Abstract

Abstract A series of solid–solution carbides, (TixW1−x)C (x=0.9, 0.8, 0.7, 0.6), was prepared by the high-energy milling of TiO2–WO3–C mixtures via subsequent carbothermal reduction. With high-energy milling, only the size reduction of the constituent powders was apparent without any chemical reaction. The milled mixture powder was transformed to a single–phase (TixW1−x)C solid solution by heat treatment in a vacuum at 1200 °C. (TixW1−x)C–Co cermets were consolidated by isothermal sintering at 1300, 1400, and 1500 °C. The powders were fully densified by liquid-phase sintering at 1500 °C because the Co melted at 1430 °C. The mechanical properties of the (TixW1−x)C–Co cermet (Hv: ~24 GPa) were significantly better than those of the conventional WC–Co (Hv: ~13 GPa) or TiC–Co cermets (Hv: ~16 GPa). The use of a solid–solution carbide instead of conventional WC almost doubled its hardness values without a loss of toughness. It is indicated that the improved hardness of the (TixW1−x)C–Co cermet originates from the high hardness of (TixW1−x)C, and the solid–solution carbide would be a valuable substitute for conventional carbide cermets.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
2. McColm · 1986
3. Highly toughened dense TiC–Ni composite by in situ decomposition of (Ti,Ni)C solid solution10.1016/j.ceramint.2014.12.011 ↗
4. Toughened ultra–fine (Ti,W)(CN)–Ni cermets10.1016/j.scriptamat.2004.09.017 ↗
5. Sintered (Ti,W)C carbides10.1016/j.scriptamat.2006.12.026 ↗
6. Microstructure and mechanical properties of TiC–WC–(Ti,W)C–Ni cermets10.1016/j.msea.2009.05.017 ↗
7. Indentation fracture of WC–Co cermets10.1007/BF00555296 ↗
8. Effect of milling on the carbothermal reduction of oxide mixture for (Ti,W)C–Ni10.2320/matertrans.MRA2007267 ↗
9. Formation of core/rim structures in Ti(C,N)–WC–Ni cermets via a dissolution and precipitation process10.1111/j.1151-2916.2000.tb01415.x ↗
10. Preparation of a fine–structured TiC–Co composite by high–energy milling and subsequent heat treatment of a Ti–Co alloy10.1016/j.ceramint.2015.07.064 ↗
11. Microstructure of (W,Ti)C–Co system containing platelet WC10.1016/j.msea.2010.06.056 ↗