Abstract

Abstract 3Y-TZP discs were coated using 5Y-PSZ and 12Ce-TZP suspensions. Samples were evaluated in terms of roughness (Ra, Rq, Rz and Rsk), B3B flexural resistance, hardness, Young's modulus by instrumented indentation and surface damage resistance and Vickers hardness by impress Vickers measurements. Coatings with thickness of ~7 μm were obtained. 3Y-TZP uncoated discs showed similar hardness and Young's modulus when compared to those coated with 5Y-PSZ. Discs coated with 12Ce-TZP had opposite behavior. Vickers and Berkovich hardness showed the same trend, with almost no difference observed between monolithic and the 5Y-PSZ coated samples, and with the 12Ce-TZP coated samples exhibiting lower hardness values. Coated samples presented lower flexural strength than uncoated ones. Correlation between roughness and B3B flexural strength was also performed, showing that surface quality achieved by the coating process is the one that rules the final resistance of the component, instead of the coating material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Ceramic steel?10.1038/258703a0 ↗
2. Effect of loading configuration on strength values in a highly transformable zirconia-based composite10.1016/j.dental.2016.06.023 ↗
3. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
4. Toughening of yttria-stabilised tetragonal zirconia ceramics10.1179/174328005X41113 ↗
5. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
6. Towards long lasting zirconia-based composites for dental implants . Part I : innovative synthesis , microstructural characterization and in vitro stability10.1016/j.biomaterials.2015.01.018 ↗
7. Zirconia-based composites for biomedical applications: role of second phases on composition, microstructure and zirconia transformability10.1016/j.jeurceramsoc.2015.04.027 ↗
8. The martensitic transformation in ceramics - its role in transformation toughening10.1016/S0079-6425(00)00005-0 ↗
9. Phase change and mechanical properties of ZrO2-Y203 solide electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
10. Low-temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
11. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
12. Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure10.1016/S0109-5641(01)00095-1 ↗
13. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
14. Enhanced reliability of yttria-stabilized zirconia for dental applications10.1016/j.actbio.2015.01.023 ↗
15. Brannvall · 2012
16. Effect of thickness, processing technique and cooling rate protocol on the flexural strength of a bilayer ceramic system10.1016/j.dental.2013.07.019 ↗
17. Mechanical behavior of ceramic-metal joint under quasi-static and dynamic four point bending: microstructures, damage and mechanisms10.1016/j.ceramint.2017.02.064 ↗
18. Effect of metallization on the strength and fracture behaviour of functional co-fired multilayer ceramics10.1016/j.jeurceramsoc.2017.02.018 ↗
19. Improvement of 3Y-TZP aging behavior by means of zirconia-based protective layers10.1016/j.jeurceramsoc.2020.03.041 ↗
20. Fracture strength, surface roughness and corrosion of ceramics10.1016/0272-8842(92)90086-S ↗
21. Fractography of self-glazed zirconia with improved reliability10.1016/j.jeurceramsoc.2017.03.008 ↗
22. Manufacturing conditioned roughness and wear of biomedical oxide ceramics for all-ceramic knee implants10.1186/1475-925X-12-84 ↗
23. Beger · 2018
24. Effect of laser surface texturing on primary stability and surface properties of zirconia implants10.1016/j.ceramint.2017.08.058 ↗
25. Evaluation of KIc of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
26. On the vickers indentation fracture toughness Test10.1111/j.1551-2916.2006.01482.x ↗
27. The compelling case for indentation as a functional exploratory and characterization tool10.1111/jace.13729 ↗
28. Instrumented and vickers indentation for the characterization of stiffness, hardness and toughness of zirconia toughened Al2O3 and SiC armor10.1016/j.jmst.2015.06.005 ↗
29. Towards long lasting zirconia-based composites for dental implants: transformation induced plasticity and its consequence on ceramic reliability10.1016/j.actbio.2016.11.040 ↗
30. Comparative study of flexural strength test methods on CAD/CAM Y-TZP dental ceramics.pdf10.1093/rb/rbv020 ↗
31. Effect of hydrofluoric acid etching duration on the roughness and flexural strength of a lithium disilicate-based glass ceramic10.1590/S0103-64402011000100008 ↗
32. Influence of surface roughness on mechanical strength of resin composite versus glass ceramic materials10.1016/j.dental.2007.05.006 ↗
33. Strength influencing variables on CAD/CAM zirconia frameworks10.1016/j.dental.2007.06.030 ↗
34. Strength and aging resistance of monolithic zirconia : an update to current knowledge10.1016/j.jdsr.2019.09.002 ↗
35. Wear mechanism and morphologic space in ceramic honing process10.1016/j.wear.2016.05.002 ↗
36. Influence of surface roughness on mechanical properties of two computer-aided design/computer-aided manufacturing (CAD/CAM) ceramic materials10.2341/11-391-L ↗
37. Comparison between Berkovich, Vickers and conical indentation tests: a three-dimensional numerical simulation study10.1016/j.ijsolstr.2008.10.032 ↗
38. Effect of loading conditions on the fracture toughness of zirconia10.1016/j.jpor.2013.01.005 ↗
39. Relevance of instrumented micro-indentation for the assessment of hardness and Young's modulus of brittle materials10.1016/j.msea.2006.11.109 ↗
40. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