Spark plasma sintering and characterization of 2Y-TZP ceramics

Weijiang Xue, Zhipeng Xie, Jian Yi, Chang-An Wang

Ceramics International· Volume 41· Issue 3
Publisher page

Abstract

Abstract A systematic study of various spark plasma sintering (SPS) parameters, namely temperature, holding time and applied pressure, was conducted to investigate their effect on the densification, microstructure and mechanical properties of 2Y-TZP ceramics. The obtained results demonstrated that 2Y-TZP can be fully densified at 1300–1600 °C within several minutes. Extending holding time resulted in a more significant grain growth at a higher sintering temperature but no remarkable change in density at a lower sintering temperature. Fully compacted samples could be attained with an applied pressure of 50 MPa at 1300 °C, at a 50 °C lower temperature than in the experiments with an applied pressure of 20 MPa. A critical grain size of 733 nm was revealed, corresponding to the fracture toughness maximum of 9.73±0.38 MPa m 1/2 . Furthermore, the optimal SPS conditions have been discussed and suggested in order to obtain a good combination of density and favorable fracture toughness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Low-temperature ageing degradation of 2.5Y-TZP heat-treated at 1650°C10.1016/j.jeurceramsoc.2004.06.022 ↗
2. Densification and grain growth of nanocrystalline 3Y-TZP during two-step sintering10.1016/j.jeurceramsoc.2008.04.030 ↗
3. 3Y-TZP ceramics with improved hydrothermal degradation resistance and fracture toughness10.1016/j.jeurceramsoc.2014.02.026 ↗
4. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
5. Transformation tougening. 2. Contribution to fracture-toughness10.1007/BF00809058 ↗
6. Grain-size-dependent transformation behavior in polycrystalline tetragonal zirconia10.1111/j.1151-2916.1992.tb07832.x ↗
7. On the transformation toughening of Y-ZrO2 ceramics with mixed Y-TZP/PSZ microstructures10.1016/S0955-2219(00)00273-9 ↗
8. R-curve behavior of 2Y-TZP with submicron grain size10.1016/j.jeurceramsoc.2005.11.012 ↗
9. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
10. Fracture toughness of nanocrystalline tetragonal zirconia with low yttria content10.1016/S1359-6454(02)00283-5 ↗
11. Mechanical properties of 2–3.5mol% Y2O3 stabilized zirconia polycrystals fabricated by the solid phase mixing and sintering method
12. Critical grain size and fracture toughness of 2mol% yttria-stabilized zirconia at ambient and cryogenic temperatures10.1016/j.scriptamat.2012.08.030 ↗
13. Spark plasma sintering of alumina10.1111/j.1151-2916.2002.tb00381.x ↗
14. Highly infrared transparent nanometric tetragonal zirconia prepared by high pressure spark plasma sintering10.1111/j.1551-2916.2011.04680.x ↗
15. Transparent nanometric cubic and tetragonal zirconia obtained by high-pressure pulsed electric current sintering10.1002/adfm.200600959 ↗
16. Transparent/translucent polycrystalline nanostructured yttria stabilized zirconia with varying colors10.1016/j.scriptamat.2007.11.014 ↗
17. Preparation of transparent 3Y-TZP nanoceramics with no low temperature degradation10.1111/jace.12919 ↗
18. Rapid sintering of nanocrystalline ZrO2 (3Y) by spark plasma sintering10.1016/S0955-2219(00)00152-7 ↗
19. Microstructure and mechanical properties of Ti3SiC2/3Y-TZP composites by spark plasma sintering10.1016/j.jeurceramsoc.2006.05.072 ↗
20. Microstructure and mechanical properties of ZrO2–Al2O3 nanocomposites prepared by spark plasma sintering10.1016/j.partic.2011.05.002 ↗
21. Rapid rate sintering of nano-grained ZrO2-based composites using pulse electric current sintering method10.1023/A:1026476430465 ↗
22. Evaluation of KIC of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
23. Rapid rate sintering of nanocrystalline ZrO2−3mol% Y2O310.1111/j.1151-2916.1996.tb08524.x ↗
24. Strength characterization of yttria partially-stabilized zirconia alumina composite10.1007/BF01151247 ↗
25. Densification and mechanical properties of TiC by SPS-effects of holding time, sintering temperature and pressure condition10.1016/j.jeurceramsoc.2012.04.017 ↗
26. Effect of grain size on mechanical properties of 3Y-TZP ceramics
27. Fracture toughness of nanocrystalline ZrO2/3mol% Y2O3 determined by vickers indentation10.1016/1359-6462(95)00587-0 ↗
28. Mechanics of transformation‐toughening in brittle materials10.1111/j.1151-2916.1982.tb10426.x ↗
29. The grain size dependence of the mechanical properties in TZP ceramics
30. Transformation tougening. 3. experimental observations in the ZrO2–Y2O3 system10.1007/BF00809059 ↗