Differential sintering of Al2O3/ZrO2–Ni composite, during pulse electric current sintering
Source abstract
Abstract
Abstract Powder mixtures of Al 2 O 3 , ZrO 2 , Ni were sintered by pulse electric current sintering at 1300 °C with a heating rate of 200 °C/min or 130 °C/min. Large ZrO 2 –Ni agglomerates are formed within the Al 2 O 3 matrix after sintering. Depending on the heating rate, these agglomerates formed networks within the matrix. The networks are heterogeneously distributed in the specimens prepared by the heating rate of 200 °C/min but homogeneously in the specimens prepared by the heating rate of 130 °C/min. The microstructure evolution of the specimen prepared by the heating rate of 200 °C/min indicates that the temperature at the edge of the specimen is higher than that at the center. The temperature difference is smaller for the specimen prepared by the heating rate of 130 °C/min. The small ZrO 2 particles tend to associate with nickel melt to form ZrO 2 –Ni agglomerates. Then the ZrO 2 –Ni agglomerates are migrated by magnetic field that induced by the pulse electric current.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
2. New design concept of structural ceramic–ceramic nanocomposite10.2109/jcersj.99.974 ↗
3. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
4. The toughening of alumina with nickel inclusions10.1016/0955-2219(90)90032-B ↗
5. Sintering of a nickel-dispersed-alumina composite and its properties10.1111/j.1151-2916.1997.tb02956.x ↗
6. Toughening alumina with nickel and zirconia10.1016/S0955-2219(00)00087-X ↗
7. R-curve behavior of alumina toughened with molybdenum and zirconia particles10.1016/S0921-5093(03)00366-6 ↗
8. Synergistic toughening of a hybrid NiAl composite reinforced with partially stabilized zirconia and molybdenum particles10.1016/S0921-5093(99)00384-6 ↗
9. Densification of Al2O3 powder using spark plasma sintering10.1557/JMR.2000.0140 ↗
10. Formation of tough interlocking microstructures in silicon nitride ceramics by dynamic ripening10.1038/417266a ↗
11. Formidable increase in the superplasticity of ceramics in the presence of an electric field10.1002/adma.200304863 ↗
12. Synthesis of nanograined ZrO2-based composites by chemical processing and pulse electric current sintering10.1016/S0167-577X(98)00125-6 ↗
13. Development of large-size ceramic/metal bulk FGM fabricated by spark plasma sintering
14. Effect of plasma activated sintering (PAS) parameters on densification of copper powder10.1016/S0025-5408(00)00246-4 ↗
15. Microstructure inhomogeneity in Al2O3 sintered bodies formed during the plasma-activated sintering process10.1023/A:1006684631127 ↗
16. W.H. Tuan, S.M. Liu, C.J. Ho, C.S. Lin, T.J. Yang, D.M. Zhang, Z.Y. Fu, J.K. Guo, Preparation of Al2O3–ZrO2–Ni nanocomposite by pulse electric current and pressureless sintering, J. Eur. Ceram. Soc. 25 (2005) 3125–3133.10.1016/j.jeurceramsoc.2004.07.001 ↗
17. Melting in semiconductor nanocrystals10.1126/science.256.5062.1425 ↗
18. Surface melting on small particles10.1063/1.120038 ↗
19. Interfacial phenomena in Al2O3-liquid metal and Al2O3-liquid alloy system10.1016/0955-2219(92)90016-7 ↗
20. Work of adhesion in ZrO2-liquid metal systems10.1007/BF00357807 ↗
21. Pulsed electric current sintering of silicon nitride10.1111/j.1151-2916.2003.tb03310.x ↗