Effect of initial cure time on toughness of geopolymer matrix composites
Source abstract
Abstract
Abstract The toughness of geopolymer matrix composites (GMC) has been identified as a limiting factor to their use in structural applications. Advanced ceramic matrix composites (CMC), which also are limited by brittle behavior, have shown gains in toughness through careful tailoring of the interface between fiber and matrix. This can create various crack dissipating mechanisms and prevent premature composite failure. Such interface modification has already been applied to a fiber reinforced geopolymer and while the resulting composite showed a reduction in brittle behavior, the modified interface produced an unacceptable loss in modulus without any other well-defined quantitative gains. Information gathered from other studies suggests the large decrease in modulus observed in the GMCs with the weakened interface may have been the result of poor matrix properties stemming from an inadequate cure. Therefore, this current study explores the effects of initial cure time on composite performance by measuring the mechanical properties GMCs with a modified interface. GMCs containing unidirectional Nextel 610 fiber were cured under two different sets of process conditions to better understand the influence of matrix properties. Additionally, specimens consisted of cleaned and carbon coated fiber surfaces, in an attempt to evaluate extremes of interfacial strength. Mechanical properties were then evaluated for comparison to determine if improved geopolymer matrix properties would allow a weakened interface to yield performance gains more in keeping with expectations based on CMC's. The results of the study indicate that specimens with carbon coating benefited from the longer initial cure time. The average increase in flexural modulus and strength over samples with one hour initial cure time was ~65% and ~170% respectively. Stress-strain behavior of the carbon-coated specimens with an extended cure time also indicated a greater degree of damage tolerance as compared to those without interphase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Geopolymers and geopolymeric materials10.1007/BF01904446 ↗
2. Interface design for oxidation-resistant ceramic composites10.1111/j.1151-2916.2002.tb00505.x ↗
3. Chawla · 2012
4. Fire-resistant aluminosilicate composites10.1002/(SICI)1099-1018(199703)21:2<67::AID-FAM596>3.0.CO;2-N ↗
5. J.W. Bridge, A.E. Grabher, D.W. Radford, Preliminary Investigation of Geopolymer Matrix-Ceramic FIber Composites for High Temperature Structural Applications, in: TEAM, Istanbul, Turkey, 2008.
6. Inorganic polymer matrix composite strength related to interface condition10.3390/ma2042216 ↗
7. P.T. Nivala, D.W. Radford, The effectiveness of toughness modifications of inorganic polymer matrix composites as measured by static flexure testing, in: 2010 SAMPE Fall Tech. Conference Exhib. Oct. 11 2010 - Oct. 14 2010, Soc. for the Advancement of Material and Process Engineering, 2010, p. SAMPE’s Utah Chapter.
8. M. Welter, Unidirectional fibre reinforced geopolymer matrix composites, 2013. 〈http://researcharchive.vuw.ac.nz/handle/10063/3078〉 (Accessed 28 April 2015).
9. Novel geopolymer based composites with enhanced ductility10.1007/s10853-006-0527-4 ↗
10. Interface engineering in oxide fibre/oxide matrix composites10.1179/095066000101528359 ↗
11. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
12. Foden · 1999
13. W.M. Kriven, J.L. Bell, M. Gordon, Microstructure and microchemistry of fully-reacted geopolymers and geopolymer matrix composites, in: Adv. Ceram. Matrix Compos. IX Proceedings April 27, 2003–April 30, 2003, American Ceramic Society, 2004, pp. 227–250.10.1002/9781118406892.ch15 ↗
14. Properties of Basalt Fiber Reinforced Geopolymer Composites
15. The Effect of Basalt Chopped Fiber Reinforcement on the Mechanical Properties of Potassium Based Geopolymer
16. K.J.D. MacKenzie, What are these things called geopolymers? A physico-chemical perspective, in: Adv. Ceram. Matrix Compos. IX Proc. April 27 2003 - April 30 2003, American Ceramic Society, 2004, pp. 175–186.
17. Joseph Davidovits, GEOPOLYMERS II: Processing and Applications of Ultra-High Temperature, Inorganic Matrix Resin for Cast Composite Structures, Molds, Tools for RP/C and Metal Industries Stable to 2,100F (1,150C), in: Anaheim, California, 1983, pp. 222–230.
18. Understanding the relationship between geopolymer composition, microstructure and mechanical properties10.1016/j.colsurfa.2005.06.060 ↗
19. Rahman · 2015
20. Online Materials Information Resource - MatWeb, (n.d.). 〈http://www.matweb.com/index.aspx〉 (Accessed 13 November 2015).
21. A.S. Rahman, D.W. Radford, Cure cycle optimization of an inorganic polymer matrix material for high temperature fiber reinforced composites, Compos. Part Appl. Sci. Manuf. (n.d.). 〈http://dx.doi.org/10.1016/j.compositesa.2016.03.001〉.10.1016/j.compositesa.2016.03.001 ↗
22. Evolution of the fibre-matrix interactions in basalt-fibre-reinforced geopolymer-matrix composites after heating
23. Novel fiber-reinforced composite materials based on sustainable geopolymer matrix10.1016/j.proeng.2011.11.2120 ↗
24. Davidovits · 2008
25. 3M Nextel (TM) Ceramic Textiles Technical Notebook, (2004). 〈http://www.3m.com/market/industrial/ceramics/misc/tech_notebook.html〉 (accessed 17 March 2015).
26. C28 Committee, Test Method for Flexural Properties of Continuous Fiber-Reinforced Advanced Ceramic Composites, ASTM International, 2011. 〈http://www.astm.org/cgi-bin/resolver.cgi?C1275-15〉 (Accessed 19 January 2015).
27. C28 Committee, Test Method for Monotonic Tensile Behavior of Continuous Fiber-Reinforced Advanced Ceramics with Solid Rectangular Cross-Section Test Specimens at Ambient Temperature, ASTM International, 2011. 〈http://www.astm.org/cgi-bin/resolver.cgi?C1275-15〉 (Accessed 19 January 2015).
28. The role of the fiber-matrix interphase on composite properties10.1016/0042-207X(90)94034-N ↗
29. Overview no. 85 The mechanical behavior of ceramic matrix composites10.1016/0001-6160(89)90291-5 ↗
30. Effect of interfaces on the properties of fiber-reinforcedfiber-reinforced ceramics10.1111/j.1151-2916.1990.tb09814.x ↗