journal article·1991-01

Strength of SiC and SiC-7·5% vol. TiB2 composite after corrosion with Na2SO4 and NaCl deposits

W.J. Tomlinson, D.M. Caslin

Ceramics International· Volume 17· Issue 1
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. On the oxidation mechanisms of silicon carbide in the 300° to 1300°C temperature range
2. Molten salt corrosion of SiC and Si3N4 ceramics10.1111/j.1151-2916.1976.tb10962.x ↗
3. Corrosion of silicon carbide in gases and alkaline melts10.1111/j.1151-2916.1976.tb09514.x ↗
4. The corrosion of silicon based ceramics in a residual fuel oil fired environment
5. High temperature strength of sintered a-SiC in salt and oxidising environments
6. Hot corrosion of sintered a-SiC at 1000°C10.1111/j.1151-2916.1985.tb10170.x ↗
7. Kinetics and mechanism of corrosion of SiC by molten salts10.1111/j.1151-2916.1986.tb04698.x ↗
8. Burner rig corrosion of SiC at 1000°C10.1111/j.1551-2916.1986.tb00008.x ↗
9. The effect of oxidation in the presence of salts on the strength of silicon nitride base ceramics10.1007/BF00797306 ↗
10. How molten salt affects silicon carbide
11. Federer · 1985
12. Corrosion of SiC ceramics by Na2SO410.1111/j.1551-2916.1988.tb00170.x ↗
13. Hot Corrosion behaviour of coated covalent ceramics10.1111/j.1551-2916.1988.tb00275.x ↗
14. Healing of surface cracks in SiC by oxidation10.1111/j.1151-2916.1970.tb12104.x ↗
15. Strength distribution of SiC ceramics after oxidation and oxidation under load10.1111/j.1151-2916.1981.tb15896.x ↗
16. Oxidation behaviour of silicon carbide ceramics at 1500°C
17. Durability testing of ceramic materials
18. Oxidation behaviour of silicon carbide under cyclic and static conditions10.1016/0272-8842(89)90002-3 ↗
19. Fabrication, formulation, mechanical properties, and oxidation of sintered Si3N4 ceramics using disc specimens10.1179/mst.1985.1.7.510 ↗
20. Microstructure and Material properties of SiCTiB2 particulate composites
21. Mechanical properties and oxidation behaviour of a hot-pressed SiC-15 vol% composite