Abstract The core–veneer bond strength of zirconia is believed to be influenced by various factors, including zirconia types. To date, studies on bond strength between veneering porcelain and zirconia core fabricated by slip-cast technique are few. The aim of this study was to investigate and compare the shear bond strength (SBS) of three core materials with two veneering porcelains. Sixty cylindrical discs (11 mm in diameter and 3 mm in thickness) were fabricated and divided into Experimental zirconia (Zir), Cercon® (Cer) and metal (Met) core group. Ceramkiss® (Ck) and InLine® (IL) veneering porcelains were fired to each core at a thickness of 3 mm. Before veneering, all core materials were sandblasted with 100 µm Al 2 O 3 , and a layer of opaque liner was applied in the first firing. The bonded samples were subjected to shear bond test following storage in distilled water (37 °C) for 24 h. Scanning electron micrograph (SEM) was used to identify the mode of bonding failure. The results were analyzed with One-way ANOVA and Independent t -test with Tukey post-hoc test. Interaction effect analysis was performed using two-way ANOVA. Met-IL showed the highest mean SBS value (28.9±3.8 MPa), whereas Cer-IL group obtained the lowest value (2.8±0.7 MPa). The mean SBS values of Zir-Ck and Zir-IL were found to be 23.1±2.4 MPa and 4.1±0.9 MPa respectively. When veneered with the same veneering porcelain, both experimental zirconia and Cercon® were comparable, whereas significant differences were observed between metal and zirconia groups. All core materials exhibited significant differences in terms of shear bond strength when veneered with different veneering ceramics. Cohesive failure occurred in the high SBS group, whereas mixed cohesive-adhesive failures were seen in the other groups. The core–veneer SBS is material dependent. The types of core and veneering materials significantly affected the SBS. Slip casted experimental zirconia and commercial zirconia demonstrated similar bonding capabilities with the existing veneering porcelain designed for zirconia core.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Building materials and conservation · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings - A new fabrication mode for all-ceramic restorations10.1016/j.dental.2008.04.019 ↗
2. Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up
3. Zirconia Posterior Fixed Partial Dentures: a Prospective Clinical 3-year Follow-up
4. A prospective evaluation of zirconia anterior partial fixed dental prostheses: clinical results after seven years10.1016/j.prosdent.2014.12.015 ↗
5. Five-year prospective clinical study of posterior three-unit zirconia-based fixed dental prostheses10.1007/s00784-011-0575-2 ↗
6. A 3- year retrospective and clinical follow-up study of zirconia single crowns performed in a private practice10.1016/j.jdent.2009.06.002 ↗
7. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study10.1016/j.prosdent.2006.08.010 ↗
8. 10-year clinical outcomes of fixed dental prostheses with zirconia frameworks
9. The influence of design parameters on the FEA-determined stress distribution in CAD/CAM produced all-ceramic dental crowns10.1016/j.dental.2004.03.013 ↗
10. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
11. Compatibility of machined Ce-TZP/AI2O3 nanocomposite and veneering ceramic10.1016/j.dental.2007.01.005 ↗
12. Influence of thickness and cooling rate on the development of spontaneous cracks in porcelain/zirconia structures10.1111/j.1834-7819.2010.01239.x ↗
13. Effect of zirconia type on its bond strength with different veneer ceramics10.1111/j.1532-849X.2008.00306.x ↗
14. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling10.1016/j.dental.2008.03.028 ↗
15. Shear bond strengths of pressed and layered veneering ceramics to high-noble alloy and zirconia cores10.1016/S0022-3913(11)60090-5 ↗
16. ISO · 1999 · 9693
17. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part 3: double veneer technique10.1111/j.1532-849X.2007.00244.x ↗
18. Shear strength of core-veneer interface in bi-layered ceramics10.1016/j.prosdent.2004.02.009 ↗
19. Experimental and FE shear-bonding strength at core/veneer interfaces in bilayered ceramics10.1016/j.dental.2011.03.001 ↗
20. Comparison between slip casting and cold isostatic pressing for the fabrication of nanostructured zirconia10.4028/www.scientific.net/AMR.896.335 ↗
21. Slip-casting alumina ceramics for crown and bridge restorations
22. Reliability and properties of core materials for all-ceramic dental restorations10.1016/j.jdsr.2008.04.001 ↗
23. Development of translucent zirconia for dental crown applications10.3923/ajsr.2015.342.350 ↗
24. ISO/TS 11405 · 2003
25. A comparison of bond strength of layered veneering porcelains to zirconia and metal10.1016/S0022-3913(10)60133-3 ↗
26. Effect of sandblasting and residual stress on strength of zirconia for restorative dentistry applications10.1016/j.jmbbm.2013.09.004 ↗
27. Effect of zirconia surface treatment on the shear bond strength of veneering ceramic10.1016/S0022-3913(11)60060-7 ↗
28. Strength influencing variables on CAD/CAM zirconia framework10.1016/j.dental.2007.06.030 ↗
29. Ceramkiss, ceramic material for veneering crowns for Cercon. Firing recommendation. 〈http://www.degudent.com/Communication_and_Service/Download/Ceramics/Cercon_ceram_kiss/GA_CerconCeramKiss_GB.pdf〉 (accessed 18.10.15)
30. IPS InLine instruction for use, 〈https://www.ivoclarvivadent.com/en/products/metal-ceramics/ips-inline-system/ips-inline〉 (accessed 18.10.15)
31. Slow cooling protocol improves fatigue life of zirconia crowns10.1016/j.dental.2014.10.005 ↗
32. Influence of zirconia surface treatment on veneering porcelain shear bond strength after cyclic loading10.1016/j.prosdent.2014.05.029 ↗
33. , Flexural and shear strength of ZrO2 and a high noble alloy bonded to their corresponding porcelains10.1016/S0022-3913(08)60206-1 ↗
34. In vitro evaluation of shear bond strength of veneering ceramics to zirconia10.4012/dmj.2009-065 ↗
35. Comparison of shear bond strength of two veneering ceramics to zirconia10.4103/1735-3327.104885 ↗
36. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: zirconia veneering ceramics10.1016/j.dental.2005.11.014 ↗
37. A.C.DinizR.M.NascimentoJ.C.M.SouzaB.B.Henriques A.F.P.Carreiro, Fracture and shear bond strength analyses of different dental veneering ceramics to zirconia, Mater. Sci. Eng. 38(1), 2014, pp. 79–84,10.1016/j.msec.2014.01.032 ↗
38. Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites10.1016/j.dental.2008.09.003 ↗
39. Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue
40. Mechanical and fracture behavior of veneer-framework composites for all-ceramic dental bridges10.1016/j.dental.2005.12.009 ↗
41. Strength influencing variables on CAD/CAM zirconia frameworks10.1016/j.dental.2007.06.030 ↗