Synthesis of CoWSi–WSi2 nanocomposite by mechanical alloying and subsequent heat treatment
Source abstract
Abstract
In this study, systematic evaluations were performed on the synthesis of CoWSi–WSi2 nanocomposite by mechanical alloying and subsequent heat treatment. In this regard, 25 mol% Co, 35 mol% W, and 40 mol% Si powder mixture was milled for different durations. Then, the mechanically alloyed powders were heat treated at 1000 °C for 1 h. The phase transformations and structural evolutions of the powders after various milling durations and heat treatment were investigated by X-ray diffraction as well as scanning and transmission electron microscopy. The results showed that the phase evolutions during mechanical alloying and subsequent heat treatment were strongly dependent on milling time. After 20 h milling, a Co(ss)–WSi2 nanocomposite was formed. Increasing milling time to 50 h caused the formation of (Co,W,Si) solid solution, WSi2 and CoWSi phases. After heat treatment of 3 h ball milled powders, no new phases were detected. On the other hand, heat treatment of 5 h, 20 h and 30 h mechanically alloyed powders led to the formation of Co(ss)–WSi2–CoWSi–W5Si3. This means that there was a critical milling time (5 h) for the formation of WSi2 and CoWSi phases after heat treatment. Before this milling time, no new phases were formed, but after this time, WSi2 and CoWSi could be formed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Growth behavior and microstructure of oxide scales grown on WSi2 coating10.1016/j.intermet.2007.11.008 ↗
2. Microstructure and wear resistance of laser melted W/W2Ni3Si metal silicides matrix in situ composites10.1016/S1359-6462(02)00571-7 ↗
3. Microstructure and dry sliding wear resistance of laser clad TiC reinforced Ti–Ni–Si intermetallic composite coating10.1016/j.surfcoat.2009.09.024 ↗
4. Microstructure and tribological properties of NiMo/Mo2Ni3Si intermetallic in-situ composites10.1016/j.jallcom.2011.01.179 ↗
5. Elevated temperature wear behaviors of a Co–Mo–Si ternary metal silicide alloy10.1016/j.scriptamat.2005.03.002 ↗
6. A novel load-insensitive Co3Mo2Si reinforced in-situ metal–matrix composite coating for wear resistance application10.1016/j.matlet.2010.08.002 ↗
7. Model scratch corrosion studies for WC/Co hard metals10.1016/j.wear.2010.01.004 ↗
8. Beryllium-free cobalt alloy for high-load bushings
9. Synthesis and kinetic study of (Mo,W)Si2–WSi2 nanocomposite by mechanical alloying10.1016/j.jallcom.2012.06.072 ↗
10. Synthesis of WSi2–SiC composite under the thermally activated combustion mode10.1016/j.ijrmhm.2010.06.011 ↗
11. Nanocrystalline tungsten–nickel heavy alloy reinforced by in-situ tungsten carbide: mechanical alloying preparation and microstructural evolution10.1016/j.ijrmhm.2012.10.015 ↗
12. Fabrication of in situ Ni(W)–WC nanocomposites via mechanical alloying and spark plasma sintering10.1016/j.jallcom.2012.07.085 ↗
13. The mechanical alloying mechanism of various Fe2O3–Al–Fe systems10.1016/j.apt.2012.08.011 ↗
14. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
15. Fe3Al/TiC nanocomposite produced by mechanical alloying10.1179/003258910X12740974839387 ↗
16. Production of Fe3Al–TiC nanocomposite by mechanical alloying of FeTi2–Al–C powders10.1179/026708310X12756557336030 ↗
17. Effects of tungsten and aluminum additions on the formation of molybdenum disilicide by mechanically-induced self-propagating reaction10.1016/j.jallcom.2009.09.189 ↗
18. Synthesis of Mo5SiB2 based nanocomposites by mechanical alloying and subsequent heat treatment10.1016/j.msea.2011.01.033 ↗
19. Mechanically activated reactive synthesis of refractory molybdenum and tungsten silicides10.1016/j.ijrmhm.2007.05.008 ↗
20. Preparation of nanocrystalline intermetallic compounds WSi2 and MoSi2 by mechanical alloying10.1016/0925-8388(95)01697-X ↗
21. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
22. Structural transformations in Co87B13 and Ni87B13 alloys during ball milling and influence of stacking faults in FCC Co on amorphous phase formation
23. Copper–cobalt fcc metastable phase prepared by mechanical alloying10.1080/13642819308217953 ↗
24. B.D. Cullity, Elements of X-ray Diffraction, 2nd ed., 1978, Addison-Wiley, NewYork, pp. 303-352.
25. R. Ferro and A. Saccone, Intermetallic Chemistry, 2008, Elsevier, The Netherlands, pp.81-219.