journal article·2015-08

Fabrication of Cf/ZrC–SiC composites using Zr–8.8Si alloy by melt infiltration

Jinming Jiang, Song Wang, Wei Li, Zhaohui Chen

Ceramics International· Volume 41· Issue 7
Publisher page

Abstract

Abstract Cf/ZrC–SiC composites were fabricated by melt infiltration at 1800 °C using Zr–8.8Si alloy and carbon felt preforms. Microstructural analysis showed the formation of both ZrC and SiC phases in the matrix, in which ZrC acted as a main composition of the resulting composites. The results showed that carbon matrix reacted preferentially with Si of Zr–8.8Si alloy, which caused the formation of SiC first and then ZrC. The designed carbon coating by pyrolysis prevented the severe reaction between fibers and the melt. The composites could be more dense and uniform with the bending strength of 53.3 MPa, when preforms had a high open porosity (47.2%) with small size pores (10–40 μm).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. L. Kaufman, E.V. Clougherty, Investigation of Boride Compounds for Very High Temperature Applications, AirForce Technical Documentary Report no. RTD-TDR-63-4096, 1963.
2. I.E. Campbell, E.M. Sherwood, High-Temperature Materials and Technology. New York, 1967.
3. Evaluation of ultra-high temperature ceramics for aero-propulsion use10.1016/S0955-2219(02)00140-1 ↗
4. Designing for ultra-high temperature applications: the mechanical and thermal properties of HfB2, HfCx, HfNx and Hf(N)10.1023/B:JMSC.0000041690.06117.34 ↗
5. W.G. Fahrenholtz, G.E. Hilmas Report on the NSF-AFOSR Joint Workshop on Future Ultra-High Temperature Materials, National Science Foundation Workshop, Arlington, 2004.
6. Thermal stability of refractory carbide/boride composites10.1016/S0254-0584(01)00486-2 ↗
7. Microstructure and mechanical properties of Cf/ZrC composites fabricated by reactive melt infiltration at relatively low temperature10.1016/j.ceramint.2013.05.004 ↗
8. Effect of an SiC addition on the oxidation of ZrB2
9. Oxidation of ZrB2–SiC ceramics under atmospheric and reentry conditions
10. Microstructure and ablation behaviors of integer felt reinforced C/C–SiC–ZrC composites prepared by a two-step method10.1016/j.ceramint.2011.12.054 ↗
11. Preparation and characterization of three-dimensional carbon fiber reinforced zirconium carbide composite by precursor infiltration and pyrolysis process10.1016/j.ceramint.2011.02.024 ↗
12. Microstructural development of a Cf/ZrC composite manufactured by reactive melt infiltration10.1016/j.jeurceramsoc.2009.10.016 ↗
13. Effects of frequency on fatigue behavior of CVI C/SiC at elevated temperature10.1016/j.compscitech.2005.06.020 ↗
14. Preparation and characterization of C/SiC–ZrB2 composites by precursor infiltration and pyrolysis process10.1016/j.ceramint.2009.11.015 ↗
15. Carbon fibre reinforced ceramic matrix composites for high performance structures10.1111/j.1744-7402.2004.tb00169.x ↗
16. Fabrication of 2D C/ZrC–SiC composite and its structural evolution under high-temperature treatment up to 1800°C10.1016/j.ceramint.2009.03.030 ↗
17. Processing of carbon-fiber reinforced (SiC+ZrC) mini-composites by soft-solution approach and their characterization10.1016/j.ceramint.2009.06.016 ↗
18. Mechanical properties and microstructures of C/SiC–ZrC composites using T700SC carbon fibers as reinforcements10.1016/j.ceramint.2010.09.048 ↗
19. Near net-shape long fibre reinforced intermetallic matrix reactive infiltration process10.1016/0167-577X(92)90217-8 ↗
20. Fabrication of ZrB2–ZrC based composites by reactive melt infiltration at relative low temperature10.1016/j.scriptamat.2011.03.033 ↗
21. Microstructure and properties of W–ZrC composites prepared by displacive compensation of porosity method10.1016/j.jallcom.2011.05.105 ↗
22. Preparation of ZrB2 based composites by reactive melt infiltration at relative low temperature10.1016/j.matlet.2011.06.070 ↗
23. Reaction kinetics and ablation properties of C/C–ZrC composites fabricated by reactive melt infiltration10.1016/j.ceramint.2010.12.002 ↗
24. Processing and characterization of 3D carbon fiber reinforced silicon carbide and silicon nitride matrix composites
25. M.W. Chase Jr. NIST-JANAF Thermochemical Tables, 4th ed., Woodbury, New York, 1998.
26. C/C–SiC composite prepared by Si–10Zr alloyed melt infiltration10.1016/j.ceramint.2011.12.038 ↗
27. Melt infiltration approach to ceramic matrix composites10.1111/j.1151-2916.1988.tb05840.x ↗
28. Liquid-phase reaction-bonding of silicon carbide using alloyed silicon–molybdenum melts10.1111/j.1151-2916.1990.tb05179.x ↗
29. The dynamics of capillary flow10.1103/PhysRev.17.273 ↗
30. Kinetics of silicon-metal alloy infiltration into porous carbon10.1016/S1359-835X(99)00089-5 ↗
31. Fundamental studies of ceramic/metal interfacial reactions at elevated temperatures
32. Wetting of ceramic materials by liquid silicon, aluminium and metallic melts containing titanium and other reactive elements: a review10.1016/0272-8842(94)90027-2 ↗
33. Reactive wetting in the liquid-silicon/solid-carbon system10.1111/j.1151-2916.1996.tb08519.x ↗
34. Brandes · 1992
35. High-temperature wettability measurements in metal/ceramic systems—some methodological issues10.1016/j.cossms.2006.07.007 ↗