Wet forming and sintering behavior of nanometer-sized ceria powder
Source abstract
Abstract
Abstract An aqueous suspension of 25 vol.% ceria powder of 14 nm diameter (powder A) was consolidated by filtration through a gypsum mold. However, many cracks were formed during drying of the ceria compact. Addition of larger ceria powder of 37 nm diameter (powder B) to the 14 nm-ceria powder was effective to prevent the formation of cracks. The densification of the dried powder compacts with 90 vol.% powder A, 10 vol.% powder B was divided into four ranges with sintering temperature: range I (500–800 °C), sintering of primary particles within a secondary particle cluster; range II (800–1200 °C), grain growth of primary particles in a dense secondary particle cluster; range III (1200–1500 °C), sintering of dense secondary particle clusters with grain growth, and range IV (1500–1600 °C), grain growth of dense secondary particle clusters. Increased fraction of powder B to 40–60 vol.% suppressed the decrease of specific surface area of powder compact in the ranges I and II, leading to a continuous densification in the rages I and II. In the ranges III and IV, the densification rate was enhanced by the addition of powder B of 60 vol.%, because the coordination number of ceria grains to a pore decreased with addition of 37 nm-powder.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Pickering emulsions and particle stabilization · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Sintering behavior of nanocrystalline zirconia prepared by chemical vapor synthesis10.1111/j.1151-2916.2000.tb01266.x ↗
2. Ultrafine-grained dense monoclinic and tetragonal zirconia10.1111/j.1151-2916.1994.tb07040.x ↗
3. Synthesis, characterization and properties of nanophase TiO210.1557/JMR.1988.1367 ↗
4. Sintering characteristics of nanocrystalline TiO210.1557/JMR.1990.0609 ↗
5. Electrochemical synthesis and sintering of nanocrystalline cerium (IV) oxide powders10.1111/j.1151-2916.1995.tb08425.x ↗
6. Sintering of fine oxide powders: II. Sintering mechanism10.1111/j.1151-2916.1997.tb02879.x ↗
7. Cerium (IV) oxide synthesis and sinterable powders prepared by the polymetric organic complex solution method10.1016/S0955-2219(01)00483-6 ↗
8. Quantitative analysis of hierarchical pores in powder compact10.2109/jcersj.98.126 ↗
9. Theoretical aspects of colloidal processing10.1016/0272-8842(95)00144-1 ↗
10. Theory of drying10.1111/j.1151-2916.1990.tb05082.x ↗
11. Surface forces and their action in ceramic materials10.1111/j.1151-2916.1990.tb05168.x ↗
12. Synthesis of whisker reinforced mullite matrix composites using colloidal processing10.2109/jcersj.100.353 ↗
13. Formation of solid electrolyte films by transfer printing method
14. Rheological properties and consolidation of the suspension in the alumina powder–silicon nitride whisker system10.2109/jcersj.97.881 ↗
15. Forming of the alumina powder–silicon nitride whisker system with aqueous suspension
16. Compaction and sintering behavior of bimodal alumina powder suspension by pressure filtration10.1111/j.1151-2916.2000.tb01267.x ↗
17. Effect of interparticle potentials and sedimentation on particle packing density of bimodal particle distribution during pressure filtration10.1111/j.1151-2916.1991.tb07313.x ↗
18. Kingary · 1976
19. Sintering of fine oxide powders: I. Microstructural evolution10.1111/j.1151-2916.1996.tb08087.x ↗