journal article·2025-02

Shrinkage-controlled hydrothermal carbon: An advanced interphase for achieving synergistic stress dispersion and load transfer in Cf/ZrB2-SiC composites

Huan Yang, Cheng Fang, Hongliang Xu, Xia Zhang, Yang Liu, Jiayin Zhao, Anzhe Wang, Hongxia Lu, Hailong Wang

Ceramics International· Volume 51· Issue 4
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Viable route to the manufacture of short carbon fiber-rich UHTC complex shapes with enhanced toughness10.1016/j.compositesb.2024.111373 ↗
2. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs – a review10.1080/09506608.2019.1652006 ↗
3. Effect of pyrolytic carbon coating on the microstructure and fracture behavior of the Cf/ZrB2-SiC composite10.1016/j.ceramint.2018.07.210 ↗
4. Characterization of hot-pressed short carbon fiber reinforced ZrB2–SiC ultra-high temperature ceramic composites10.1016/j.jallcom.2008.04.092 ↗
5. Fabrication and characterization of an ultra‐high‐temperature carbon fiber‐reinforced ZrB2–SiC matrix composite10.1111/j.1551-2916.2007.01876.x ↗
6. Enhancing the fracture resistance of carbon fiber reinforced SiC matrix composites by interface modification through a simple fiber heat-treatment process10.1016/j.carbon.2016.08.047 ↗
7. Microstructure and mechanical behaviors of T700 carbon fiber reinforced C/SiC composites via precursor infiltration and pyrolysis10.1016/j.msea.2016.03.090 ↗
8. High efficient and continuous surface modification of carbon fibers with improved tensile strength and interfacial adhesion10.1016/j.apsusc.2017.03.279 ↗
9. Using PyC modified 3D carbon fiber to reinforce UHTC under low temperature sintering without pressure10.1007/s40145-021-0495-9 ↗
10. Boron carbonitride coatings synthesized by LPCVD, structure and properties10.1016/j.carbon.2017.06.024 ↗
11. Evaluation of the effect of PyC coating thickness on the mechanical properties of T700 carbon fiber tows10.1016/j.apsusc.2018.08.195 ↗
12. Effect of pyrolytic carbon interface thickness on microstructure and mechanical properties of lightweight zirconium boride modified carbon-bonded carbon fiber composites10.1016/j.compositesb.2016.03.094 ↗
13. Boron nitride (BN) and BN based multiple-layer interphase for SiCf/SiC composites: a review10.1016/j.ceramint.2022.07.021 ↗
14. Tensile strength, oxidation resistance and wettability of carbon fibers coated with a TiC layer using a molten salt method10.1016/j.matdes.2013.02.084 ↗
15. Biomass-based hydrothermal carbons for catalysis and environmental cleanup: a review10.1080/17518253.2022.2028017 ↗
16. Hydrothermal synthesis and applications of advanced carbonaceous materials from biomass: a review10.1007/s42114-020-00158-0 ↗
17. Coating of solid substrates with carbon via hydrothermal carbonization10.1016/j.matlet.2021.129315 ↗
18. Effects of multilayer hydrothermal carbon interphases on mechanical properties and thermal shock resistance of CF/ZrB2-SiCBN10.1016/j.jeurceramsoc.2022.05.029 ↗
19. Constructing hydrothermal carbonization coatings on carbon fibers with controllable thickness for achieving tunable sorption of dyes and oils via a simple heat-treated route10.1016/j.jcis.2019.10.047 ↗
20. Influence of fiber coating thickness on microstructure and mechanical properties of carbon fiber-reinforced zirconium diboride based composites10.1016/j.ceramint.2013.07.040 ↗
21. Replication and coating of silica templates by hydrothermal carbonization10.1002/adfm.200600501 ↗
22. A multiscale hydrothermal carbon layer modified carbon fiber for composite fabrication10.1039/C8RA04064H ↗
23. Carboxylate-rich carbonaceous materials via one-step hydrothermal carbonization of glucose in the presence of acrylic acid10.1021/cm802141h ↗
24. Influence of hydrothermal carbon coating on the properties of CF/ZrB2/SiBCN prepared by slurry injection10.1016/j.jeurceramsoc.2020.08.019 ↗
