The roles of microstructure and surface energy on subcritical crack growth in glass-ceramics
Source abstract
Abstract
Abstract This study aimed to investigate the microstructure, failure probabilities, the susceptibility to subcritical crack growth (SCG), and the surface energy of two comercial brands IPS E.max CAD, Ivoclar Vivadent (LD-C) and Celtra DUO, Dentsply (LS-C) and experimental lithium disilicate (LD-E) and metasilicate (LM-E) glass-ceramics. Discs of each material were made to determine the subcritical crack growth parameters and the biaxial flexural strength (ISO 6872). The stresses to failure (MPa) were submitted to Weibull's analysis (CI 95%). The SCG was tested in water at five constant stress rates: 0.005; 0.05; 0.5; 5 and 50 MPa/s. By measuring the contact angles of water and diiodomethane on the glass-ceramics, we calculated the surface energy (mN/m). The characteristic strengths (MPa) and the Weibull moduli were 382.8 ± 8.3 and 10.1 ± 1.5, 148.5 ± 4.0 and 8.4 ± 0.8, 233.5 ± 10.4 and 5 ± 0.6, and 280.4 ± 9.1 and 6.8 ± 0.9 for LD-C, LS-C, LD-E and LM-E, respectively. The parameter of susceptibility to SCG (n) was: LD-C (18.2 ± 2.5), LS-C (25.6 ± 5.8), LD-E (23.2 ± 8.1), and the LM-E (15.1 ± 2.1). The polar and dispersive energy of LD-C was (~45) and (~26) respectively. The microstructures show that the commercial glass-ceramics are more refined and uniform than the experimental ones, which led to less strength variation. The stress corrosion cracking of the glass-ceramics, mainly LD-C, seemed to be a combination of the surface energy and microstructural features.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Dental materials and restorations · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Clinical applications of biomaterials: State-of-the-art progress, trends, and novel approaches
2. Glass-ceramics in dentistry: a review10.3390/ma13051049 ↗
3. An in situ and ex situ study of the microstructural evolution of a novel lithium silicate glass-ceramic during crystallization firing10.1016/j.dental.2020.03.011 ↗
4. Höland
5. CAD/CAM systems available for the fabrication of crown and bridge restorations10.1111/j.1834-7819.2010.01300.x ↗
6. Ceramic dental biomaterials and CAD/CAM technology: State of the art10.1016/j.jpor.2014.07.003 ↗
7. Influence of material thickness on fractural strength of CAD/CAM fabricated ceramic crowns10.4012/dmj.2016-296 ↗
8. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
9. Principles and phenomena of bioengineering with glass-ceramics for dental restoration10.1016/j.jeurceramsoc.2006.04.101 ↗
10. Translucency of esthetic dental restorative CAD/CAM materials and composite resins with respect to thickness and surface roughness10.1016/j.prosdent.2014.12.003 ↗
11. Structural, chemical and optical characterizations of an experimental SiO2–Y-TZP ceramic produced by the uniaxial/isostatic pressing technique10.1016/j.jmbbm.2020.103749 ↗
12. Fracture toughness of experimental mica-based glass-ceramics and four commercial glass-ceramics restorative dental materials10.4012/dmj.2018-077 ↗
13. B.D.F. Vallerini, M.D.O.C. Villas-bôas, Nucleation Heat Treatment on the Crystalline Fraction and Crystal Morphology of Lamav Cad Lithium Disilicate, (n.d.) 1–23.
14. Novel glass-ceramics materials characterization for dental applications10.1016/j.dental.2017.08.015 ↗
15. Minimally invasive vertical preparation design for ceramic veneers: a multicenter retrospective follow-up clinical study of 265 lithium disilicate veneers
16. Determination of the slow crack growth susceptibility coefficient of dental ceramics using different methods10.1002/jbm.b.31892 ↗
17. Bolgar · 2018
18. DIN ISO 6872 · 2015
19. Conshohocken
20. Standard test method for microindentation hardness of materials
21. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
22. Estimation of the surface free energy of polymers10.1002/app.1969.070130815 ↗
23. Sakaguchi
24. A protocol for determining the surface free energy of dental materials10.1016/S0109-5641(03)00102-7 ↗
25. Properties of hot-pressed lithium silicate glass-ceramics10.1016/j.dental.2019.02.027 ↗
26. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
27. Trade-off between fracture resistance and translucency of zirconia and lithium-disilicate glass ceramics for monolithic restorations
28. Impact of crystallization firing process on the microstructure and flexural strength of zirconia-reinforced lithium silicate glass-ceramics10.1016/j.dental.2018.06.010 ↗
29. Influence of annealing temperature on the strength of dental glass ceramic materials10.1016/j.dental.2004.09.004 ↗
30. Wear, strength, modulus and hardness of CAD/CAM restorative materials10.1016/j.dental.2016.08.222 ↗
31. Flexural strength and microstructure of two lithium disilicate glass ceramics for CAD/CAM restoration in the dental clinic10.5395/rde.2013.38.3.134 ↗
32. NIST recommended practice guide: fractography of ceramics and glasses