journal article·2019-06Open access

Microstructure and shear strength of ZrB2SiC/Ti6Al4V joint by TiCuZrNi with Cu foam

Gang Wang, Zhentao Wang, Wei Wang, Rujie He, Kaixuan Gui, Caiwang Tan, Wei Cao

Ceramics International· Volume 45· Issue 8

Abstract

Abstract In this paper, brazing behaviors between ZrB2 SiC and Ti 6Al 4V by Cu foam interlayer were studied. The microstructure, formation mechanism, mechanical property and fracture surface of the joints were systematically studied. The results showed that the phases in the joints were α+β-Ti, TiCu, Ti2Cu, Cu(s, s), TiC, TiB2 and Ti3SiC2. An optimum shear strength reached up to 435 MPa at a brazing temperature of 910 °C and holding time of 20 min. Such a shear strength was 90 MPa higher than the one without the Cu foam. The obtained high shear strength of joint was discussed from microstructure and residual stress. With the increase of brazing time, Cu(s,s) gradually disappeared and the content of Ti2Cu intermetallic compound increased, which was harmful for the joint. Furthermore, the residual stress of joint with Cu foam was calculated to be 324 MPa, lower than the one without Cu foam interlayer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Structure evolution of ZrB2-SiC during the oxidation in air10.1557/JMR.2008.0251 ↗
2. Fabrication and characterization of B4C-ZrB2-SiC ceramics with simultaneously improved high temperature strength and oxidation resistance up to 1600oC10.1016/j.ceramint.2016.01.202 ↗
3. Brazing of ZrB2–SiC–C ceramic and GH99 superalloy to form reticular seam with low residual stress10.1016/j.ceramint.2014.08.051 ↗
4. Brazing of C/C composites to Ti6Al4V using graphene nano-platelets reinforced TiCuZrNi brazing alloy10.1016/j.matlet.2016.07.111 ↗
5. Joining of zirconium diboride-based ultra high-temperature ceramic composites using metallic glass interlayers10.1016/j.msea.2007.01.015 ↗
6. Joining of ZrB2-based ultra-high-temperature ceramic composites using Pd-based braze alloys10.1016/j.scriptamat.2009.03.053 ↗
7. Joining of ZrB2-based ultra-high-temperature ceramic composites to Cu-Clad-Molybdenum for advanced aerospace applications10.1111/j.1744-7402.2008.02291.x ↗
8. Dissimilar diffusion brazing of WC-Co to AISI 4145 steel using RBCuZn-D interlayer10.1016/j.jmapro.2017.06.001 ↗
9. Transient liquid phase bonding of HfC-based ceramics10.1007/s10853-013-7746-2 ↗
10. Wettability and transient liquid phase bonding of hafnium diboride composite with Ni–Nb alloys10.1007/s10853-012-6778-3 ↗
11. Bonding of zirconia to superalloy with the active brazing technique10.1016/S0955-2219(00)00162-X ↗
12. Microstructure and shear strength of self-joined ZrB2 and ZrB2–SiC with pure Ni10.1016/j.scriptamat.2010.08.056 ↗
13. Microstructure and mechanical properties of ZrB2–SiC ultra high temperature ceramic composite joint using TiZrNiCu filler metal10.1179/1362171811Y.0000000063 ↗
14. ZrB2–SiC/Ti6Al4V joints: wettability studies using Ag- and Cu-based braze alloys10.1007/s10853-012-6790-7 ↗
15. Joining of ZrB2 ceramics to Ti6Al4V by Ni-Based interlayers10.1007/s11665-014-0868-0 ↗
16. Interfacial microstructure and mechanical properties of ZrB2-SiC-C ceramic and GH99 superalloy joints brazed with a Ti-modified FeCoNiCrCu high-entropy alloy10.1016/j.matdes.2016.02.055 ↗
17. Brazing of ZrB2–SiC ceramic with amorphous CuTiNiZr filler10.1016/j.ceramint.2015.12.032 ↗
18. Brazing ZrB2-SiC ceramics to Ti6Al4V alloy with TiCu-based amorphous filler10.1016/j.jmapro.2017.10.021 ↗
19. Reaction-composite brazing of carbon fiber reinforced SiC composite and TC4 alloy using Ag-Cu-Ti-(Ti + C) mixed powder10.1016/j.msea.2012.11.031 ↗
20. Effects of interfacial reaction and atomic diffusion on the mechanical property of Ti3SiC2 ceramic to Cu brazing joints10.1016/j.vacuum.2016.05.002 ↗