25. An efficient hydrothermal transformation approach for construction of controllable carbon coating on carbon fiber from renewable carbohydrate10.1016/j.apsusc.2019.06.186 ↗
26. Pyrolysis of sucrose-derived hydrochar10.1016/j.jaap.2021.105404 ↗
27. Fabricating 2.5 D SiCf/SiC composite using polycarbosilane/SiC/Al mixture for matrix derivation10.1111/j.1551-2916.2006.01480.x ↗
28. Effects of in-situ carbon layer and volume fraction of SiC fiber on the mechanical properties and fracture behaviors of SiCf/SiC composites fabricated by a modified PIP method10.1016/j.jeurceramsoc.2022.11.012 ↗
29. Effect of curing process and pyrolysis temperature on the microstructure, adhesion and corrosion resistance of PCS-derived coatings10.1016/j.ceramint.2022.06.110 ↗
30. Modification of the fiber-matrix interface in the carbon fiber reinforced ZrB2-based ultra-high temperature ceramic composites
31. Rapid spark plasma sintering to produce dense UHTCs reinforced with undamaged carbon fibres10.1016/j.matdes.2017.05.029 ↗
32. Key role of interphase in continuous fiber 3D printed ceramic matrix composites10.1016/j.compositesa.2022.107127 ↗
33. Design and optimization of the coating thickness on chopped carbon fibers and sintering temperature for ZrB2-SiC-Cf composites prepared by hot pressing10.1016/j.jeurceramsoc.2019.03.038 ↗
34. Mechanical properties of SiCf/SiC composites with alternating PyC/BN multilayer interfaces10.1080/17436753.2017.1339517 ↗
35. Using PyC coated short chopped carbon fiber to tackle the dilemma between toughness and strength of ZrC-SiC10.1016/j.ceramint.2018.09.196 ↗
36. Fabrication and microstructure evolution of Csf/ZrB2-SiC composites via direct ink writing and reactive melt infiltration10.1007/s40145-021-0512-z ↗
37. Tensile behavior of ceramic matrix minicomposites with engineered interphases fabricated by chemical vapor infiltration10.1016/j.jeurceramsoc.2022.01.047 ↗
38. On understanding the mechanical properties and damage behavior of Cf/SiC composites by indentation method10.1016/j.jmrt.2023.08.117 ↗
39. Single fiber push-out characterization of interfacial mechanical properties in unidirectional CVI-C/SiC composites by the nano-indentation technique10.1016/j.apsusc.2015.10.018 ↗
40. Influence of fiber surface properties of SiCf/SiC composites on the interfacial debonding behavior10.1016/j.jeurceramsoc.2023.09.081 ↗
41. Model development for work of fracture of hybrid composites10.1002/app.44711 ↗
42. Study on toughening mechanisms of pyrolytic carbon interface layer in Cf/ZrB2-SiC composites using in-situ tensile experimental and numerical methods10.1016/j.jeurceramsoc.2021.04.028 ↗
43. Micromechanical model of composite materials subjected to ball indentation10.1177/002199839302700304 ↗
44. The effect of heat treatment on the strength and toughness of carbon fiber/silicon carbide composites with different pyrolytic carbon interphase thicknesses10.1016/j.carbon.2013.01.076 ↗
45. Reaction mechanism and microstructure development of ZrSi2 melt-infiltrated Cf/SiC-ZrC-ZrB2 composites: the influence of preform pore structures10.1016/j.jmat.2018.05.005 ↗
46. Imbibition triggered by capillary condensation in nanopores10.1021/acs.langmuir.6b04534 ↗
47. Comparison of the orientational dynamics of water confined in hydrophobic and hydrophilic nanopores10.1021/jp026349l ↗
48. Capillary dynamic under nanoconfinement: coupling the energy dissipation of contact line and confined water10.1016/j.ijheatmasstransfer.2018.07.114 ↗
49. Mechanical behavior of SiCf/SiC composites with alternating PyC/SiC multilayer interphases10.1016/j.matdes.2012.07.073 ↗
50. Mechanical and electromagnetic shielding performance of carbon fiber reinforced multilayered (PyC-SiC) n matrix composites10.1016/j.carbon.2016.10.004 ↗