Effect of TiO2 on sinterability and physical properties of pressureless sintered Ti3AlC2 ceramics
Source abstract
Abstract
Abstract TiO2 was selected as effective sintering aid for pressureless sintering of Ti3AlC2 ceramics in this study. The addition of only 5 wt% TiO2 largely promotes the densification and nearly dense Ti3AlC2 ceramic was obtained by pressureless sintering at 1500 °C. Significant strengthening and toughening effects were observed with the addition of TiO2. High Vickers hardness, flexural strength and fracture toughness of 3.22 GPa, 298 MPa and 6.2 MPa m−1/2, respectively, were achieved in specimen pressureless sintered with 10 wt% TiO2. Additionally, the addition of 5 wt% TiO2 had no deleterious effect on the excellent oxidation resistance of Ti3AlC2 ceramic under 1200 °C water vapor atmosphere, while addition of 10 wt% TiO2 accelerates the oxidation rate by two orders of degree.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Progress in research and development on max phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
2. Recent progress in theoretical prediction, preparation, and characterization of layered ternary transition-metal carbides10.1146/annurev-matsci-082908-145340 ↗
3. Radiation tolerance of Mn+1AXn phases, Ti3AlC2 and Ti3SiC210.1016/j.actamat.2010.04.029 ↗
4. Contribution of core-loss fine structures to the characterization of ion irradiation damages in the Nanolaminated ceramic Ti3AlC210.1016/j.actamat.2013.08.041 ↗
5. Effects of neutron irradiation of Ti3SiC2 and Ti3AlC2 in the 121–1085 °C temperature range10.1016/j.jnucmat.2016.11.016 ↗
6. Effect of neutron irradiation on select max phases10.1016/j.actamat.2014.10.068 ↗
7. Max phase carbides and nitrides: properties for future nuclear power plant in-core applications and neutron transmutation analysis10.1016/j.nucengdes.2011.12.009 ↗
8. Opportunities for advanced ceramics and composites in the nuclear sector10.1111/jace.12406 ↗
9. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
10. Oxidation behavior of Ti3AlC2 at 1000–1400 °C in Air10.1016/S0010-938X(02)00177-4 ↗
11. Influence of water vapor on the oxidation behavior of Ti3AlC2 and Ti2AlC10.1016/j.scriptamat.2007.09.011 ↗
12. Oxidation-induced crack healing in Ti3AlC2 Ceramics10.1016/j.scriptamat.2007.09.006 ↗
13. Pressureless sintering and properties of Ti3AlC210.1111/j.1744-7402.2009.02403.x ↗
14. Microstructure and properties of Ti3AlC2 prepared by the solid–liquid reaction synthesis and simultaneous in-situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
15. Tribophysical properties of polycrystalline bulk Ti3AlC210.1111/j.1551-2916.2005.00588.x ↗
16. Synthesis and mechanical properties of Ti3AlC2 by spark plasma sintering10.1023/A:1024777213910 ↗
17. Formation of Ti3AlC2/Al2O3 and Ti2AlC/Al2O3 composites by combustion synthesis in Ti–Al–C–TiO2 systems10.1016/j.jallcom.2010.01.043 ↗
18. Pressure-assisted combustion synthesis of dense layered Ti3AlC2 and its mechanical properties10.1111/j.1551-2916.2004.00012.x ↗
19. Synthesis and microstructure of Ti3AlC2 by mechanically activated sintering of elemental powders10.1016/j.ceramint.2005.07.024 ↗
20. Powder synthesis, sintering kinetics, and nickel-activated pressureless sintering of Ti3AlC210.1111/j.1744-7402.2010.02572.x ↗
21. Synthesis and pressureless sintering of Ti3SiC2 powder10.1557/JMR.2009.0063 ↗
22. Pressureless sintering and mechanical properties of titanium aluminum carbide10.1016/j.matlet.2007.09.005 ↗
23. Strengthening of Ti3AlC2 by Incorporation of Al2O310.1016/j.scriptamat.2003.12.002 ↗
24. In situ synthesis, mechanical and cyclic oxidation properties of Ti3AlC2/Al2O3 composites10.1080/17436753.2018.1434953 ↗
25. Effect of grain size, notch width, and testing temperature on the fracture toughness of Ti3Si(Al)C2 and Ti3AlC2 using the Chevron-Notched beam (Cnb) method10.1016/j.jeurceramsoc.2007.07.011 ↗
26. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
27. Strengthening of Ti3AlC2 by incorporation of Si to form Ti3Al1−xSixC2 solid solutions10.1016/j.actamat.2005.10.057 ↗
28. Long-term oxidation of Ti2AlC in air and water vapor at 1000–1300 °C temperature range10.1149/2.052202jes ↗
29. Improving the oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution10.1016/j.actamat.2004.04.015 ↗
30. High oxidation resistance of hot pressed silicon nitride containing Yttria and Lanthania10.1016/S0955-2219(98)00237-4 ↗
31. The rate-controlling processes in the oxidation of hipped Si3N4 with and without sintering additives10.1016/0955-2219(91)90110-L ↗