Rubbing induced strain-glass phase on ceramic BaTiO3 surface
Source abstract
Abstract
Abstract A comparative microstructural study of as sintered and rubbed surfaces of BaTiO3 (BTO) ceramic pellet has been carried out using lab (8 keV Cu-Kα) as well as synchrotron (8–19 keV) based powder x-ray diffraction (XRD) at room temperature. These studies show a drastic change in the surface-microstructure of the BTO ceramics. Just a minutes rubbing of the BTO ceramics on a rough surface causes broadening of diffraction peaks. Nearly 3-times increase in the peak width and ∼ 3-times increase in integrated peak intensity of (00l) type peaks has been observed. The changes were analyzed as rubbing induced (00l) texturing and occurrence of anisotropic strain with maxima along [00l]. High temperature XRD studies reveal that for the strained BTO grains, the tetragonal to cubic transformation does not initiates at the proper TC ∼120 °C and does not complete even at temperatures ∼ 350 °C, which is ∼ 3 times the normal TC. About 20% of the tetragonal phase still remains untransformed. These features have been attributed to the formation of strain-glass phase at the rubbed surface of the BTO ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Non-crystalline structure in solidified gold silicon alloys10.1038/187869b0 ↗
2. A highly processable metallic glass: Zr41.2Ti13.8Cu12.5Ni10.0Be22.510.1063/1.110520 ↗
3. Mydosh · 1993 · vol 17
4. Kinetic arrest of the first-order ferromagnetic-to-antiferromagnetic transition in Ce (Fe0.96Ru0.04)2: formation of a magnetic glass10.1103/PhysRevB.72.180401 ↗
5. Enhancement of equilibrium fraction in La0.5Ca0.5MnO3 by recrystallization10.1088/0953-8984/20/25/255245 ↗
6. Kinetic arrest of the first-order R-3c to Pbnm phase transition in supercooled LaxMnO3+δ (x = 1 and 0.9)10.1088/0953-8984/24/22/225405 ↗
7. In-field X-ray and neutron diffraction studies of re-entrant charge-ordering and field induced metastability in La0.175Pr0.45Ca0.375MnO3-δ10.1063/1.4994790 ↗
8. Evidence for strain glass in the ferroelastic-martensitic system Ti50-xNi50+x10.1103/PhysRevLett.95.205702 ↗
9. The relaxational properties of compositionally disordered ABO3 perovskites10.1088/0953-8984/15/9/202 ↗
10. Recent progress in relaxor ferroelectrics with perovskite structure10.1007/s10853-005-5915-7 ↗
11. Strain glass and ferroic glass–Unusual properties from glassy nano-domains10.1002/pssb.201451351 ↗
12. Shape memory effect and super elasticity in a strain glass alloy10.1103/PhysRevLett.97.225703 ↗
13. Premartensite serving as an intermediary state between strain glass and martensite in ferromagnetic Ni-Fe-Mn-Ga10.1016/j.matdes.2018.04.067 ↗
14. A FeNiMnC alloy with strain glass transition10.1016/j.pnsc.2018.01.013 ↗
15. Strain glass transition in high damping Mn-22Cu-5Ni-2Fe alloy10.1016/j.pnsc.2018.07.004 ↗
16. Mechanical relaxation and freezing in the room temperature strain glass alloy Ti50(Pd40Cr10)10.1088/1361-648X/aad3f0 ↗
17. Tilt strain glass in Sr and Nb co-doped LaAlO3ceramics10.1016/j.actamat.2019.02.007 ↗
18. Strain glass in ferroelastic systems: premartensitic tweed versus strain glass10.1080/14786430903074771 ↗
19. Ferroelectric-relaxor behavior of Ba(Ti0.7Zr0.3)O3 ceramics10.1063/1.1495069 ↗
20. Crossover from classical to relaxor ferroelectrics in BaTi1−xHfxO3 ceramics10.1088/0953-8984/18/13/013 ↗
21. Processing-induced strain glass states in a Ni49.5Ti50.5 shape memory alloy