Hot corrosion behaviour of Yb2Si2O7 environmental barrier coatings in molten NaVO3 salt

Yongqiu Zhang, Binglin Zou, Xiaolong Chen, Xiaolong Cai, Ying Wang, Pai Huang, Ge Yu, Zhengwei Gu

Ceramics International· Volume 47· Issue 21
Publisher page

Abstract

Abstract The hot corrosion behaviour of Yb2Si2O7 environmental barrier coatings in molten salt NaVO3 was studied at 1000 °C-1300 °C. Results showed that YbVO4 and Yb2SiO5 were the main corrosion products, with rod-like and granular morphologies, respectively. The content of corrosion products was dependent on the corrosion temperatures. The content of YbVO4 decreased at 1000 °C-1200 °C and disappeared at 1300 °C. However, the content of Yb2SiO5 increased at 1100 °C-1300 °C and Yb2SiO5 was the main corrosion product at 1300 °C. The amorphous phase in the Yb2Si2O7 coating had a remarkable effect on the corrosion results. After heat treatment was conducted at 1400 °C for 12 h, the amorphous phase crystallised and then YbVO4 was the main corrosion product at 1300 °C. A model describing the formation of corrosion products was established on the basis of the corrosion products and the corrosion mechanism was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Protective coatings for gas turbines
2. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
3. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
4. Mass spectrometric identification of Si-OH (g) species from the reaction of silica with water vapor at atmospheric pressure10.1111/j.1151-2916.1997.tb02935.x ↗
5. Water vapor-mediated volatilization of high-temperature materials10.1146/annurev-matsci-071312-121636 ↗
6. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
7. Kinetics and mechanism of corrosion of SiC by molten salts10.1111/j.1151-2916.1986.tb04698.x ↗
8. Corrosion of SiC/SiCcomposite in Na2SO4 vapor environments from 1000 to 1500°C10.1016/j.compositesa.2005.07.010 ↗
9. Corrosion failures in gas turbine hot components10.1007/s11668-012-9571-3 ↗
10. Hot corrosion of α-SiC ceramics by V2O5 melt10.1007/BF01045359 ↗
11. CMAS degradation of environmental barrier coatings10.1016/j.surfcoat.2007.06.045 ↗
12. Calcium-magnesium aluminosilicate interaction with yttrium monosilicate environmental barrier coatings10.1111/j.1551-2916.2010.03916.x ↗
13. Molten silicate reactions with plasma sprayed ytterbium silicate coatings10.1016/j.surfcoat.2015.12.053 ↗
14. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
15. Volcanic ash melting under conditions relevant to ash turbine interactions10.1038/ncomms10795 ↗
16. Current status of environmental barrier coatings for Si-based ceramics
17. Theoretical and experimental determination of the major thermo-mechanical properties of RE2SiO5 (RE=Tb, Dy, Ho, Er, Tm, Yb, Lu, and Y) for environmental and thermal barrier coating applications10.1016/j.jeurceramsoc.2015.09.013 ↗
18. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
19. Corrosion of RE2Si2O7 (RE=Y, Yb, and Lu) environmental barrier coating materials by molten calcium-magnesium-alumino-silicate glass at high temperatures10.1016/j.jeurceramsoc.2019.05.036 ↗
20. Recession behavior of Yb2Si2O7 phase under high speed steam jet at high temperatures10.1016/j.corsci.2007.06.014 ↗
21. Residual stress analysis of multilayer environmental barrier coatings10.1111/j.1551-2916.2008.02888.x ↗
22. Thermal expansion of rare-earth pyrosilicates10.1111/jace.12388 ↗
23. Thermal properties of single-phase Y2SiO510.1016/j.jeurceramsoc.2008.07.026 ↗
24. Silica activity measurements in the Y2O3-SiO2 system and applications to modeling of coating volatility10.1111/jace.12974 ↗
25. Mass spectrometric measurements of the silica activity in the Yb2O3-SiO2 system and implications to assess the degradation of silicate-based coatings in combustion environments10.1016/j.jeurceramsoc.2015.07.019 ↗
26. Response of ytterbium disilicate–silicon environmental barrier coatings to thermal cycling in water vapor10.1016/j.actamat.2015.12.053 ↗
27. Effect of processing on high-velocity water vapor recession behavior of Yb-silicate environmental barrier coatings10.1016/j.jeurceramsoc.2018.11.048 ↗
28. The influence of calcium–magnesium–aluminosilicate deposits on internal stresses in Yb2Si2O7 multilayer environmental barrier coatings10.1016/j.actamat.2015.12.016 ↗
29. The interaction of calcium-magnesium-aluminosilicate with ytterbium silicate environmental barrier materials10.1016/j.surfcoat.2015.08.069 ↗
30. Effects of sintering additives on hot corrosion behavior of γ-Y2Si2O7 ceramics in Na2SO4+V2O5 molten salt10.1016/j.jeurceramsoc.2020.08.068 ↗
31. Hot corrosion behavior of Yb2Si2O7 ceramic under NaVO3 salt attack10.1016/j.ceramint.2019.09.070 ↗
32. Comparative study on high-temperature performance and thermal shock behavior of plasma-sprayed Yb2SiO5 and Yb2Si2O7 coatings10.1016/j.surfcoat.2018.06.056 ↗
33. Phase and microstructure evolution in plasma sprayed Yb2Si2O7 coatings10.1016/j.jeurceramsoc.2018.11.018 ↗
34. Density functional study of the phase stability and Raman spectra of Yb2O3, Yb2SiO5 and Yb2Si2O7 under pressure10.1039/C8CP02497A ↗
35. Low-temperature Raman spectra of YbVO410.1016/j.vibspec.2007.05.002 ↗