Abstract Nano-particles of CaZrO 3 were successfully synthesized at 800 °C using the molten-salt method, and the effects of processing parameters, such as temperature, holding time and amount of salt on the crystallization of CaZrO 3 were investigated. Na 2 CO 3 , CaCl 2 and nano-ZrO 2 were used as starting materials. On heating, Na 2 CO 3 reacted with CaCl 2 to form NaCl and in situ CaCO 3 . Na 2 CO 3 –NaCl molten eutectic salt provided a liquid medium for reaction of CaCO 3 and ZrO 2 to form CaZrO 3 . The results demonstrated that CaZrO 3 started to form at about 700 °C and that, after the temperature was increased to 1000 °C, the amounts of CaZrO 3 in the resultant powders increased with a concomitant decrease in CaCO 3 and ZrO 2 contents. After washing with hot-distilled water, the samples heated for 3 h at 800 °C were single-phase CaZrO 3 with 70–90 nm particle size. Furthermore, the synthesized CaZrO 3 particles retained the size and morphology of the ZrO 2 powders, which indicated that a template formation mechanism dominated the formation of CaZrO 3 by molten-salt synthesis.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Calcium zirconate: preparation, properties and application to the solid oxide galvanic cells10.1016/S0013-4686(02)00540-6 ↗
2. Fabrication and characterization of perovskite CaZrO3 oxide thin films10.1016/j.ceramint.2003.12.037 ↗
3. Decreasing of CaZrO3 sintering temperature with glass frit addition10.1016/j.ceramint.2004.06.009 ↗
4. Low temperature synthesis of CaZrO3 powder from molten Salts10.1111/j.1551-2916.2006.01383.x ↗
5. Z. Song, Q. Li, D. Ma, J. Wen, F. Yuan, S. Deng, Production Process for Electrically Fused Calcium Zirconate, China Patent (2003) 6.
6. Sintering and densification of calcium zirconate powders prepared by coprecipitation
7. Wet chemical synthesis of the calcium zirconates CaZrO3 and CaZr4O9
8. Chemical synthesis of pure and Gd-doped CaZrO3 powders10.1016/S0955-2219(99)00130-2 ↗
9. Solution combustions synthesis of calcium zirconate, CaZrO3, powders10.1016/j.jssc.2009.12.015 ↗
10. X-ray microstructure characterization of ball-milled nanocrystalline microwave dielectric CaZrO3 by Rietveld method10.1107/S0021889804034351 ↗
11. Synthesis of NiWO4 nano-particles in low temperature molten salt medium10.1016/j.ceramint.2009.03.010 ↗
12. Lw temperature synthesis of SrWO4 nano-particles by a molten salt method10.1016/j.ceramint.2009.05.015 ↗
13. The effects of temperature and different precursors in the synthesis of nano spinel in KCl molten salt10.1016/j.ceramint.2011.08.009 ↗
14. Kubaschewski · 1979
15. Roth · 1984 · 63
16. Molten salt synthesis of LaAlO3 powder at low temperatures10.1016/j.jeurceramsoc.2007.01.008 ↗
17. Molten salt synthesis of zinc aluminate powder10.1016/j.jeurceramsoc.2007.02.195 ↗
18. Potentiometric measurements in molten chlorides solubilities of metal oxides in the molten eutectic mixture CsCl–KCl–NaCl at 600°C10.1016/0013-4686(93)80086-F ↗
19. On the solubility of bivalent metal oxides in molten alkaline chlorides10.1016/0013-4686(94)80031-6 ↗