journal article·2019-04

Densification of C/SiC composite surface by the hybrid process of laser cladding and subsequent heat treatment

Ning-ning Ma, Jian Chen, Zheng-ren Huang, Xue-jian Liu, Zhong-ming Chen

Ceramics International· Volume 45· Issue 6
Publisher page

Abstract

Abstract To improve the surface roughness of carbon fiber reinforced silicon carbide (C/SiC) composite, a glass film was prepared by the hybrid process of laser cladding and subsequent heat treatment in the study. The results indicate that the laser cladding technology solves the poor wettability between the molten glass and substrate; the heat treatment increases the density and surface smoothness of the glass film. At the same time, the heat treatment repairs the cracks and decreases the porosities of the laser cladding layer. The surface roughness of the glass film before polishing is 7.846 nm rms, and the thickness is 16 µm. There is a good metallurgical bonding without porosity between the glass film and substrate. Especially, the critical load estimated by scratch test is 129 N, which is 8 times that of heat treatment without laser cladding.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High Entropy Alloys Studies · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Mechanical and thermal performance of C/SiC composites for SPICA mirror
2. J.B. Hadaway, R. Eng, H.P. Stahl, J.R. Carpenter, J.R. Kegley, W.D.J.P.S. Hogue, Cryogenic performance of lightweight SiC and C/SiC mirrors, 5487 (2004) 1018-1029.10.1117/12.552409 ↗
3. Microscopic surface structure of C/SiC composite mirrors for space cryogenic telescopes10.1364/AO.46.002049 ↗
4. Effect of environment on the stress‐rupture behavior of a carbon‐fiber‐reinforced silicon carbide ceramic matrix composite10.1111/j.1551-2916.2004.01536.x ↗
5. Oxidation behavior of carbon–carbon composites with a three-layer coating from room temperature to 1700 °C10.1016/S0008-6223(98)00293-0 ↗
6. PVD SiC and PVD Si coatings on RB SiC for surface modification
7. The nature of wetting of silicon carbide with the melts of aluminoborosilicate glasses10.1007/BF00730846 ↗
8. Laser cladding of aerospace materials10.1016/S0924-0136(01)01121-9 ↗
9. Laser cladding of turbine blades10.1016/S0257-8972(99)00603-9 ↗
10. Analysis of coaxial laser cladding processing conditions10.1016/j.surfcoat.2004.06.029 ↗
11. Laser cladding of Zr65Al7.5Ni10Cu17.5 amorphous alloy on magnesium10.1016/j.matlet.2006.04.033 ↗
12. Process parameter selection for Inconel 625-Cr 3 C 2 laser cladded coatings
13. Laser cladding Co-based alloy/SiCp composite coatings on IF steel10.1016/j.matdes.2003.08.006 ↗
14. Oxidation protective multilayer coatings for carbon–carbon composites
15. Influence of boron ion implantation on the oxidation behavior of CVD-SiC coated carbon-carbon composites10.1016/S0008-6223(99)00126-8 ↗
16. Characterisation of CoB–Co2B coatings by the scratch test10.1080/02670844.2015.1121315 ↗
17. State of residual stress in laser-deposited ceramic composite coatings on aluminum alloys10.1016/j.actamat.2006.07.049 ↗
18. Influence of laser deposition technique on surface integrity of 12Ni maraging tool steel
19. Microstructure characteristics of Ni-based WC composite coatings by laser induction hybrid rapid cladding10.1016/j.msea.2007.07.058 ↗
20. W.W. Duley, - Co2 Lasers Effects and Applications, Academic Pr.*, 1976.10.1016/B978-0-12-223350-0.50008-0 ↗
21. Numerical and experimental studies of molten pool formation during an interaction of a pulse laser (Nd:YAG) with a magnesium alloy10.1016/j.optlastec.2008.07.012 ↗
22. Technology, morphology and characterization of laser clad composite NiCrBSi–WC coatings on stainless steel10.1016/j.surfcoat.2005.11.093 ↗
23. The wettability of SiC particles by molten aluminium alloy10.1016/S0924-0136(01)00975-X ↗