Interactions of sulfur-containing gas with magnesia-chromite refractory in nickel flash smelting furnace
Source abstract
Abstract
As-received and spent magnesia-chromite refractories from a nickel flash smelting furnace were analyzed and compared to shed light on the interactions between the gas phase and the refractory material, a topic that has not received previous research effort. Based on the results, process-originated gaseous sulfur-containing species, such as SO 2 and SO 3 , played a key role in the refractory reactions. In the absence of a surface deposit, the hot end of the refractory underwent attack by SO 2 , resulting in sulfation of both the periclase and chromite phases, which has not been reported before. In the presence of a surface deposit, the sulfation of main phases in the near-surface regions did not occur, but sulfur-bearing species diffused deeper into the refractory material, where they reacted with MgO and CaO, forming MgSO 4 and CaSO 4 . In addition to the detected sulfur penetration, impurity elements, e.g., As; K, and Pb, had diffused towards the cold end of the refractory. This suggests these elements could have entered the refractory as gaseous species and then condensed at low enough temperatures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Metal Extraction and Bioleaching · Iron and Steelmaking Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Crundwell · 2011 · 610
2. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
3. Melt corrosion of oxide and oxide-carbon refractories10.1179/095066099101528234 ↗
4. Flash smelting and converting furnaces: a 50 Year retrospect
5. Refractories for copper production10.1080/08827509608914131 ↗
6. Post-mortem study of magnesia-chromite refractory used in the gas area of a Submerged Arc Furnace for the copper-making process10.1016/j.bsecv.2018.12.001 ↗
7. Ranki-Kilpinen · 2002 · 261
8. Crundwell · 2011 · 610
9. The effect of deposit temperature on the catalytic SO2-to-SO3 conversion in a copper flash smelting heat recovery boiler10.1007/s11663-017-1130-6 ↗
10. The Influence of order in the cation sublattice of MgAl2O4, MgCr2O4 and MgFe2O4 spinels on the kinetics of topochemical reactions with sulphur oxides
11. Study of refractory wear in the tuyere region of a Peirce-Smith nickel convertor10.1179/cmq.1998.37.2.99 ↗
12. N.Z. Fotoyi, R.H. Eric, Interaction of MgO-MgR2O4(R: Al, Cr, Fe) Refractories with SO2-Containing Gases in Southern African Pyrometallurgy 2011, Edited by R.T. Jones & P. den Hoed, Southern African Institute of Mining and Metallurgy, Johannesburg, 6–9 March 2011.
13. Refractory challenges in nickel and cobalt processing furnaces in Ni-Co 2021: the 5th international symposium on nickel and cobalt
14. High temperature gaseous corrosion resistance of MgO-containing refractories – a comparative study10.1016/j.ceramint.2016.07.047 ↗
15. Collaboration: authors and editors of the volumes III/17B-22A-41B. Magnesium oxide (MgO) Debye temperature, heat capacity, density, melting and boiling points, hardness. In: Madelung, O., Rössler, U., Schulz, M. (eds) II-VI and I-VII Compounds; Semimagnetic Compounds. Landolt-Börnstein - Group III Condensed Matter, vol 41B. Springer, Berlin, Heidelberg.
