Effect of temperature gradient on competitive growth behavior of Si and YSi2 in a Si–Y eutectic alloy prepared by Bridgeman method
Source abstract
Abstract
Abstract The Si–Y eutectic alloy has been prepared by Bridgeman method where the high temperature gradient (GE) can be obtained by means of double heating combining with liquid metal cooling. The microstructures of longitudinal section and cross section at different GE have been observed. It can be seen clearly that the YSi2 phase presents the evolution process of thick banded shape, island shape, reticular shape and fine strip shape as GE increases from 90 K/cm to 200 K/cm. Based on the interface growth temperature model, it can be concluded that the interface growth temperatures of Si phase and YSi2 phase both will decrease linearly with increasing GE while that of eutectic structure will keep a constant of 1485.6 K. Two critical temperature gradients GEC1 = 52 K/cm and GEC2 = 111 K/cm have been calculated. Eutectic coupling growth will take the dominant position when the actual GE is greater than GEC2. The primary Si phase will begin to form as GE is smaller than GEC2 and will be thicker as GE is smaller than GEC1. The coupling effect of withdrawal rate and GE on the microstructures of the Si–Y alloy also has been analyzed comprehensively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Semiconductor materials and interfaces · nanoparticles nucleation surface interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Effects of zirconium addition on microstructure and ablation resistance of carbon fibre reinforced carbon and SiC ceramic matrix composite prepared by reactive melt infiltration10.1179/1743676114Y.0000000159 ↗
2. Processing-microstructure-properties relationships of MoSi2-SiC composites10.1016/S0955-2219(02)00035-3 ↗
3. Development of a high temperature Cf/XSi2–SiC (X=Mo, Ti) composite via reactive melt infiltration10.1016/j.jeurceramsoc.2006.05.058 ↗
4. Effect of yttrium on the oxide scale adherence of pre-oxidized silicon-containing heat-resistant alloy10.1016/j.corsci.2011.07.002 ↗
5. Effect of yttrium alloying on intermediate to high-temperature oxidation behavior of Mo-Si-B alloys10.1007/s11661-012-1589-3 ↗
6. Homogeneous and heterogeneous melting behavior of bulk and nanometer-sized Cu systems: a numerical study10.1007/s10853-007-1522-0 ↗
7. Fabrication of SiCf/SiC composites by chemical vapor infiltration and vapor silicon infiltration10.1016/j.matlet.2010.05.013 ↗
8. Distribution of components in Ge–Si bulk single crystals grown under the continuous feeding of the melt with the second component (Si)10.1016/S0022-0248(01)01270-2 ↗
9. The dependence of lamellar spacing on growth rate and temperature gradient in the lead–tin eutectic alloy10.1016/S0924-0136(99)00344-1 ↗
10. Competitive growth of Si and YSi2 phases in a eutectic Si-Y alloy prepared by the Bridgeman method10.1016/j.ceramint.2018.04.150 ↗
11. Flemings · 1974 · 126
12. Effect of withdrawal rate on the microstructure of directionally solidified NiAl–Cr(Mo) hypereutectic alloy10.1016/j.intermet.2011.10.018 ↗
13. Effects of withdrawal rate and temperature gradient on the microstructure evolution in directionally solidified NiAl-36Cr-6Mo hypereutectic alloy10.1007/s11837-014-1008-x ↗
14. Effect of Temperature gradient and solidification rate on eutectic growth of Al-Si alloy during unidirectional solidification
15. Solidification microstructure of bridgman-grown Si–TaSi2 eutectic in situ composite10.1016/j.jcrysgro.2013.04.014 ↗
16. Microstructure and microsegregation in a Ni-based single crystal superalloy directionally solidified under high thermal dradient10.3724/SP.J.1037.2009.00419 ↗
17. A study of temperature gradient in liquid phase for double-zone heat directional solidification
18. Fu · 1985 · 176
19. Microstructure and mechanical properties of Al2O3/Y3Al5O12/ZrO2 hypereutectic directionally solidified ceramic prepared by laser floating zone10.1016/j.jeurceramsoc.2014.04.033 ↗
20. Self-assemble silicide architectures by directional solidification10.1016/j.jeurceramsoc.2005.01.033 ↗
21. Microstructure refinement approaches of melt-grown Al2O3/YAG/ZrO2 eutectic bulk10.1016/j.ceramint.2013.02.089 ↗
22. Microstructural morphology and irregular eutectic growth of directionally solidified Al2O3/YAG eutectic in situ composite
23. Dislocation mechanism of deformation and strength of Al2O3/YAG single crystal composites above 1500°C10.1016/S0955-2219(00)00028-5 ↗
24. Microstructure and mechanical properties of ceramics obtained from chemically co-precipitated Al2O3-GdAlO3 nano-powders with eutectic composition10.1016/j.ceramint.2017.02.125 ↗
25. Orientation relationships of unidirectionally aligned GdAlO3/Al2O3 eutectic fibers10.1016/j.jeurceramsoc.2014.04.042 ↗
26. Effect of growth rate on rod spacing and undercooling of Bridgman-grown Si-TaSi2 eutectic in situ composite10.1016/j.jallcom.2012.11.014 ↗
27. Critical undercoolings for the transition from the lateral to continuous growth in undercooled silicon and germanium10.1016/j.actamat.2004.03.027 ↗
28. Microstructure evolution of Ni, Cr, Al-TaC in situ composite directionally solidified under a high temperature gradient10.1016/S0921-5093(00)01908-0 ↗
29. The Si−Y (silicon-yttrium) system10.1007/BF02867814 ↗
30. Competitive growth of different phases in eutectic alloys under directional solidification10.1360/04ye0301 ↗
31. Cellular and dendritic growthⅡ10.1016/0022-0248(74)90127-4 ↗
32. Eutectic growth: a modification of the Jackson and Hunt theory10.1016/0956-7151(91)90114-G ↗