journal article·2019-10

cBN-Al2O3 composites in NaCl environment under high pressure and high temperature conditions

Dongliang Chu, Hongan Ma, Jian Wang, Zhuangfei Zhang, Weixia Shen, Xiaopeng Jia

Ceramics International· Volume 45· Issue 14
Publisher page

Abstract

Abstract A series of experiments of cubic boron nitride (cBN)-Al2O3 composites was conducted in NaCl environment under a pressure of 5 GPa at 1200–1650 °C using a Chinese multi-anvil high-pressure apparatus. The oxidation resistance of cBN-Al2O3 composites reached 1300 °C, which was 200 °C higher than that of raw cBN powder. The porosity was estimated by the content of NaCl impurities in cBN-Al2O3 composites. The content of NaCl impurity increases with increasing temperature and decreases with increasing Al2O3 level under high pressure and high temperature conditions. cBN+30 vol% Al2O3 sintered at 5 GPa and 1200 °C shows no NaCl impurity, and the Vickers hardness of the sample is 21.6 GPa which is half of cBN+10 vol% Al.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Spark plasma sintering of Al2O3-cBN composites facilitated by Ni nanoparticle precipitation on cBN powder by rotary chemical vapor deposition10.1016/j.jeurceramsoc.2011.05.019 ↗
2. Ultrahard nanotwinned cubic boron nitride10.1038/nature11728 ↗
3. Compositions, mechanical properties and microstructures of cBN-based composites sintered with Al or TiC10.1080/17436753.2017.1290330 ↗
4. Preparation and characterization of cBN-based composites from cBN-Ti3AlC2 mixtures10.1016/j.diamond.2016.05.003 ↗
5. Interaction of Al and cBN under high temperature and high pressure10.3724/SP.J.1077.2008.00253 ↗
6. Study of high-pressure sintering behavior of cBN composites starting with cBN-Al mixtures10.1557/jmr.2008.0316 ↗
7. Titanium/aluminum diborides in composites produced in the cBN-TiC-Al system by reaction sintering under high pressure10.3103/S1063457608050067 ↗
8. Mechanical properties of cBN-Al composite materials10.1016/j.ceramint.2010.07.034 ↗
9. Effects of Ni addition on properties of vitrified bond cBN composites in strong magnetic field10.1016/j.ceramint.2018.02.143 ↗
10. Spark plasma sintering and characterization of WC-Co-cBN composites10.4028/www.scientific.net/KEM.616.194 ↗
11. Fabrication of a novel Al2O3-Ti(C0.7N0.3)-cBN composite with excellent performance in the turning of difficult-to-machine stellite alloys10.1016/j.ceramint.2018.04.088 ↗
12. Al2O3- cBN composites sintered by SPS and HPHT methods10.1016/j.jeurceramsoc.2016.01.027 ↗
13. Effects of cubic BN addition and phase transformation on hardness of Al2O3- cubic BN composites10.1016/j.ceramint.2010.09.058 ↗
14. Densification and microstructure of Al2O3-cBN composites prepared by spark plasma sintering10.2109/jcersj2.116.744 ↗
15. Reaction process of heat treating barium ferrite magnetic powder
16. Structural transformations of boron trioxide under high pressure and high temperature10.1016/j.ceramint.2018.04.041 ↗