Sintering and physicochemical properties of compositions in the SiC–Al2O3–La2O3–Cr2O3 system II. Oxidation resistance of pressureless sintered compacts in the SiC–Al2O3–La2O3–Cr2O3 system
Source abstract
Abstract
Abstract Compacts prepared from SiC (70–55 wt%), Al2O3 (10 wt%) and LaCrO3 (20–35 wt%) by pressureless sintering in carbon at 1700°C were studied for their oxidation resistance in air at 1300, 1400 and 1500°C. The oxidation resistance of the material at 1500°C was dependent on the quantity of La2O3–Al2O3–SiO2 melt, which diffused from inside to the surface of the compacts. Instead, chromium compounds were retained in the material and barred the melt diffusion. Nevertheless, at 1300°C, La2O3 of the compacts reacted with SiO2 and gave a dependable protective layer of lanthanum silicates.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Pressureless sintering of β-SiC with Al2O3 additions10.1007/BF00351412 ↗
2. M. Omori, A.S. Akuma, T. Hirai, SiC sintered composite with Y2O3 and Al2O3, in: Ceramics Today — Tomorrow's Ceramics, Elsevier Science Publishers B. V., 1991, pp. 1327–1335.
3. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
4. Oxidation kinetics of hot-pressed silicon carbide in dry and wet oxygen
5. Effect of alumina content on the oxidation of hot-pressed silicon carbide10.1111/j.1151-2916.1975.tb19016.x ↗
6. The effect of chromia on the protection of alumina–SiC–C bricks against oxidation
7. Phase relations in the system La2O3–Al2O3–SiO2 at 1550°C
8. Carbon films from polyacrylonitrile10.1557/JMR.1989.0452 ↗
9. JANAF, Thermochemical Data, 2nd ed., USA Nat. Bu. Stan., 1971.