Influence of the heat treatment on mechanical properties and oxidation resistance of SiC–Si3N4 composites
Source abstract
Abstract
Abstract The basic mechanical properties and oxidation behaviour of liquid-phase-sintered SiC–Si 3 N 4 composites were investigated as a function of the heat treatment at oxidising condition at 1350 °C/0–204 h. The results were compared to those obtained for a reference silicon carbide material, prepared by the same fabrication route. The heat treatment at higher temperature had a positive effect on fracture toughness values but no changes of hardness were observed. It was shown that the oxidation resistance increases with increasing temperature of heat treatment from 1650 °C to 1850 °C. Oxidation always followed parabolic rate law indicating diffusion as the rate limiting mechanisms. The addition of silicon nitride content had no significant influence on oxidation resistance of SiC–Si 3 N 4 composites.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Microstructural development during liquid phase sintering of silicon carbide ceramics10.1016/S0955-2219(96)00198-7 ↗
2. Pressureless sintered silicon carbide tailored with aluminium nitride sintering agent10.1016/j.jeurceramsoc.2012.07.020 ↗
3. Influence of the α/β-SiC phase transformation on microstructural development and mechanical properties of liquid phase sintered silicon carbide10.1023/A:1004552704872 ↗
4. Effect of β-to-α phase transformation on the microstructural development and mechanical properties of fine-grained silicon carbide ceramics10.1111/j.1151-2916.2001.tb00773.x ↗
5. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
6. Strength and fracture toughness of in situ-toughened silicon carbide10.1023/A:1018635131661 ↗
7. Effect of annealing treatments on microstructure and mechanical properties of liquid-phase-sintered silicon carbide10.1016/S0955-2219(00)00254-5 ↗
8. Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide10.1111/j.1151-2916.1998.tb02748.x ↗
9. Grain growth and fracture toughness of fine-grained silicon carbide ceramics10.1111/j.1151-2916.1995.tb09100.x ↗
10. In situ toughened silicon carbide with Al–B–C additions10.1111/j.1151-2916.1996.tb08145.x ↗
11. Oxidation behavior of liquid-phase sintered SiC with AlN and Er2O3 additives between 1200°C and 1400°C10.1016/S0955-2219(03)00030-X ↗
12. Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure10.1111/j.1151-2916.1994.tb04637.x ↗
13. Pressureless sintering of β-SiC with Al2O3 additions10.1007/BF00351412 ↗
14. Microstructural changes in liquid-phase-sintered α-silicon carbide10.1016/S0167-577X(96)00139-5 ↗
15. Properties of liquid phase presureless sintered SiC-based materials obtained without powder bed
16. High-temperature properties of liquid-phase-sintered α-SiC10.1016/S0921-5093(99)00769-8 ↗
17. Liquid phase sintering of SiC with rare-earth oxides
18. Effect of rare-earth cation additions on the high temperature oxidation behaviour of LPS-SiC10.1016/j.msea.2003.11.037 ↗
19. Intergranular glassy phase free SiC ceramics retains strength at 1500°C10.1016/j.scriptamat.2004.02.008 ↗
20. Sintering, high temperature strength and oxidation resistance of liquid-phase-pressureless-sintered SiC-AlN ceramics with addition of rare-earth oxides10.1016/j.jeurceramsoc.2008.12.020 ↗
21. Improvement in the oxidation resistance of liquid-phase-sintered silicon carbide with aluminum oxide additions10.1016/j.ceramint.2004.10.012 ↗
22. Oxidation of polycrystalline a-silicon carbide ceramic10.1016/S0272-8842(96)00051-X ↗
23. Effect of the sintering additive content on the protective passive oxidation behaviour of presureless liquid-phase-sintered SiC10.1016/j.jeurceramsoc.2012.05.004 ↗
24. Improved high temperature properties of SiC-ceramics sintered with Lu2O3-containing additives10.1016/S0955-2219(02)00282-0 ↗
25. resistance of SiC-AlN ceramics coated by oxidation-assisted-pack cementation process10.1016/j.jeurceramsoc.2010.10.015 ↗
26. Oxidation behavior of liquid-phase sintered silicon carbide with aluminum nitride and rare-earth oxides10.1111/j.1151-2916.2002.tb00448.x ↗
27. Liquid phase sintered silicon carbide (LPS-SiC) ceramics having remarkably high oxidation resistance in wet air10.1016/j.jeurceramsoc.2005.05.015 ↗
28. Strength improvement of LPS-SiC ceramics by oxidation treatment10.1016/j.ijrmhm.2009.08.004 ↗
29. Advanced Technical Ceramics-Monolithic ceramics-Fracture toughness-Part 5: Single-edge V-notch beam (SENVB) method. European Standard. Third draft ENV 14425-5, April 2001.
30. Thermal shock resistance and fracture toughness of liquid-phase-sintered SiC-based ceramics10.1016/j.jeurceramsoc.2009.01.021 ↗
31. Hardness–grain-size relations in ceramics10.1111/j.1151-2916.1994.tb04641.x ↗
32. Effect of Ar and N2 sintering atmosphere on the high-temperature oxidation behaviour of pressureless liquid-phase-sintered α-SiC in air10.1016/j.jeurceramsoc.2009.08.004 ↗
33. Blowing of silica microforms on silicon carbide10.1016/j.jnoncrysol.2004.10.007 ↗