journal article·2019-07

Effect of diffusion-assisting holes on the tensile properties of a thick-section two dimensional C/SiC composite fabricated by chemical vapor infiltration

Jiaxin Zhang, Yongsheng Liu, Yi Zhang, Jing Wang, Hui Zhao, Baoxi Zhang, Laifei Cheng

Ceramics International· Volume 45· Issue 10
Publisher page

Abstract

Abstract The concept of diffusion-assisting holes (DAHs) has been developed to increase matrix deposition in the middle layers of the thick-section ceramic matrix composites (CMCs) that are fabricated by chemical vapor infiltration (CVI). However, the effect of DAHs on the tensile properties of CMCs has not been studied. Here, the tensile properties and the state of matrix deposition of a 10-mm-thick two dimensional (2D) C/SiC with DAHs are investigated. Results showed, with DAHs, a zone of increased deposition with a radius of ca. 1.4 mm around a hole was introduced and the net-section strength of the 10-mm-thick 2D C/SiC was increased by 48.1%. In addition, the tensile load bearing capacity was also increased by 34.1%, although the load bearing section decreased with DAHs. The increased net-section strength and tensile load bearing capacity of the C/SiC are attributed to the increased matrix deposition in the middle layers of the thick-section composite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Application of fracture mechanics to fiber composites
3. Effect of glass sealing on the oxidation behavior of three dimensional C/SiC composites in air10.1016/S0008-6223(00)00148-2 ↗
4. Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration10.1016/S0008-6223(98)00076-1 ↗
5. Fracture behavior and mechanism of 2D C/SiC–BCx composite at room temperature10.1016/j.msea.2010.10.045 ↗
6. Low-cost preparation and frictional behaviour of a three-dimensional needled carbon/silicon carbide composite10.1016/j.jeurceramsoc.2008.06.021 ↗
7. Electrostatic assembly preparation of high-toughness zirconium diboride-based ceramic composites with enhanced thermal shock resistance performance10.1021/acsami.6b00822 ↗
8. Reaction kinetics and ablation properties of C/C–ZrC composites fabricated by reactive melt infiltration10.1016/j.ceramint.2010.12.002 ↗
9. Stochastic virtual tests for high-temperature ceramic matrix composites10.1146/annurev-matsci-122013-025024 ↗
10. Ceramic-matrix composites enable revolutionary gains in turbine engine efficiency
11. Mechanical and electrical properties of carbon nanotube buckypaper reinforced silicon carbide nanocomposites10.1016/j.ceramint.2015.12.011 ↗
12. Scalable preparation of graphene reinforced Zirconium diboride composites with strong dynamic response10.1016/j.carbon.2018.07.067 ↗
13. Thermophysical properties of three-dimensional ceramic-filler-modified carbon/carbon composites10.1016/j.ceramint.2018.10.015 ↗
14. Improved shear strength of SiC-coated 3D C/SiC composite joints with a tailored Ti-Si-C interlayer10.1016/j.jeurceramsoc.2018.11.016 ↗
15. The CVI-process : state of the art and perspective10.1002/9780470291313.ch37 ↗
16. The CVI-processing of ceramic matrix composites10.1051/jphyscol:1989526 ↗
17. Microstructure and mechanical properties of three-dimensional textile hi-nicalon SiC/SiC composites by chemical vapor infiltration10.1111/j.1151-2916.2002.tb00248.x ↗
18. High performance 3D textile Hi-Nicalon SiC/SiC composites by chemical vapor infiltration10.1016/S0272-8842(01)00002-5 ↗
19. Microstructure and properties of diamond/SiC composites prepared by tape-casting and chemical vapor infiltration process10.1016/j.jeurceramsoc.2014.05.042 ↗
20. Microstructures and mechanical properties of three-dimensional ceramic filler modified carbon/carbon composites10.1016/j.ceramint.2013.06.015 ↗
21. Effects of porosity on in-plane and interlaminar shear strengths of two-dimensional carbon fiber reinforced silicon carbide composites10.1016/j.matdes.2016.03.017 ↗
22. Improvement of the mechanical and thermophysical properties of C/SiC composites fabricated by liquid silicon infiltration10.1016/j.compscitech.2015.04.019 ↗
23. Thermal shock behavior of 3-dimensional C/SiC composite10.1016/S0008-6223(01)00225-1 ↗
24. Mechanical and electromagnetic shielding properties of carbon fiber reinforced silicon carbide matrix composites10.1016/j.carbon.2015.08.011 ↗
25. Failure behavior of 2D C/SiC I-beam under bending load10.1016/j.compstruct.2015.04.066 ↗
26. Carbon/silicon carbide composites prepared by chemical vapor infiltration combined with silicon melt infiltration10.1016/S0008-6223(98)00310-8 ↗
27. Fabricating thick-section carbon fiber/silicon carbide composites by machining-aided chemical vapor infiltration10.1016/j.ceramint.2017.07.025 ↗
28. Strengthening thick-section 3D needled C/SiC composites by tuning matrix deposition10.1016/j.ceramint.2019.01.096 ↗
29. Synthesis of highly tailored ceramic matrix composites by pressure-pulsed CVI10.1016/S0167-2738(01)00743-3 ↗
30. Fabrication of ceramic composites: forced CVI10.1016/0022-3115(94)00395-5 ↗
31. Vapor-phase fabrication and properties of continuous-filament ceramic composites10.1126/science.253.5024.1104 ↗
32. Acoustic emission characterization of fracture toughness for fiber reinforced ceramic matrix composites10.1016/j.msea.2012.09.081 ↗
33. The effect of heat treatment on the strength and toughness of carbon fiber/silicon carbide composites with different pyrolytic carbon interphase thicknesses10.1016/j.carbon.2013.01.076 ↗
34. Behavior of two-dimensional C/SiC composites subjected to thermal cycling in controlled environments10.1016/j.carbon.2005.07.003 ↗
35. Effect of loading rate and temperature on monotonic tensile behavior in two-dimensional C/SiC composites10.1016/j.ceramint.2014.08.024 ↗
36. The yarn size dependence of tensile and in-plane shear properties of three-dimensional needled textile reinforced ceramic matrix composites10.1016/j.matdes.2014.11.061 ↗
37. Characterization of tensile behavior of a two-dimensional woven carbon/silicon carbide composite fabricated by chemical vapor infiltration10.1016/j.msea.2008.07.050 ↗
38. Microstructure and tensile behavior of multiply needled C/SiC composite fabricated by chemical vapor infiltration10.1016/j.jmatprotec.2008.02.035 ↗