Evaluation of nanosecond laser ablation and scratch resistance of tantalum carbide coated graphite substrates
Source abstract
Abstract
Abstract The present work aimed at investigating the effect of nanosecond laser parameters on ablation characteristics such as ablation depth and surface roughness of plasma sprayed tantalum carbide coated graphite substrates. The micro scratch tests were performed on the laser ablated and as-sprayed coatings to evaluate the critical loads and coefficient of friction. The laser ablated surface with minimum ablation depth and surface roughness was found to exhibit 18% higher critical loads when compared to that of as-sprayed surface. However, laser ablated surfaces exhibited slightly higher friction coefficient than as-sprayed surfaces due to formation of metastable oxide layer (Ta6O) on the top surface of TaC coatings as indicated by XRD. The maximum ablation and scratch resistance could be found at maximum pulse energy of 250 μJ, maximum scanning speed of 1000 mm/s and moderate hatch spacing of 20 μm. While, the failure of as-sprayed TaC coatings was attributed to local collapsing of material due to degradation of mechanical properties such as elastic modulus, surface porosity and surface roughness, laser ablated surfaces exhibited wedge spallation at the end of scratch zone only.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Laser-induced spectroscopy and plasma · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. ZrB2-SiC-WC coating with SiC diffusion bond coat on graphite by spark plasma sintering process10.1016/j.ceramint.2017.07.123 ↗
2. Microstructure and oxidation behavior of sol-gel mullite coating on SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2015.06.033 ↗
3. Ablation mechanism of TaC coating fabricated by chemical vapor deposition on carbon-carbon composites10.1016/S1003-6326(10)60133-1 ↗
4. Ablation characteristics of carbon fiber reinforced carbon (CFRC) composites in the presence of silicon carbide (SiC) coating10.1016/j.surfcoat.2003.10.071 ↗
5. Ablation resistant composite coating of HfC-TaC-SiC for C/C composites deposited by supersonic atmospheric plasma spraying
6. Ablation tests on HfC- and TaC- based ceramics for aeropropulsive applications10.1016/j.jeurceramsoc.2014.11.018 ↗
7. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
8. Preparation and characterization of tantalum carbide (TaC) ceramics10.1016/j.ijrmhm.2015.06.015 ↗
9. Synthesis, densification, and microstructure of TaC-TaB2-SiC ceramics10.1111/jace.15867 ↗
10. Wear resistance and adhesive failure of thermal spray ceramic coatings deposited onto graphite in response to ultrasonic nanocrystal surface modification technique10.1016/j.apsusc.2017.11.013 ↗
11. Performance of rocket nozzle materials with several solid propellants
12. Femtosecond pulsed laser ablation deposition of tantalum carbide10.1016/j.apsusc.2007.07.178 ↗
13. Laser ablation synthesis of tantalum carbide particles with specific phase assemblage and special interface10.1007/s00339-015-9171-7 ↗
14. Laser surface treatment of magnesium alloy with WC and TiC powders using HPDL
15. Improving the hot corrosion resistance of plasma sprayed ceria-yttria stabilized zirconia thermal barrier coatings by laser surface treatment10.1016/j.matdes.2013.12.075 ↗
16. Optimization of Ni-based WC/Co/Cr composite coatings produced by multilayer laser cladding
17. Scratch resistance and damage mechanism of laser remelted thermally sprayed ceramic coating10.1016/j.surfcoat.2019.02.078 ↗
18. Effect of plasma sprayed and laser re-melted Al2O3 coatings on hardness and wear properties of stainless steel10.1016/j.ceramint.2016.04.044 ↗
19. Bengisu · 2001
20. Development and optimization of porosity measurement techniques10.1016/j.ceramint.2015.11.015 ↗
21. Sarpün · 2009 · 119
22. Use of the Taguchi method and grey relational analysis to optimize turning operations with multiple performance characteristics10.1081/AMP-120029852 ↗
23. Material removal effect of microchannel processing by femtosecond laser10.1016/j.optlaseng.2017.06.001 ↗
24. Effect of parameters on picosecond laser ablation of Cr12MoV cold work mold steel10.1007/s00339-017-1435-y ↗
25. Nanosecond laser-metal ablation at different ambient conditions10.1016/j.sab.2018.02.012 ↗
26. Accumulation effects in laser ablation of metals with high-repetition-rate lasers
27. Femtosecond laser for cavity preparation in enamel and dentin: ablation efficiency related factors
28. Laser-based repair for carbon fiber reinforced composites
29. Denkena · 2007 · 99
30. Effect of laser power and powder flow rate on dilution rate and surface finish produced during laser metal deposition of Titanium alloy
31. Influence of hatch spacing on heat and mass transfer, thermodynamics and laser processability during additive manufacturing of Inconel 718 alloy10.1016/j.ijmachtools.2016.07.010 ↗
32. Experimental study and empirical modelling of laser surface finishing of silicon carbide
33. The effect of scan speed on engraving depth and surface roughness of AISI H13 tool steel10.4028/www.scientific.net/AMR.264-265.1258 ↗
34. Ablation behaviour of a TaC coating on SiC coated C/C composites at different temperatures10.1016/j.ceramint.2012.06.034 ↗
35. High temperature oxidation study of tantalum carbide-hafnium carbide solid solutions synthesized by spark plasma sintering
36. Khanna · 2002
37. Identification of critical load for scratch adhesion strength of nitride-based thin films using wavelet analysis and a proposed analytical model10.1016/j.surfcoat.2015.07.061 ↗
38. Enhancement of the mechanical properties of hydroxyapatite/sulphonated poly ether ether ketone treated layer for orthopaedic and dental implant application10.1155/2018/9607195 ↗
39. Damage mechanisms and cracking behavior of thermal sprayed WC-CoCr coating under scratch testing10.1016/j.wear.2014.02.017 ↗
40. Comparative study on microstructure and corrosion performance of 316 stainless steel prepared by laser melting deposition with ring-shaped beam and Gaussian beam10.1016/j.optlastec.2018.09.057 ↗
41. Investigation of the adhesion strength and deformation behaviour of in situ fabricated NbC coatings by scratch testing10.1016/j.surfcoat.2016.05.004 ↗