Role of Cation Ordering and Surface Segregation in High-Voltage Spinel LiMn1.5Ni0.5–xMxO4 (M = Cr, Fe, and Ga) Cathodes for Lithium-Ion Batteries

Dong Wook Shin, Craig A. Bridges, Ashfia Huq, M. Parans Paranthaman, Arumugam Manthiram

Chemistry of Materials· Volume 24· Issue 19
Publisher page

Abstract

The high-voltage doped spinel oxides LiMn 1.5 Ni 0.5– x M x O 4 (M = Cr, Fe, and Ga; 0 ≤ x ≤ 0.08) synthesized at 900 °C have been investigated systematically before and after postannealing at 700 °C. Neutron diffraction studies reveal that the cation-ordered domain size tends to increase upon annealing at 700 °C. Time-of-flight secondary-ion mass spectroscopy data reveal that the dopant cations M = Cr, Fe, and Ga segregate preferentially to the surface, resulting in a more stable cathode–electrolyte interface and superior cyclability at both room temperature and 55 °C with conventional electrolytes. The doping with Cr and Fe stabilizes the structure with a significant disordering of the cations in the 16d sites even after postannealing at 700 °C, resulting in high rate capability due to low charge-transfer resistance and polarization loss. In contrast, the Ga-doped and undoped LiMn 1.5 Ni 0.5 O 4 samples experience an increase in cation ordering upon postannealing at 700 °C, resulting in degradation in the rate capability due to an increase in the charge-transfer resistance and polarization loss.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Electrochemical Energy Laboratory and Materials Science and Engineering Program, The University of Texas at Austin, Austin, Texas 78712, United States

References (25)

Show source-provided references
1. Manthiram A. · J. Phys. Chem. Lett. · 2011 · 2 · 17610.1021/jz1015422 ↗
2. Tarascon J. M. · Nature · 2001 · 414 · 35910.1038/35104644 ↗
3. Hwang B. J. · J. Power Sources · 2002 · 108 · 25010.1016/S0378-7753(02)00023-X ↗
4. Patoux S. · J. Power Sources · 2009 · 189 · 34410.1016/j.jpowsour.2008.08.043 ↗
5. Liu G. Q. · J. Solid State Electrochem. · 2010 · 14 · 219110.1007/s10008-010-1061-5 ↗
6. Duncan H. · J. Electrochem. Soc. · 2011 · 158 · A53710.1149/1.3567954 ↗
7. Liu J. · Chem. Mater. · 2009 · 21 · 169510.1021/cm9000043 ↗
8. Liu J. · J. Electrochem. Soc. · 2009 · 156 · A83310.1149/1.3206590 ↗
9. Kunduraci M. · J. Electrochem. Soc. · 2006 · 153 · A134510.1149/1.2198110 ↗
10. Kunduraci M. · Electrochim. Acta · 2008 · 53 · 419310.1016/j.electacta.2007.12.057 ↗
11. Ma X. · J. Electrochem. Soc. · 2010 · 157 · A92510.1149/1.3439678 ↗
12. Shin D. W. · Electrochem. Commun. · 2011 · 13 · 121310.1016/j.elecom.2011.08.041 ↗
13. Arunkumar T. A. · Electrochem. Solid-State Lett. · 2005 · 8 · A40310.1149/1.1945369 ↗
14. Kim J. H. · Chem. Mater. · 2004 · 16 · 90610.1021/cm035050s ↗
15. Rodríguez-Carvajal J. · Physica B · 1993 · 192 · 5510.1016/0921-4526(93)90108-I ↗
16. Roìsnel T. · Mater. Sci. Forum · 2001 · 378 · 11810.4028/www.scientific.net/MSF.378-381.118 ↗
17. Ismail A. · J. Phys. Chem. C · 2012 · 116 · 70410.1021/jp2074682 ↗
18. Navrotsky A. · Science · 2010 · 330 · 19910.1126/science.1195875 ↗
19. Kunduraci M. · J. Power Sources · 2007 · 165 · 35910.1016/j.jpowsour.2006.11.051 ↗
20. Lee E. · Energy Environ. Sci. · 2012 · 5 · 604710.1039/c2ee03068c ↗
21. Ammundsen B. · J. Phys. Chem. B · 1998 · 102 · 793910.1021/jp981549b ↗
22. Ohzuku T. · Electrochim. Acta · 2001 · 46 · 232710.1016/S0013-4686(00)00725-8 ↗
23. Park O. K. · Energy Environ. Sci. · 2011 · 4 · 162110.1039/c0ee00559b ↗
24. Hirayama M. · J. Am. Chem. Soc. · 2010 · 132 · 1526810.1021/ja105389t ↗
25. Song J. · Chem. Mater. · 2012 · 24 · 310110.1021/cm301825h ↗