16. PAULING FILE in: inorganic solid phases, SpringerMaterials (online database)
17. Corrosive interaction between slags high in copper and nickel oxides and periclase, periclase-chromite, and chromite refractories10.1007/s11148-006-0003-3 ↗
18. Reaction sequences in flash smelting and converting furnaces: an in-depth view10.1007/s11663-021-02283-7 ↗
19. Deposit build-up and corrosion in a copper flash smelting heat recovery boiler10.1007/s11085-016-9666-4 ↗
20. Mechanism and kinetics of thermal decomposition of nickel(II) sulfate(VI) hexahydrate10.1023/B:JTAN.0000033184.32714.7f ↗
21. TG/DTA/MS Study of the thermal decomposition of FeSO4·6H2O10.1007/s10973-005-7267-6 ↗
22. H. Zargar, G. Oprea, T. Troczynski, Influence of solid solution formation on the solid state sintering of MgCr2O4. Proceedings of the Unified International Technical Conference on Refractories UNITECR2013, pp. 313-317. https://doi.org/10.1002/9781118837009.ch55.10.1002/9781118837009.ch55 ↗
23. Phase formation processes and structural changes in chromite-periclase refractories used during nickel production10.1007/s11148-012-9433-2 ↗
24. Chemical corrosion mechanisms of magnesia-chromite and chrome-free refractory bricks by copper metal and anode slag10.1016/j.jeurceramsoc.2006.08.020 ↗
25. The influence of slag compositional changes on the chemical degradation of magnesia-chromite refractories exposed to PbO-based non-ferrous slag saturated in spinel10.1016/j.jeurceramsoc.2014.08.017 ↗
26. The effect of a temperature gradient on the phase formation inside a magnesia-chromite refractory in contact with a non-ferrous PbO-SiO2-MgO slag10.1016/j.jeurceramsoc.2015.03.028 ↗
27. The effect of phase formation during use on the chemical corrosion of magnesia-chromite refractories in contact with a non-ferrous PbO-SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
28. Chemical wear mechanism of magnesia-chromite refractory for an oxygen bottom-blown copper smelting furnace: a post-mortem analysis10.1016/j.ceramint.2020.09.124 ↗
29. Corrosion of magnesia-chromite refractory by PbO-rich copper slags10.1016/j.corsci.2021.109949 ↗
30. Corrosion study of novel Cr-free alumina-spinel refractory material dedicated to the copper industry10.1016/j.jeurceramsoc.2022.08.038 ↗
31. Crystal chemistry of some AB2O4 compounds10.1111/j.1151-2916.1963.tb11755.x ↗
32. Investigations into the kinetics and mechanism of gas–solid state processes in MgO–MgR2O4 (R: Al, Cr, Fe) spinels–SO2–O2 system10.1016/j.ceramint.2007.04.019 ↗
33. Kinetics of the topochemical reaction of the solid solutions of magnesia spinels: Mg(Cr0.5Fe0.5)2O4, Mg(Al0.5Cr0.5)2O4, Mg(Al0.5Fe0.5)2O4 with sulphur oxides10.1016/j.tca.2019.178344 ↗
34. Thermochemistry of MgCr2O4, MgAl2O4, MgFe2O4 spinels in SO2−O2−SO3 atmosphere10.2298/PAC1601025G ↗
35. Application of a novel and simple TEST to evaluate the corrosion resistance of magnesia-based refractories to sulfur gases10.1016/j.ceramint.2020.07.113 ↗
36. The catalytic role of process dust in the SO2-to-SO3 conversion in flash smelting heat recovery boilers
37. Catalytic sulphation of limestone/lime with platinum10.1007/BF01979622 ↗
38. Decomposition thermodynamics of magnesium sulfate10.1021/ie102554f ↗
39. Comparison of the sulfation rates of calcium, magnesium and zinc oxides with SO2 and SO310.1002/cjce.5450630614 ↗
40. Interpretation of the sulfation rate of CaO, MgO, and ZnO with SO2 and SO310.1002/aic.690331110 ↗
41. Kinetics of the reaction of dense CaO particles with SO210.1021/ie2009668 ↗
42. Diffusion through CaSO4 formed during the reaction of CaO with SO2 and O210.1002/aic.690390419 ↗
43. Isotope study on diffusion in CaSO4 formed during sorbent-flue-gas reaction10.1002/aic.690411020 ↗
44. Identification of magnesia-chromite refractory degradation mechanisms of secondary smelter linings10.1016/j.jeurceramsoc.2016.02.036 ↗
45. Corrosion mechanism of magnesia-chrome and alumina-chrome refractories in E-scrap smelting10.1016/j.ceramint.2021.10.054 ↗
46. Reactions between magnesia-chrome refractories and copper converter slags: corrosion behaviour and prevention by Fe-rich layer formation10.1016/j.ceramint.2022.02.018 ↗