Mechanical properties of sintered La9.33Si2Ge4O26 oxyapatite materials for SOFC electrolytes
Source abstract
Abstract
Abstract Mechanical properties of La 9.33 Si 2 Ge 4 O 26 prepared by mechanical alloying and subsequent sintering at 1300–1400 °C for 1 h were evaluated. Hardness and Young's modulus values in the range 7.3–9.6 GPa and 106–135 GPa, respectively, were obtained from nanohardness tests. The fracture toughness values derived from the Palmqvist method varied between 3.5 and 3.9 MPa m 1/2 from classical microindentation test with an indentation load of 9.8 N. Yield stress ( σ y ) was determined by inverse analysis from microhardness tests. The maximum value of σ y (1829 MPa) was obtained for the sample sintered at 1400 °C showing the highest density (5.42 g/cm 3 ).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Oxide ionic conductivities of apatite-type lanthanum silicates and germanates and their possibilities as electrolyte of lower temperature operating SOFC10.1016/j.ceramint.2009.10.022 ↗
2. Powder synthesis, processing and characterization of lanthanum silicates for SOFC applications10.1016/j.jallcom.2009.10.106 ↗
3. Synthesis and characterization of oxide ions conductors with the apatite structure for intermediate temperature SOFC10.1016/j.matchemphys.2005.06.040 ↗
4. Ionic conductivity of apatite-type rare-earth silicates prepared by mechanical milling10.1016/j.jallcom.2008.09.070 ↗
5. New approach to develop dense lanthanum silicate oxyapatite sintered ceramics with high conductivity10.1016/j.ssi.2009.12.004 ↗
6. Preparation of aluminium lanthanum oxyapatite tapes, La10AlSi5O26.5, by tape casting and reaction sintering10.1016/j.jeurceramsoc.2011.03.023 ↗
7. Oxide ionic conductivity of apatite type Nd9.33(SiO4)6O2 single crystal10.1016/S0955-2219(98)00215-5 ↗
8. R. Serra, C.Alves, F.A.C. Oliveira, T. Marcelo, J. Mascarenhas, B. Trindade, Enhanced sinterability of mechanical alloyed La9.33Si2Ge4O26 oxyapatite powders for IT-SOFC electrolytes. Accepted for Publication in Ceramics International. 10.1016/j.ceramint.2012.03.042.
9. Nanostructured Mo3Al-based composites strengthened by Al2O3 precipitates10.1016/j.jallcom.2010.04.202 ↗
10. Ultra-microhardness testing procedure with Vickers indenter10.1016/S0257-8972(01)01413-X ↗
11. Fracture toughness evaluation of WC-Co alloys by indentation testing
12. ASTM E384-99 Standard test method for microindentation hardness of materials, ASTM International, West Conshohocken, PA, USA, 1999
13. A new aproach for reverse analyses in depth-sensing indentation using numerical simulation10.1016/j.actamat.2006.08.019 ↗
14. Computational modeling of the forward and reverse problems in instrumented sharp indentation10.1016/S1359-6454(01)00295-6 ↗
15. A modified swift law for prestrained materials10.1016/S0749-6419(98)00027-8 ↗
16. Influence of hydroxyl groups on the crystallization of lanthanum silicate glass10.1016/0022-3093(76)90126-5 ↗
17. Comparative study of micro-indentation and Chevron notch fracture toughness measurements of silicate and phosphate glasses10.1016/j.jnoncrysol.2004.08.181 ↗
18. Young's modulus of some SOFCs materials as a function of temperature10.1016/j.jeurceramsoc.2007.05.009 ↗
19. Determination of hardness, Young's modulus and fracture toughness of lanthanum tungstates as novel proton conductors10.1016/j.ceramint.2011.01.002 ↗
20. Application of Indentation Technique in Determining Fracture Toughness of Ceramics10.1016/0013-7944(88)90074-4 ↗
21. Fracture mechanics methods for ceramics, rocks and concrete