ETS-synthesized Hi-Nicalon fiber–SiC matrix composite
Source abstract
Abstract
Abstract Tough ceramic matrix composites, such as SiC/SiC, require a compliant reinforcement/matrix interface coating. The deposition of desired interface coatings on small diameter fibers in SiC/SiC composites is a substantial challenge and costly. A new carbon-rich source gas, ethyltrichlorosilane (ETS), was used to fabric SiC/SiC composite with eight harness satin-woven Hi-Nicalon fabric cloth as reinforcement by the chemical vapor infiltration (CVI) process. A graphite fiber/matrix interlayer was spontaneously formed in the material from the ETS during the CVI matrix densification process, resulting in the composite having a sound interfacial shear stress of 86 MPa. The composite showed a high proportional limit stress of 450±65 MPa and an ultimate flexural strength of 567±75 MPa, coupled with ductile fracture behavior. This study indicates that the costly interfacial coating process might be omitted when ETS is used as source gas for SiC/SiC composite.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Thermal properties of materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Intermediate temperature strength degradation in SiC/SiC composites10.1016/S0955-2219(02)00144-9 ↗
2. Microstructure and mechanical properties of FCVI carbon fiber/SiC composites
3. HSR/EPM combustor materials development program10.1016/S0921-5093(98)01079-X ↗
4. Silicon carbide fiber reinforced glass-ceramic matrix composites exhibiting high strength and toughness10.1007/BF00543747 ↗
5. Fiber–matrix interfaces in ceramic composites10.1557/PROC-458-147 ↗
6. Fiber coatings and the mechanical properties of a fiber-reinforced ceramic composite
7. Hi-Nicalon™ fiber-reinforced CVI-SiC matrix composites: I effects of PyC and PyC–SiC multilayers on the fracture behaviors and flexural properties10.2320/matertrans.43.2568 ↗
8. Hi-Nicalon™ fiber-reinforced CVI-SiC matrix composites: II interfacial shear strength and its effects on the flexural properties10.2320/matertrans.43.2574 ↗
9. The concept of layered interlayers in SiC/SiC
10. Interfacial bond strength in SiC/C/SiC composite materials, as studied by single-fiber pushout tests10.1111/j.1151-2916.1998.tb02434.x ↗
11. Strong interface in CMCs a condition for efficient multilayered interlayers10.1557/PROC-365-371 ↗
12. W. Yang, Development of CVI process and property evaluation of CVI-SiC/SiC composites. Ph.D. thesis, Institute of Advanced Energy, Kyoto University, 2002.
13. Thermodynamic calculations for the chemical vapor deposition of silicon carbide10.1111/j.1151-2916.1983.tb10091.x ↗
14. ASTM C 1341-97, Standard test method for flexural properties of continuous fiber-reinforced advanced ceramic composites, 2000, pp. 509–526.
15. Mechanisms of toughening in ceramic matrix composites10.1002/9780470291092.ch20 ↗
16. An approach to the mechanical behavior of SiC/SiC and C/SiC ceramic matrix composites, part II theoretical approach10.1007/BF02403938 ↗