21. Joining of SiO2-BN ceramic to Nb using a CNT-reinforced brazing alloy10.1039/C4RA11110A ↗
22. Effects of processing parameters on microstructure and mechanical behavior of SiO2/Ti-6Al-4V joint brazed with AgCu/Ni interlayer10.1016/j.msea.2009.10.050 ↗
23. Interlayer design to control interfacial microstructure and improve mechanical properties of active brazed Invar/SiO2-BN joint10.1016/j.msea.2013.03.055 ↗
24. Microstructure and mechanical properties of TiAl alloy joint vacuum brazed with Ti-Zr-Ni-Cu brazing powder without and with Mo additive10.1016/j.matdes.2015.11.008 ↗
25. Microstructure and mechanical properties of the GH783/2.5DC/SiC joints brazed with Cu-Ti+Mo composite filler10.1016/j.matdes.2011.11.058 ↗
26. Brazing TC4 alloy to Si3N4 ceramic using nano-Si3N4 reinforced AgCu composite filler10.1016/j.matdes.2015.03.046 ↗
27. Joining ceramics to metals using metallic foam10.1016/j.msea.2008.06.007 ↗
28. In-situ and ex-situ microtensile testing of individual struts of Al foams and Ni/Al hybrid foams10.1016/j.matdes.2018.04.075 ↗
29. Microstructure and mechanical performance of ultrasonic spot welded open cell Cu foam/Al joint10.1016/j.jmapro.2018.04.022 ↗
30. Three-dimensional graphene-reinforced Cu foam interlayer for brazing C/C composites and Nb10.1016/j.carbon.2017.03.099 ↗
31. Carbon nanotubes-reinforced Ni foam interlayer for brazing SiO2-BN with Ti6Al4V alloy using TiZrNiCu brazing alloy10.1016/j.ceramint.2017.11.136 ↗
32. Vacuum brazing Nb and BN-SiO2 ceramic using a composite interlayer with network reinforcement architecture10.1016/j.ceramint.2017.03.136 ↗
33. Microstructural evolution and thermal stress relaxation of Al2O3/1Cr18Ni9Ti brazed joints with nickel foam10.1016/j.vacuum.2017.10.030 ↗
34. Control interfacial microstructure and improve mechanical properties of TC4-SiO2f/SiO2 joint by AgCuTi with Cu foam as interlayer10.1016/j.ceramint.2016.07.084 ↗
35. Relief of residual stress in Al2O3/Nb joints brazed with Ag-Cu-Ti/Cu/Ag-Cu-Ti composite interlayer10.1016/j.acme.2018.08.001 ↗
36. Diffusion bonding of ZrB2–SiC and Nb using dynamic compressed Ni foam interlayer10.1016/j.msea.2013.02.047 ↗
37. Vacuum brazing of sapphire with Inconel 600 using Cu/Ni porous composite interlayer for gas pressure sensor application10.1016/j.matdes.2013.08.046 ↗
38. Brazing ZTA ceramic to TC4 alloy using the Cu foam as interlayer10.1016/j.vacuum.2018.05.038 ↗
39. In-Situ synthesized TiC nano-flakes reinforced C/C composite-Nb brazed joint10.1016/j.jeurceramsoc.2017.11.059 ↗
40. Effects of alloying elements on the cytotoxic response of titanium alloys10.1016/j.msec.2010.12.013 ↗
41. Interfacial reaction behavior and mechanical characterization of ZrO2/TC4 joint brazed by Ag-Cu filler metal10.1016/j.msea.2015.08.067 ↗
42. Interfacial product of ZrB2-SiC brazing joint and growth kinetics of reaction layer
43. Low temperature brazing of titanium by the application of a Zr-Ti-Ni-Cu-Be bulk metallic glass alloy as a filler10.1016/j.intermet.2009.06.012 ↗
44. Research on the liquid phase spread-ing and microstructure of Ti/Cu eutectic reaction
45. A novel approach to brazing C/C composite to Ni-based superalloy using alumina interlayer10.1016/j.jeurceramsoc.2011.12.016 ↗
46. Joining ceramics to metals using metallic foam10.1016/j.msea.2008.06.007 ↗
47. Advances in brazing of ceramics10.1007/BF01117909 ↗
48. Laser welding of Ti40Zr25Ni3Cu12Be20 bulk metallic glass10.1016/j.msea.2012.01.114 ↗
49. An analytical characterization of the anisotropy of the elastic modulus of misaligned short-fiber-reinforced polymers10.1016/S0266-3538(97)00129-2 ↗
50. Thermal-expansion stresses in reinforced plastics10.6028/jres.037.015 ↗