Influence of low velocity impact on oxidation performance of SiC coated C/SiC composites
Source abstract
Abstract
Abstract Dropped-weight impact tests were carried out to investigate the coating damage behavior of SiC coated plain-woven C/SiC composites under low velocity impact. The oxidation performance after impact was evaluated in a wet oxygen environment. The relationships between coating damage area, oxidizing weight loss and the flexural strength after oxidation with the impact energy were analyzed. It was concluded from the test results that 0.5 J was the impact energy corresponding to damage initiation of the coating, where the oxidation loss was 2.49% and the strength retention ratio was 94.92%, almost the same as the untreated coating. Between 0.5 J and 2 J, the weight loss of oxidation increased with impact energy, and the oxidation mechanism gradually changed from a diffusion-controlled local oxidation to a reaction-controlled uniform oxidation. When the impact energy was larger than 2 J, although the coating damage still increased with impact energy, weight loss and residual flexural strength remained almost constant. The residual strength remaining was no more than 8% of the non-oxidized C/SiC, indicating that the coating totally loses its anti-oxidation function.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Velocity Impact and Material Behavior · Mechanical Behavior of Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. SiC-matrix composites: non-brittle ceramics for thermo-structural application10.1111/j.1744-7402.2005.02009.x ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. Advanced ceramic matrix composite materials for current and future propulsion system applications10.1016/j.actaastro.2004.05.052 ↗
4. High-temperature protective coatings for C/SiC composites10.1016/j.jascer.2014.07.004 ↗
5. Oxidation behavior from room temperature to 1500°C of 3D-C/SiC composites with different coatings10.1111/j.1151-2916.2002.tb00205.x ↗
6. Oxidation behavior of oxidation protective coatings for PIP–C/SiC composites at 1500°C10.1016/j.ceramint.2011.06.063 ↗
7. Oxidation behavior of 2D C/SiC with a multi-layer CVD SiC coating10.1016/j.surfcoat.2005.03.009 ↗
8. Oxidation behavior of 3D C/SiC composites in two oxidizing environments10.1016/S0266-3538(00)00190-1 ↗
9. Oxidation behaviour of three-dimensional woven C/SiC composites10.1179/026708301101510456 ↗
10. Oxidation behaviors of C/SiC in the oxidizing environments containing water vapor10.1016/S0921-5093(02)00644-5 ↗
11. Low velocity impact damage evaluation of 2D C/SiC composite material10.4028/www.scientific.net/AMR.79-82.1835 ↗
12. The effects of stitched density on low-velocity impact damage of cross-woven carbon fiber reinforced silicon carbide composites10.1016/j.ceramint.2015.09.137 ↗
13. Effect of impact energy on damage resistance and mechanical property of C/SiC composites under low velocity impact10.1016/j.msea.2017.01.062 ↗
14. Damage analysis of thin 3D-woven SiC/SiC composite under low velocity impact loading10.1016/j.compositesa.2011.10.013 ↗
15. Ceramic matrix composites life cycle testing under reusable launcher environmental conditions10.1111/j.1744-7402.2005.02017.x ↗
16. Effect of impact damage on flexural strength of C/C-SiC composites10.1016/S0921-5093(99)00250-6 ↗
17. Effect of damage on flexural modulus of C/C-SiC composites10.1016/S0921-5093(03)00019-4 ↗
18. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: II, theoretical approach10.1111/j.1151-2916.1994.tb07097.x ↗
19. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: II, modeling10.1111/j.1151-2916.1994.tb07016.x ↗