journal article·2012-01

Dielectric tunable properties of high dielectric breakdown Ba0.5Sr0.5TiO3–Zn2P2O7 composite ceramics

Qiwei Zhang, Jiwei Zhai, Bo Shen, Xi Yao

Publisher page

Abstract

Abstract Dielectric properties of Ba0.5Sr0.5TiO3–xZn2P2O7 (x = 1, 3, 5, 10, 15 wt%) composite ceramics, which were prepared by solid-state reaction process, were intensively investigated. The results showed that the Curie temperature (Tc) of composites gradually shifted to lower temperature (−140 °C) with increasing the content of Zn2P2O7, and the dielectric constant were tuned effectively from 2020 to 107, while maintaining a relatively high tunability. Zn2P2O7 additions remarkably inhibited the grain growth of Ba0.5Sr0.5TiO3 phases, and improved the breakdown strength of samples up to 385 kV/cm. The sample with x = 10 wt% exhibited good dielectric properties (ɛr = 290, tg δ = 0.0006, T = 20.5%, BDS = 297 kV/cm). Meanwhile Zn2P2O7 addition also made the Tc far away from the room temperature, which reduced the sensitivity of the dielectric constant to temperature change and simultaneously improved the stability of materials.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Ceramics materials based on (Ba,Sr)TiO3 solid solutions for tunable microwave devices10.1007/s10832-004-5104-0 ↗
2. Ferroelectric materials for microwave tunable applications10.1023/B:JECR.0000015661.81386.e6 ↗
3. Breakthrough advances in low loss, tunable dielectric materials10.1007/s100190050098 ↗
4. Low-losses, highly tunable Ba0.6Sr0.4TiO3/MgO composite10.1063/1.2837621 ↗
5. Dielectric tunable properties of low dielectric constant Ba0.5Sr0.5TiO3–Mg2TiO4 microwave composite ceramics10.1063/1.2784202 ↗
6. Raman and dielectric study of Ba0.4Sr0.6TiO3–MgAl2O4 tunable microwave composite10.1063/1.3000057 ↗
7. Alumina based ceramics for high-voltage insulation10.1016/j.jeurceramsoc.2009.09.025 ↗
8. Effect of BaO–A2O3–B2O3–SiO2 glass additive on densification and dielectric properties of Ba0.3Sr0.7TiO3 ceramics10.2109/jcersj2.116.345 ↗
9. Preparation and dielectric properties of B2O3–Li2O doped BaZr0.35Ti0.65O3 ceramics sintered at a low temperature10.1016/j.ceramint.2007.09.056 ↗
10. Microwave dielectric properties and low-temperature sintering of Ba0.60Sr0.40TiO3 ceramics10.1111/j.1551-2916.2009.03226.x ↗
11. Microwave dielectric properties of A2P2O7 (A=Ca, Sr, Ba, Mg, Zn, Mn)10.1143/JJAP.43.3521 ↗
12. Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides10.1107/S0567739476001551 ↗
13. Effect of liquid-phase sintering on the breakdown strength of barium titanate10.1111/j.1551-2916.2007.01637.x ↗
14. Improving sintering behaviour of BaTiO3 by small doping additions10.1007/BF00352898 ↗
15. Dielectric properties of fine-grained barium titanate ceramics10.1063/1.336051 ↗
16. The cell volume effect in barium strontium titanate10.1016/S0038-1098(97)00289-5 ↗
17. Dielectric strength of fine grained barium titanate ceramics10.1007/BF00275336 ↗
18. Thermochemical description of dielectric breakdown in high dielectric constant materials10.1063/1.1565180 ↗
19. Proposed universal relationship between dielectric breakdown and dielectric constant10.1109/IEDM.2002.1175919 ↗