments on the high-cycle fatigue behavior of Ti–6Al–4V – from anodizing to laser-assisted techniques10.1016/j.ijfatigue.2016.06.010 ↗
7. L.H. Laiterman, M.V. Radovan, G.F. Cabak, Experimental investigation of adhesive bond strength between metal and optical glass, in: Proc. SPIE 7735, Ground-based and Airborne Instrumentation for Astronomy III, 773542, San Diego, California, USA, June 27, 2010.10.1117/12.857775 ↗
8. Pre-bonding technology based on excimer laser surface treatment10.1016/S0169-4332(99)00384-0 ↗
9. Laser induced surface nanostructuring of Ti-6Al-4V10.1016/j.ijadhadh.2013.05.004 ↗
10. E. Brandl, A. Kurtovic, C. Wilhelmi, Method for the Nanostructuring of Ceramic, Glass, Carbon, Boron, Silicon and Compound Materials, EU Patent application EP20130002753, 2013.
11. Effect of pulsed laser irradiation on the SiC surface10.1111/ijac.12655 ↗
12. Regulation (EC) No. 1907/2006 of the European Parliament and of The Council of 18 December 2006 concerning the Registration, Evaluation, Authorisation and Restriction of Chemicals (REACH), establishing a European Chemicals Agency, amending Directive 1999/4: REACH. Grie: KFT Chemieservice GmbH, 2013.
13. Surface texturing of sialon ceramic by femtosecond pulsed laser10.1016/j.promfg.2016.12.098 ↗
14. Experimental investigation of laser surface processing of flexure silicon nitride ceramic10.1016/S1003-6326(06)60256-2 ↗
15. Surface characterization and compositional evaluation of a fibre laser processed silicon nitride (Si3N4) engineering ceramic
16. Excimer laser surface modification of engineering ceramics for adhesive bonding10.1016/S0924-0136(96)02505-8 ↗
17. Silicon nitride ceramics for product and process innovations10.4028/www.scientific.net/AST.65.70 ↗
18. 〈http://www.fcti.de/de/download/FCT-SiN-Standard-Materials-2016_12-en.pdf〉.
19. Invar® M93 data sheet from 〈http://www.aperam.com/alloysandspecialities/fileadmin/pdf/datasheets_uk/Documentation_web_Invar__Anglais_16_septembre_09.pdf〉.
20. Henkel Hysol®EA9321 data sheet, from 〈http://www.na.henkel-adhesives.com〉.
21. DIN EN 1288-5 (2000-09) standard, Glass in Building - Determination of the Bending Strength of Glass - Part 5: Coaxial Double Ring Test on Flat Specimens with Small Test Surface Areas.
22. V. Dietrich, P. Hartmann, F. Kerz, Bending strength measurements at different materials used for IR-cut filters in mobile camera devices, in: Proc. SPIE 9359, Optical Components and Materials XII, 93590D (16 March 2015).10.1117/12.2079310 ↗
23. ASTM D905-D908, Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading.
24. Synthesis and characterization of SiO2 nano- and micro-wires by a non-catalytic technique10.1007/s10853-013-7406-6 ↗
25. Nanostructured columnar tin oxide thin film electrode for lithium ion batteries10.1021/cm0519378 ↗
26. Adhesion phenomena in bonded joints10.1016/j.ijadhadh.2012.04.007 ↗
27. Bonded joints for dissimilar adherends at very low temperatures- an adhesive selection approach10.1016/j.tafmec.2016.08.012 ↗
28. Adhesive joints at high and low temperatures using similar and dissimilar adherends and dual adhesives10.1016/j.ijadhadh.2006.04.002 ↗
29. Design/analysis of the JWST ISIM bonded joints for survivability at cryogenic temperatures