How does pore-induced crack change as temperatures decrease from 293 K to 77 K?
Source abstract
Abstract
Abstract The pore-induced cracks in pressureless-sintered SiC ceramics have been investigated at ambient and cryogenic temperatures. The Weibull plots of flexural strength were determined to compare the effects of pore-induced cracks on fracture behavior at 77 K and 293 K. The stress field near crack tip was investigated based on the microstructure of sintered SiC. The measurements of lattice constants of single crystal SiC were carried out by in situ X-ray diffraction. It was found that the effect of defect-induced crack on fracture was diminished at cryogenic temperatures, owing to the decreases of cracks׳ effective size and increases of propagate resistance. The improved fracture reliability and enhanced flexural strength of SiC ceramics facilitate their applications in space-based reflectors.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Some notes on the correlation between fracture and defect statistics: are Weibull statistics valid for very small specimens10.1016/j.jeurceramsoc.2005.08.021 ↗
2. Structural reliability: a processing-dependent phenomenon10.1111/j.1151-2916.1982.tb10380.x ↗
3. Fracture of brittle materials: effects of test method and threshold stress on the Weibull modulus10.1016/S0955-2219(00)00183-7 ↗
4. Light weight monolithic silicon carbide telescope for space application10.1117/12.624878 ↗
5. Development of the SOFIA silicon carbide secondary mirror
6. Influence of grain size, free silicon content and temperature on the strength and toughness of reaction-bonded silicon carbide10.1016/0272-8842(94)90042-6 ↗
7. Effect of particle dispersion on microstructure and strength of reaction-bonded silicon carbide10.1016/S0921-5093(01)01897-4 ↗
8. Development of high-strength reaction-sintered silicon carbide10.1016/S0925-9635(03)00066-9 ↗
9. High-temperature mechanical behavior of carbon–silicide–carbide composites developed by alloyed melt infiltration10.1016/j.jeurceramsoc.2007.09.053 ↗
10. Experimental probability estimators for Weibull plots10.1007/BF01729379 ↗
11. Enhanced fracture toughness of silicon nitride ceramics at cryogenic temperatures10.1016/j.scriptamat.2012.02.007 ↗
12. Some effects of cavities on the fracture of ceramics: II, spherical cavities10.1111/j.1151-2916.1979.tb18815.x ↗
13. Stress intensity factor estimates for annular cracks at spherical voids10.1111/j.1151-2916.1980.tb10737.x ↗
14. Effect of the grain boundary thermal expansion coefficient on the fracture toughness in silicon nitride10.1111/j.1151-2916.1995.tb08667.x ↗
15. The concept of filament strength and the Weibull modulus10.1520/JTE11131J ↗
16. Determination of surface crack size densities in glass
17. Fracture statistics of ceramics-Weibull statistics and deviations from Weibull statistics10.1016/j.engfracmech.2006.05.028 ↗
18. Statistical approach to brittle fracture10.1007/BF00540858 ↗
19. Fracture of ceramics and glasses10.1016/0022-3697(87)90121-1 ↗