journal article·2018-04

Fabrication of dense Ce0.9Mg0.1P2O7-PmOn composites by microwave heating for application as electrolyte in intermediate-temperature fuel cells

Bhupendra Singh, Nitika Devi, Lakshya Mathur, Rajesh K. Singh, Aman Bhardwaj, Sun-Ju Song, Dirk Henkensmeier

Ceramics International· Volume 44· Issue 6
Publisher page

Abstract

Abstract In the present work, we report a method of fabrication of dense 10 mol% Mg 2+ -doped cerium pyrophosphate-phosphate (Ce 0.9 Mg 0.1 P 2 O 7 -P m O n ; CMP-P) composites by microwave heat-treatment of the preformed Ce 0.9 Mg 0.1 P 2 O 7 substrates in the presence of phosphoric acid. The composite was characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and electrochemical impedance spectroscopy (EIS). The microwave heating at 375 °C for 5 min resulted in the formation of dense CMP-P composites which retained most of the pyrophosphate phase. The electrical conductivity was extracted from the EIS data and for the CMP-P composite prepared by H 3 PO 4 loading for 10 h and microwave heat-treatment for 5 min it was found to be >10 −2 S m −1 in 100–250 °C range with a maximum of 0.062 S cm −1 at 190 °C, which was significant for its application as electrolyte in intermediate temperature fuel cells.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Solid-state spectroscopy and crystallography

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Intermediate temperature proton‐conducting membrane electrolytes for fuel cells10.1002/wene.64 ↗
2. Solid-state protonic conductors: principles, properties, progress and prospects10.1016/S0167-2738(99)00152-6 ↗
3. Solid acids as fuel cell electrolytes10.1038/35073536 ↗
4. A review on proton conducting electrolytes for clean energy and intermediate temperature-solid oxide fuel cells10.1016/j.rser.2017.05.147 ↗
5. New developments in proton conducting membranes for fuel cells10.1016/j.coche.2014.01.012 ↗
6. Lowering the temperature of solid oxide fuel cells10.1126/science.1204090 ↗
7. Advanced materials for SOFC application: strategies for the development of highly conductive and stable solid oxide proton electrolytes10.1016/j.pmatsci.2015.08.001 ↗
8. Fast ionic conduction in tetravalent metal pyrophosphate-alkali carbonate composites: new potential electrolytes for intermediate-temperature fuel cells10.1016/j.jpowsour.2017.02.006 ↗
9. Ionic conductivity of Gd3+ doped cerium pyrophosphate electrolytes with core-shell structure10.1149/2.062404jes ↗
10. Proton conduction in acceptor doped SnP2O710.1016/j.ssi.2010.12.011 ↗
11. An approach for restoring the proton conductivity of sintered tin pyrophosphate membranes for intermediate temperature fuel cell10.1016/j.jpowsour.2015.12.045 ↗
12. Dense composite electrolytes of Gd3+-doped cerium phosphates for low-temperature proton-conducting ceramic-electrolyte fuel cells10.1016/j.ceramint.2014.12.037 ↗
13. Electrical behavior of CeP2O7 electrolyte for the application in low temperature proton conducting ceramic electrolyte fuel cells10.1149/2.055212jes ↗
14. Proton conductors of cerium pyrophosphate for intermediate temperature fuel cell10.1016/j.electacta.2011.05.040 ↗
15. Ionic conductivity of Mn2+ doped dense tin pyrophosphate electrolytes synthesized by a new co-precipitation method10.1016/j.jeurceramsoc.2014.04.024 ↗
16. Effect of partial substitution of Sn4+ by M4+ (M=Si, Ti, and Ce) on sinterability and ionic conductivity of SnP2O710.1016/j.ceramint.2014.11.011 ↗
17. Effect of MnO doping in tetravalent metal pyrophosphate (MP2O7; M=Ce, Sn, Zr) electrolytes10.1016/j.ceramint.2015.10.082 ↗
18. Synthesis and characterization of dense SnP2O7-SnO2 composite ceramics as intermediate-temperature proton conductors10.1039/C0JM02596H ↗
19. Proton conduction in non-doped and acceptor-doped metal pyrophosphate (MP2O7) composite ceramics at intermediate temperatures10.1039/c2jm15335a ↗
20. Synthesis and characterization of MnO-doped titanium pyrophosphates (Ti1−xMnxP2O7; x = 0–0.2) for intermediate-temperature proton-conducting ceramic-electrolyte fuel cells10.1007/s11581-017-2024-y ↗
21. An H3PO4-doped polybenzimidazole/Sn0.95Al0.05P2O7 composite membrane for high-temperature proton exchange membrane fuel cells10.1016/j.jpowsour.2011.03.094 ↗
22. A proton-conducting composite membrane: Sn0.95Al0.05P2O7 and polystyrene-b-poly(ethylene/ propylene)-b-polystyrene10.1016/j.electacta.2010.07.043 ↗
23. Novel Nafion–zirconium phosphate nanocomposite membranes with enhanced stability of proton conductivity at medium temperature and high relative humidity10.1016/j.electacta.2007.07.019 ↗
24. Proton‐conducting zirconium pyrophosphate/poly (2, 5‐benzimidazole) composite membranes prepared by a PPA direct casting method10.1002/macp.200700261 ↗
25. Sn0.9In0.1P2O7-based organic/inorganic composite membranes application to intermediate-temperature fuel cells10.1149/1.2388737 ↗
26. Mn2+-doped CeP2O7 composite electrolytes for application in low temperature proton-conducting ceramic electrolyte fuel cells10.1149/2.090401jes ↗
27. Phase composition and long-term conductivity of acceptor doped Ce(PO3)4 and CeP2O7 with variable P/metal ratio and of CeP2O7-KH2PO4 composite10.1149/2.050308jes ↗
28. Electrical conductivity of M2+-doped (M=Mg, Ca, Sr, Ba) cerium pyrophosphate-based composite electrolyte for low-temperature proton conducting electrolyte fuel cells10.1016/j.jallcom.2013.06.017 ↗
29. Conductivity of SnP2O7 and In-doped SnP2O7 prepared by an aqueous solution method10.1016/j.ssi.2008.11.006 ↗
30. Studies on ionic conductivity of Sr2+-doped CeP2O7 electrolyte in humid atmosphere10.1021/jp311547g ↗
31. Structure, water uptake, and electrical conductivity of TiP2O710.1111/j.1551-2916.2010.04281.x ↗
32. Electrical behavior and stability of K2HPO4-KH5(PO4)2-Ce0.9Gd0.1P2O7 composite electrolytes for intermediate temperature proton-conducting fuel cells10.1149/2.0841603jes ↗
33. Fabrication of dense cerium pyrophosphate-polystyrene composite for application as low-temperature proton-conducting electrolytes10.1149/2.0351510jes ↗